daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Phase Structure and Hydrogen Storage Properties of Yttrium-Nickel-Based Alloys with Different Stoichiometric Ratio AITranslate

1.National Engineering Research Center of Nonferrous Metals Materials and Products for New Energy,GRINM Group Co.,Ltd.,100088,China
2.GRIMAT Engineering Institute Co.,Ltd.,101407,China
3.General Research Institute for Nonferrous Metals,Beijing 100088,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hydrogen is an ideal secondary energy source,with high energy density,zero carbon emission,and a wide range of sources. Efficient and safe hydrogen storage materials are one of the keys to enabling hydrogen energy applications. Rare earth-based hydrogen storage alloys have the advantages of high volumetric hydrogen storage density,superior kinetic,and moderate temperature for hydrogen absorption and desorption. Due to the structural limitations,the actual hydrogen storage capacity of the commercialized AB5 type alloy is close to the theoretical hydrogen storage capacity of 1.4%. The hydrogen storage capacity of rare earth alloys should be further improved to meet practical application needs. In recent years,rare earth AB2 type hydrogen storage alloys with large theoretical hydrogen storage capacity (>2.0%) are a class of promising hydrogen storage materials. However,the structures of rare earth AB2 alloys are prone to occur hydrogen-induced amorphization and disproportionation after hydrogen absorption and desorption. Compared with other rare earth AB2 alloys,YNi2 alloy has a smaller relative molecular mass and a smaller atomic radius ratio (RA/RB),but YNi2 alloy can only form crystalline Y0.95Ni2H2.6 (1.27%). Hydrogen-induced amorphization can occur when more hydrogen atoms are absorbed,and adjusting the stoichiometric ratio of alloys is a common method to improve the hydrogen storage properties of the rare earth hydrogen storage alloys. By this method,the unit cell volume of the alloys will change due to the change of the atomic ratio and a second phase may also be formed,which can improve the hydrogen storage capacity and plateau characteristics of the alloys. At present,the effect of stoichiometric ratio on the structure and hydrogen storage performance of the yttrium-nickel-based alloys has not been investigated. In this study,YNix (x=1.9,2.1,2.3,2.5) alloys were prepared by magnetic induction melting under Ar atmosphere from high purity metals Y (99.5%) and Ni (99.9%). After melting,the alloys were wrapped in tantalum foil and then placed in an argon filled quartz tube for step annealing. The annealing process was carried out at 600 ℃ for 6 h,750 ℃ for 6 h,850 ℃ for 12 h,750 ℃ for 60 h then cooled down with the furnace. The heating rates were 5 ℃·min−1 below 600 ℃·and 1 ℃·min−1 above 600 ℃. The influence of stoichiometric ratio x on the phase structure and hydrogen storage properties of the alloys was investigated by X-ray diffractometer (XRD),electron probe micro analysis (EPMA) and Sievert's methods. It was found that with the increase of the stoichiometric ratio x from 1.9 to 2.5,YNi phase in the alloy disappeared,the abundance of Y0.95Ni2 phase gradually decreased,and YNi3 phase appeared and gradually increased. When x=2.5,the abundance of YNi3 phase reached to 92.85%. The hydrogen storage performance showed that with the increase of the stoichiometric ratio,the hydrogen absorption rate of the alloy was gradually accelerated due to the increase of Ni content and phase boundary,which could improve the diffusion rate of hydrogen on the surface and interior of the alloy. With the increase of the stoichiometric ratio x,the capacity decay in the first four cycles of the alloys gradually decreased because the abundance of Y0.95Ni2 phase that was prone to occur amorphization and disproportionation in the alloys gradually decreased. When x=2.5,the abundance of YNi3 phase in the alloy were greater than 90%,and the hydrogen storage capacity did not decay. The stable hydrogen absorption capacity of the alloys increased also due to the decrease of the Y0.95Ni2 phase abundance. YNi2.5 alloy showed the maximum stable hydrogen absorption capacity of 1.716%. Pressure-capacity-temperature (PCT) curves of the alloys showed that the reversible hydrogen absorption and desorption performance of the alloys were improved by increasing the stoichiometric ratio. When x=1.9 and 2.1,the PCT curves of the alloy did not show plateau for hydrogen absorption and desorption. When x=2.3 and 2.5,PCT curves exhibited a double plateau for hydrogen absorption and desorption. Since the main phase in the alloy was YNi3 phase,the plateau characteristic of PCT curves were like that of YNi3 alloy. The plateau pressures of the hydrogen absorption curve were 0.0035 and 0.50 MPa,respectively. The structural changes of the alloys before and after hydrogen absorption and desorption show that the capacity attenuation of YNix (x=1.9,2.1,2.3,2.5) alloys were mainly due to the disproportionation of Y0.95Ni2 phase to form YNi3 phase YH2 phase. YNi3 phase structure did not change after hydrogen absorption and desorption,and could stably absorb and desorb hydrogen. The above results indicated that the increase of the stoichiometric ratio could significantly improve the hydrogen absorption and desorption capacity and the reversible hydrogen storage capacity of yttrium-nickel-based alloys. In the following research,it will be continued to increase the stoichiometric ratio and optimize alloy composition in order to further increase the hydrogen storage capacity and improve the plateau characteristics.

