Preparation of High Pure Tungsten Trioxide by Method of Activated Carbon Absorption and Ethandiol Purification AITranslate
Abstract AITranslate
Ammonium tungstate is made from scheelite by acid dissolution. Then ammonium tungstate is obsorbed by activated carbon at pH 1 .8 and absolved at strong base. Tungstic acid is precipitated at pH1.Tungstic acid is then dissolved in hot ethandiol and it is reprecipitated under HC1 condition. The purified precipitate burns at elevated temperature and high pure tungsten trioxide can be obtained. Tungsten trioxide is 99. 9% (by scanning electron microscopy, ICP, photometric analysis).This method has the advantages of simple operation, easy post treatment and improved efficiency over the ion exchange or solvent extraction method.
KeyWords AITranslate
1胡习茹.用苯胺萃取法分离三氧化钨中的钼[J].黎明化工,1996(2):27-28. 被引量:2
2杨建安,文焱炳.磷酸清洁工艺中溶剂萃取净化法的研究进展[J].精细与专用化学品,2010,18(8):33-36. 被引量:1
3Sherif,M,李金平.室温下还原WO3合成全密实纳米晶WC[J].国外金属加工,1998(2):17-20.
4冯斌.新戊二醇的净化法[J].甲醛与甲醇,2001(3):12-16.
5曹小华,黎先财,陶春元,赵文杰,谢宝华.过氧化氢氧化环己酮绿色合成己二酸[J].化工中间体,2006,2(11):29-32. 被引量:4
6王岭,张文辉,李书荣.测定活性炭吸附甲苯等温线的试验方法[J].林产化工通讯,2002,36(4):19-22.
7二氟甲烷净化法[J].甲醛与甲醇,2003(2):44-44.
8施立钦.工业废渣氯化钠的综合利用[J].宁波职业技术学院学报,2005,9(2):87-89. 被引量:7
9王建华,丁文光,周建平,菅秀君.环戊烯催化氧化合成戊二醛[J].化工进展,2002,21(4):259-261. 被引量:4
10氟氯烃的净化法[J].甲醛与甲醇,2002(6):40-41.
Basic Information:
DOI:
Chinese Library Classification Number:TQ136.13[化学工程—无机化工]
Citation Information:
Ammonium tungstate is made from scheelite by acid dissolution. Then ammonium tungstate is obsorbed by activated carbon at pH 1 .8 and absolved at strong base. Tungstic acid is precipitated at pH1.Tungstic acid is then dissolved in hot ethandiol and it is reprecipitated under HC1 condition. The purified precipitate burns at elevated temperature and high pure tungsten trioxide can be obtained. Tungsten trioxide is 99. 9% (by scanning electron microscopy, ICP, photometric analysis).This method has the advantages of simple operation, easy post treatment and improved efficiency over the ion exchange or solvent extraction method.
quote
| GB/T 7714-2015 | [1] ZHANG Yong-an, ZHANG Wen-pu, TAN Gui-ning, et al. Preparation of High Pure Tungsten Trioxide by Method of Activated Carbon Absorption and Ethandiol Purification[J]. Rare Metals and Cemented Carbides, 1994(3): 6-10. |
| MLA | [1] ZHANG Yong-an, et al., "Preparation of High Pure Tungsten Trioxide by Method of Activated Carbon Absorption and Ethandiol Purification." Rare Metals and Cemented Carbides, no. 3, 1994, pp. 6-10. |
| APA | [1] ZHANG Yong-an, ZHANG Wen-pu, TAN Gui-ning, & ZHAO Hui-chun. (1994). Preparation of High Pure Tungsten Trioxide by Method of Activated Carbon Absorption and Ethandiol Purification. Rare Metals and Cemented Carbides(3), 6-10. |
| IEEE | [1] ZHANG Yong-an, ZHANG Wen-pu, TAN Gui-ning, and ZHAO Hui-chun, "Preparation of High Pure Tungsten Trioxide by Method of Activated Carbon Absorption and Ethandiol Purification," Rare Metals and Cemented Carbides, no. 3, pp. 6-10, 1994. keywords: {absorption, activated carbon, ethandiol, tungstic acid,tungsten trioxide.} |