daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Material Design of Citric Acid-Modified Cellulose Composite Polymeric Materials with Both Tough and Sustainable Enhancement by Multiple Noncovalent Bonds AITranslate

Osaka University; Osaka University; Osaka University; Osaka University; Osaka University; Osaka University;Nara Laboratory;Nara Laboratory; Osaka Institute of Technology; Osaka University; Osaka University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

To achieve a carbon circulation society, petroleum-derived resources must be replaced with cellulose and other bioderived resources. Although cellulose serving as a filler enhances the mechanical properties of polymeric materials upon mixing, it remains a challenge to increase the contents of cellulose fillers while maintaining the enhanced mechanical properties. Regarding mechanical properties, polymer composites containing cellulose fillers can usually be improved by adding a small percentage of cellulose fillers. Unfortunately, mixing large amounts of cellulose fillers creates brittle polymer composites. Herein, we report polymer composites containing large amounts of citric acid-modified cellulose. Moreover, the polymeric matrices consist of reversible cross-links formed by β-cyclodextrin and adamantane and secondary linear polymers. By optimizing the ratios of the reversible cross-links and the secondary linear polymers, we successfully increase the content of cellulose fillers to 10%, which is 1 order of magnitude higher than the conventional cellulose filler contents, maintaining high toughness and Young’s modulus values. In addition, utilizing hydrogen bonds is appropriately advantageous in the reinforcing effect of citric acid-modified cellulose compared to native cellulose.

KeyWords AITranslate

polymer composites cellulose fillers reversible crosslinks hydrogen bonds host−guest complexation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02107

Chinese Library Classification Number:

Citation Information:

To achieve a carbon circulation society, petroleum-derived resources must be replaced with cellulose and other bioderived resources. Although cellulose serving as a filler enhances the mechanical properties of polymeric materials upon mixing, it remains a challenge to increase the contents of cellulose fillers while maintaining the enhanced mechanical properties. Regarding mechanical properties, polymer composites containing cellulose fillers can usually be improved by adding a small percentage of cellulose fillers. Unfortunately, mixing large amounts of cellulose fillers creates brittle polymer composites. Herein, we report polymer composites containing large amounts of citric acid-modified cellulose. Moreover, the polymeric matrices consist of reversible cross-links formed by β-cyclodextrin and adamantane and secondary linear polymers. By optimizing the ratios of the reversible cross-links and the secondary linear polymers, we successfully increase the content of cellulose fillers to 10%, which is 1 order of magnitude higher than the conventional cellulose filler contents, maintaining high toughness and Young’s modulus values. In addition, utilizing hydrogen bonds is appropriately advantageous in the reinforcing effect of citric acid-modified cellulose compared to native cellulose.

quote

GB/T 7714-2015 [1] Takuma Wada, Junsu Park, Kenji Yamaoka, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c02107.
MLA [1] Takuma Wada, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c02107.
APA [1] Takuma Wada, Junsu Park, Kenji Yamaoka, Yuki Asaki, Akihide Sugawara, Ryohei Ikura, Yuya Takahashi, Naomi Takenaka, Yasutomo Uetsuji, Hiroshi Uyama, & Yoshinori Takashima. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c02107
IEEE [1] Takuma Wada, Junsu Park, Kenji Yamaoka, Yuki Asaki, Akihide Sugawara, Ryohei Ikura, Yuya Takahashi, Naomi Takenaka, Yasutomo Uetsuji, Hiroshi Uyama, and Yoshinori Takashima, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c02107. keywords: {polymer composites;cellulose fillers;reversible crosslinks;hydrogen bonds;host−guest complexation}