KeyWords AITranslate

yttrium-nickel-based alloy stoichiometric ratio hydrogen storage performance phase structure

[1]罗龙,吴文远,边雪,李培玉,齐健博. 基于AB5合金复合贮氢材料的研究进展[J].稀有金属,2018,42(5):546.

L Luo,W Y Wu,X Bian,P Y Li,J B Qi. Research progress of composite hydrogen storage materials based on AB5 alloy[J].Chinese Journal of Rare Metals,2018,42(5):546.

[2]Rusman N A A,Dahari M. A review on the current progress of metal hydrides material for solid-state hydrogen storage applications [J].International Journal of Hydrogen Energy,2016,41:12108.

[3]Ouyang L Z,Huang J L,Wang H,Liu J W,Zhu M. Progress of hydrogen storage alloys for Ni-MH rechargeable power batteries in electric vehicles:a review[J].Materials Chemistry and Physics,2017,200:164.

[4]孙如梦,周礼菊,司大强,黄瑶,王雷刚. 基于DEFORM-3D的新能源电池壳底部台阶镦挤成形工艺改进与优化 [J].锻压技术,2023,48(9):1.

R M Sun,L J Zhou,D Q Si,Y Huang,L G Wang. Improvement and optimization on upset-extrusion forming process for bottom step of new energy battery shell based on DEFORM-3D [J].Forging & Stamping Technology,2023,48(9):1.

[5]胡娅琪,张博,姚琳,秦蓓. 无电沉积法制备硼掺杂石墨烯负载钯纳米颗粒催化剂及对过氧化氢的电化学检测 [J].分析试验室,2022,41(9):106.

Y Q Hu,B Zhang,L Yao,B Qin. Pd nanoparticles on boron doped graphene catalyst for electrochemical detection of hydrogen peroxide prepared by electroless deposition method[J].Chinese Journal of Analysis Laboratory,2022,41(9):1065.

[6]王步祥,舒庆. 单原子电催化析氢催化剂的研究进展 [J].有色金属科学与工程,2022,13(5):92.

B X Wang,Q Shu. Research progress in single-atomic electrocatalytic hydrogen evelution reaction catalyst [J].Nonferrous Metals Science and Engineering,2022,13(5):92.

[7]丁奔,蔡军,张兵,陈琳,赵谦. GH4169稀土强化镍基高温合金热变形行为 [J].塑性工程学报,2023,30(9):131.

B Ding,J Cai,B Zhang,L Chen,Q Zhao. Hot deformation behavior of GH4169 rare earth reinforced Ni-base superalloy [J].Journal of Plasticity Engineering,2023,30(9):131.

