Achieving a Reversible and Durable Zn Anode Using the Polyzwitterionic Hydrogel Electrolyte for Efficient Zn-Ion Energy Storage AITranslate

Xinjiang University; Xinjiang University; Dalian University of Technology; Xinjiang University; Dalian University of Technology; Xinjiang University; Xinjiang University; Beijing University of Chemical Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Rechargeable aqueous Zn-ion hybrid supercapacitors (ZHSCs), featuring high safety, ecofriendliness, and cost effectiveness, have been regarded as a compelling complement to traditional lithium-ion batteries and have attracted increasing attention. However, the notorious dendrite growth and side reactions reduce the durability and reversibility of the Zn anode, causing a serious challenge for the application of ZHSCs. Herein, a polyzwitterionic P(HEA-co-SBMA)-based hydrogel electrolyte (denoted as PHSHE) for highly reversible Zn plating/stripping is fabricated to tackle tricky issues of Zn anodes and achieve high-performance ZHSCs. The zwitterionic groups carried by the polymer chains construct ion migration channels to facilitate ion migration, endowing the PHSHE with high ionic conductivity and Zn2+ transference number. Experimental findings reveal that the PHSHE can promote even Zn deposition and restrain side reactions. Accordingly, Zn anodes can be operated steadily in the PHSHE-intensified Zn//Cu cell for 650 cycles and Zn//Zn cell for 400 h. Furthermore, the quasi-solid-state ZHSC based on the PHSHE delivers a high capacity retention (80.8% after 14,000 cycles), mechanical flexibility, and application feasibility. This study is a step forward for stable Zn-based energy storage enabled by polyzwitterionic hydrogel electrolytes.

KeyWords AITranslate

Znion hybrid supercapacitors polyzwitterionic hydrogel electrolyte Zn anode issues dendrite inhibition side reaction suppression
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02124

Chinese Library Classification Number:

Citation Information:

Rechargeable aqueous Zn-ion hybrid supercapacitors (ZHSCs), featuring high safety, ecofriendliness, and cost effectiveness, have been regarded as a compelling complement to traditional lithium-ion batteries and have attracted increasing attention. However, the notorious dendrite growth and side reactions reduce the durability and reversibility of the Zn anode, causing a serious challenge for the application of ZHSCs. Herein, a polyzwitterionic P(HEA-co-SBMA)-based hydrogel electrolyte (denoted as PHSHE) for highly reversible Zn plating/stripping is fabricated to tackle tricky issues of Zn anodes and achieve high-performance ZHSCs. The zwitterionic groups carried by the polymer chains construct ion migration channels to facilitate ion migration, endowing the PHSHE with high ionic conductivity and Zn2+ transference number. Experimental findings reveal that the PHSHE can promote even Zn deposition and restrain side reactions. Accordingly, Zn anodes can be operated steadily in the PHSHE-intensified Zn//Cu cell for 650 cycles and Zn//Zn cell for 400 h. Furthermore, the quasi-solid-state ZHSC based on the PHSHE delivers a high capacity retention (80.8% after 14,000 cycles), mechanical flexibility, and application feasibility. This study is a step forward for stable Zn-based energy storage enabled by polyzwitterionic hydrogel electrolytes.

quote

GB/T 7714-2015 [1] Liheng Xie, Yuexin Liang, Zhiyu Wang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c02124.
MLA [1] Liheng Xie, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c02124.
APA [1] Liheng Xie, Yuexin Liang, Zhiyu Wang, Wentao Zhang, Fengjiao Guo, Xiaqing Chang, Hongyu Mi, & Jieshan Qiu. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c02124
IEEE [1] Liheng Xie, Yuexin Liang, Zhiyu Wang, Wentao Zhang, Fengjiao Guo, Xiaqing Chang, Hongyu Mi, and Jieshan Qiu, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c02124. keywords: {Znion hybrid supercapacitors;polyzwitterionic hydrogel electrolyte;Zn anode issues;dendrite inhibition;side reaction suppression}