[8]Liu J J,Li Y,Han D,Yang S Q,Chen X C,Zhang L,Han S M. Electrochemical performance and capacity degradation mechanism of single-phase La-Mg-Ni-based hydrogen storage alloys [J].Journal of Power Sources,2015,300:77.

[9]Xin G B,Yuan H P,Yang K,Jiang L J,Liu X P,Wang S M. Investigation of the capacity degradation mechanism of La-Mg-Ca-Ni AB3-type alloy [J].International Journal of Hydrogen Energy,2016,41(46):21261.

[10]李学军,崔舜,周增林,宋月清,林晨光,黄长庚,钱文连. 稀土(镁)系AB2型贮氢合金的研究进展[J].材料导报,2008,7:77.

X J Li,S Cui,Z L Zhou,Y Q Song,C G Lin,C G Huang,W L Qian. Research development of RE-(Mg)-system AB2-type hydrogen storage alloys[J].Materials Reports,2008,7:77.

[11]Gschneidner K A,Pecharsky V K. Binary rare earth Laves phases-an overview [J].Z Kristallogr,2006,221(5-7):375.

[12](邓凡锋,邓文清,张婷,王维康,刘洪刚,陈林,李浩,潘义,方正. 在线稀释-傅里叶变换红外光谱法用于质子交换膜燃料电池汽车用氢燃料中微痕量杂质组分的快速分析[J].分析试验室,2023,42(3):312.)

F F Deng,W Q Deng,T Zhang,W K Wang,H G Liu,L Chen,H Li,Y Pan,Z Fang. Rapid analysis of impurity components in fuel hydrogen for proton exchange membrane fuel cell vehicle using on-line dilution-Fourier transform infrared spectroscopy method[J].Chinese Journal of Analysis Laboratory,2023,42(3):312.

[13]Ivey D G,Northwood D O. Storing hydrogen in AB2 Laves-type compounds[J].Z Phys Chem Neue Fol.,1986,147:191.

[14]Funaki K,Orimo S,Fujii H. Hydrogen-induced amorphization of YNi2 enhanced by mechanical grinding[J].Journal of Alloys and Compounds,1997,253:110.

[15]Li P,Zhai F,Wan Q,Zhao K,Li Z,Volinsky A A,Qu X H. Study of the hydrogen-induced amorphization in the LaNi2.28 alloy[J].RSC Advances,2014,4:267.

[16]Aoki K,Li X G,Masumoto T. Factors controlling hydrogen-induced amorphization of C15 Laves compounds [J].Acta Metallurgica et Materialia,1992,40(7):1717.

[17]Shen H,Paul-Boncour V,Latroche M,Cuevas F,Li P,Yuan H P,Li Z N,Zhang J X,Jiang L J. Investigation of the phase occurrence and H sorption properties in the Y33.33Ni66.67-xAlx (0≤x≤33.33) system[J].Journal of Alloys and Compounds,2021,888:161375.

[18]Suzuki K,Lin X. Local structure evolution in hydrogen-induced amorphization of YFe2 and YNi2 Laves phases [J].Journal of Alloys and Compounds,1993,193(1):7.

[19]杨康,蒋利军,苑慧萍,辛恭标,万 琦,赵旭山. Ce替代Y对Y1-xCexFe2 (x=0,0.15,0.25和0.50)合金吸氢性能的影响[J].稀有金属,2017,41(11):1202.

K Yang,L J Jiang,H P Yuan,G B Xin,Q Wan,X S Zhao. Hydrogen absorption property of Y1-xCexFe2 (x=0,0.15,0.25 and 0.50) alloys with Ce substitution for Y[J].Chinese Journal of Rare Metals,2017,41(11):1202.

[20]Dilixiati M,Kanda K,Ishikawa K,Aoki K. Hydrogen-induced amorphization in C15 Laves phases RFe2[J].Journal of Alloys and Compounds,2002,337:128.

[21]Aono K,Orimo S,Fujii H. Structural and hydriding properties of MgYNi4:a new intermetallic compound with C15b-type Laves phase structure [J].Journal of Alloys and Compounds,2000,309(1-2):L1.

[22]Zhao S Q,Wang H,Liu J W. Exploring the hydrogen-induced amorphization and hydrogen storage reversibility of Y(Sc)0.95Ni2 Laves phase compounds [J].Materials,2021,14(2):276.

[23]Li Z M,Wang H,Ouyang L Z,Liu J W,Zhu M. Reversible hydriding in YFe2-xAlx (x=0.3,0.5,0.7) intermetallic compounds [J].Journal of Alloys and Compounds,2016,689:843.

[24]陈瑜竹. 合金化方法调控YFe2型储氢合金的相结构与储氢特性 [D].广州:华南理工大学,2020. 57.

Y Z Chen. Alloying Substitution Tuning the Phase Structure and Hydrogen Storage Characteristics of YFe2 Hydrogen Storage Alloy [D].Guangzhou:South China University of Technology,2020. 57.

[25]Li Z M,Wang H,Ouyang L Z,Liu J W,Zhu M. Increasing de-/hydriding capacity and equilibrium pressure by designing non-stoichiometry in Al-substituted YFe2 compounds[J].Journal of Alloys and Compounds,2017,704:491.

[26]Zhang Y H,Zhao D L,Li B W,Zhao X L,Wu Z W,Wang X L. Microstructures and electrochemical characteristics of the La0.75Mg0.25Ni2.5Mx (M=Ni,Co;x=0-1.0) hydrogen storage alloys [J].International Journal of Hydrogen Energy,2008,33(7):1868.

[27]Blach T P,Gray E M. Sieverts apparatus and methodology for accurate determination of hydrogen uptake by light-atom hosts [J].Journal of Alloys and Compounds,2007,446-447:692.

[28]Rodríguez-Carvajal J. Recent advances in magnetic structure determination by neutron powder diffraction[J].Physica B:Condensed Matter,1993,192:55.

[29]Latroche M,PaulboncourA V,Percheronguegan A. Structural instability in R1-xNi2 compounds and their hydrides (R=Y,rare-earth) [J].Z Phys Chem,1993,179:261.

[30]Zhang J L,Han S M,Li Y,Liu J J,Yang S Q,Zhang L,Wang J D. Effects of PuNi3- and Ce2Ni7-type phase abundance on electrochemical characteristics of La-Mg-Ni-based alloys[J].Journal of Alloys and Compounds,2013,581:693.

[31]王浩,罗永春,邓安强,赵磊,姜婉婷. 退火温度对无镁La-Y-Ni系A2B7型合金相结构和电化学性能的影响[J].无机材料学报,2018,33(4):434.

H Wang,Y C Luo,A Q Deng,L Zhao,W T Jiang. Annealing temperature on structural and electrochemical property of Mg-free La-Y-Ni based A2B7-type hydrogen storage alloys[J].Journal of Inorganic Materials,2018,33(4):434.

[32]Zhang Y H,Li Y Q,Shang H W,Yuan Z M,Yang T,Guo S H. Structures and hydrogen storage performances of rare earth-Mg-Ni-Mn-based AB2-type alloys applied to Ni-MH battery[J].Journal of Solid State Electrochemistry,2017,21:1015.

[33]郭淼,苑慧萍,刘彧儒,蒋利军. AB3.3~3.7型La-Y-Ni稀土储氢合金微观结构和电化学性能研究[J].稀有金属,2023,47(2):210.

M Guo,H P Yuan,Y R Liu,L J Jiang. Study on the microstructure and electrochemical properties of AB3.3~3.7-type La-Y-Ni rare earth storage alloys[J].Chinese Journal of Rare Metals,2023,47(2):210.

[34]Vanessen R H,Buschow K H J. Hydrogen sorption characteristics of Ce-3d and Y-3d intermetallic compounds[J].Journal of the Less Common Metals,1980,70:189.

[35]Bobet J L,Chevalier B,Song M Y,Darriet B,Etourneau J. Reactive mechanical grinding of magnesium in hydrogen and the effects of additives[J].Mater Manuf Process,2002,17,351.

[36]Fu K,Jiang X J,Guo Y R,Li S,Zheng J,Tian W H,Li X G. Experimental investigation and thermodynamic assessment of the yttrium-hydrogen binary system[J].Progress in Natural Science:Materials International,2018,28(3):332.

[37]Begun G M,Land J F,Bell J T. High temperature equilibrium measurements of the yttrium-hydrogen isotope (H2,D2,T2) systems[J].The Journal of Chemical Physics,1980,72(5):2959.

[38]Zhang J,Zhou G,Chen G,Latroche M,Percheron-Guégan A,Sun D. Relevance of hydrogen storage properties of ANi3 intermetallics (A=La,Ce,Y) to the ANi2 subunits in their crystal structures[J].Acta Materialia,2008,56:5388.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY22030010

Chinese Library Classification Number:TG139+.7

Citation Information:

Hydrogen is an ideal secondary energy source,with high energy density,zero carbon emission,and a wide range of sources. Efficient and safe hydrogen storage materials are one of the keys to enabling hydrogen energy applications. Rare earth-based hydrogen storage alloys have the advantages of high volumetric hydrogen storage density,superior kinetic,and moderate temperature for hydrogen absorption and desorption. Due to the structural limitations,the actual hydrogen storage capacity of the commercialized AB5 type alloy is close to the theoretical hydrogen storage capacity of 1.4%. The hydrogen storage capacity of rare earth alloys should be further improved to meet practical application needs. In recent years,rare earth AB2 type hydrogen storage alloys with large theoretical hydrogen storage capacity (>2.0%) are a class of promising hydrogen storage materials. However,the structures of rare earth AB2 alloys are prone to occur hydrogen-induced amorphization and disproportionation after hydrogen absorption and desorption. Compared with other rare earth AB2 alloys,YNi2 alloy has a smaller relative molecular mass and a smaller atomic radius ratio (RA/RB),but YNi2 alloy can only form crystalline Y0.95Ni2H2.6 (1.27%). Hydrogen-induced amorphization can occur when more hydrogen atoms are absorbed,and adjusting the stoichiometric ratio of alloys is a common method to improve the hydrogen storage properties of the rare earth hydrogen storage alloys. By this method,the unit cell volume of the alloys will change due to the change of the atomic ratio and a second phase may also be formed,which can improve the hydrogen storage capacity and plateau characteristics of the alloys. At present,the effect of stoichiometric ratio on the structure and hydrogen storage performance of the yttrium-nickel-based alloys has not been investigated. In this study,YNix (x=1.9,2.1,2.3,2.5) alloys were prepared by magnetic induction melting under Ar atmosphere from high purity metals Y (99.5%) and Ni (99.9%). After melting,the alloys were wrapped in tantalum foil and then placed in an argon filled quartz tube for step annealing. The annealing process was carried out at 600 ℃ for 6 h,750 ℃ for 6 h,850 ℃ for 12 h,750 ℃ for 60 h then cooled down with the furnace. The heating rates were 5 ℃·min−1 below 600 ℃·and 1 ℃·min−1 above 600 ℃. The influence of stoichiometric ratio x on the phase structure and hydrogen storage properties of the alloys was investigated by X-ray diffractometer (XRD),electron probe micro analysis (EPMA) and Sievert's methods. It was found that with the increase of the stoichiometric ratio x from 1.9 to 2.5,YNi phase in the alloy disappeared,the abundance of Y0.95Ni2 phase gradually decreased,and YNi3 phase appeared and gradually increased. When x=2.5,the abundance of YNi3 phase reached to 92.85%. The hydrogen storage performance showed that with the increase of the stoichiometric ratio,the hydrogen absorption rate of the alloy was gradually accelerated due to the increase of Ni content and phase boundary,which could improve the diffusion rate of hydrogen on the surface and interior of the alloy. With the increase of the stoichiometric ratio x,the capacity decay in the first four cycles of the alloys gradually decreased because the abundance of Y0.95Ni2 phase that was prone to occur amorphization and disproportionation in the alloys gradually decreased. When x=2.5,the abundance of YNi3 phase in the alloy were greater than 90%,and the hydrogen storage capacity did not decay. The stable hydrogen absorption capacity of the alloys increased also due to the decrease of the Y0.95Ni2 phase abundance. YNi2.5 alloy showed the maximum stable hydrogen absorption capacity of 1.716%. Pressure-capacity-temperature (PCT) curves of the alloys showed that the reversible hydrogen absorption and desorption performance of the alloys were improved by increasing the stoichiometric ratio. When x=1.9 and 2.1,the PCT curves of the alloy did not show plateau for hydrogen absorption and desorption. When x=2.3 and 2.5,PCT curves exhibited a double plateau for hydrogen absorption and desorption. Since the main phase in the alloy was YNi3 phase,the plateau characteristic of PCT curves were like that of YNi3 alloy. The plateau pressures of the hydrogen absorption curve were 0.0035 and 0.50 MPa,respectively. The structural changes of the alloys before and after hydrogen absorption and desorption show that the capacity attenuation of YNix (x=1.9,2.1,2.3,2.5) alloys were mainly due to the disproportionation of Y0.95Ni2 phase to form YNi3 phase YH2 phase. YNi3 phase structure did not change after hydrogen absorption and desorption,and could stably absorb and desorb hydrogen. The above results indicated that the increase of the stoichiometric ratio could significantly improve the hydrogen absorption and desorption capacity and the reversible hydrogen storage capacity of yttrium-nickel-based alloys. In the following research,it will be continued to increase the stoichiometric ratio and optimize alloy composition in order to further increase the hydrogen storage capacity and improve the plateau characteristics.

quote

GB/T 7714-2015 [1] Zhenyu Hou, Huiping Yuan, Yuru Liu, et al. Phase Structure and Hydrogen Storage Properties of Yttrium-Nickel-Based Alloys with Different Stoichiometric Ratio[J]. Chinese Journal of Rare Metals, 2024, 48(12): 1671-1680. DOI:10.13373/j.cnki.cjrm.XY22030010.
MLA [1] Zhenyu Hou, et al., "Phase Structure and Hydrogen Storage Properties of Yttrium-Nickel-Based Alloys with Different Stoichiometric Ratio." Chinese Journal of Rare Metals, vol. 48, no. 12, 2024, pp. 1671-1680, https://doi.org/10.13373/j.cnki.cjrm.XY22030010.
APA [1] Zhenyu Hou, Huiping Yuan, Yuru Liu, Hao Shen, Zhinian Li, & Lijun Jiang. (2024). Phase Structure and Hydrogen Storage Properties of Yttrium-Nickel-Based Alloys with Different Stoichiometric Ratio. Chinese Journal of Rare Metals, 48(12), 1671-1680. https://doi.org/10.13373/j.cnki.cjrm.XY22030010
IEEE [1] Zhenyu Hou, Huiping Yuan, Yuru Liu, Hao Shen, Zhinian Li, and Lijun Jiang, "Phase Structure and Hydrogen Storage Properties of Yttrium-Nickel-Based Alloys with Different Stoichiometric Ratio," Chinese Journal of Rare Metals, vol. 48, no. 12, pp. 1671-1680, 2024, doi: 10.13373/j.cnki.cjrm.XY22030010. keywords: {yttrium-nickel-based alloy;stoichiometric ratio;hydrogen storage performance;phase structure}