Effect of Raw Materials of Tungsten Oxide on the Particle Size of Tungsten Powder AITranslate

Department of Metallurgical, Central South China University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The raw materials of various tungsten oxides strongly affect the particle size of tungsten powder. Therefore, it is highly important to make the right production and choice of the tungsten raw material in the production of tungsten powder. The fine tungsten powder has been effectively obtained by hydrogen reduction of purple tungsten oxide.

KeyWords AITranslate

tungsten oxide tungsten powder particle size.

1罗斌辉,张华明.生产优质粗颗粒WC的工艺研究[J].稀有金属与硬质合金,2008,36(1):38-41. 被引量:1

2彭卫珍.蓝钨物理性能对钨粉和碳化钨粉性能的影响[J].硬质合金,2004,21(3):142-148. 被引量:7

3陈树茂,廖小英,张秋和,熊小明,王文华,袁宜红.传统流程生产超细钨粉的工艺优化[J].中国钨业,2005,20(2):36-39. 被引量:5

4吴晓东,柴永新,傅明喜.蓝钨氢还原工艺及其还原机理的探讨[J].硬质合金,2005,22(2):65-68. 被引量:6

5罗斌辉,张华明.不同氧化钨原料对钨粉性能的影响研究[J].硬质合金,2006,23(3):139-142. 被引量:14

6徐迎春,姜萍.紫色氧化钨的生产、检测及应用[J].江西冶金,2007,27(3):29-31. 被引量:2

7陈绍衣.用W_(18)O_(49)制造超细钨粉及超细碳化钨粉[J].中南工业大学学报,1997,28(5):456-460. 被引量:14

8杨安享,李洪桂,赵中伟.AH法制备钨粉过程中钨粉粒度的控制研究[J].中国钨业,2008,23(4):31-34.

9晏慧娟,熊艰.传统流程制备超细钨粉的研究进展[J].上饶师范学院学报,2008,28(3):50-54. 被引量:3

10张立,吴冲浒,文晓,吴厚平,熊湘君.从硬质合金典型材质发展看中国硬质合金工业的技术进步[J].中国钨业,2011,26(4):34-39. 被引量:11

1丁辉,李潇.碳化钨、碳化钼的制取及研究进展[J].产业科技创新,2020(15):37-38.

2张冬梅,王文华.扫描电镜在钨制品生产中的应用[J].江西有色金属,2005,19(1):41-44.

3陈树茂,廖小英,张秋和,熊小明,王文华,袁宜红.传统流程生产超细钨粉的工艺优化[J].中国钨业,2005,20(2):36-39. 被引量:5

4吴晓东,柴永新,傅明喜.蓝钨氢还原工艺及其还原机理的探讨[J].硬质合金,2005,22(2):65-68. 被引量:6

5罗斌辉,张华明.不同氧化钨原料对钨粉性能的影响研究[J].硬质合金,2006,23(3):139-142. 被引量:14

6孙晓昱,陆金生.氧化钨的状态分析[J].科学技术与工程,2007,7(1):36-40. 被引量:2

7刘清才,王海波,孙亚丽.以紫钨为原料制备优质超细WC粉末的实验[J].重庆大学学报:自然科学版,2007,30(5):100-102. 被引量:4

8徐迎春,姜萍.紫色氧化钨的生产、检测及应用[J].江西冶金,2007,27(3):29-31. 被引量:2

9孙亚丽.以紫钨为原料制备超细WC-Co硬质合金[J].中国钨业,2007,22(5):27-29. 被引量:7

10黄道远,易丹青,刘瑞,李荐.从APT到纳米WC的形貌结构演变[J].硬质合金,2007,24(4):203-206. 被引量:2

1廖寄乔,肖彩林,黄志锋.氧化钨相成分对超细钨粉均匀性的影响[J].粉末冶金材料科学与工程,2000,5(1):39-43. 被引量:1

2罗斌辉,张华明.不同氧化钨原料对钨粉性能的影响研究[J].硬质合金,2006,23(3):139-142. 被引量:14

3廖寄乔,唐美英.氧化钨相成分对超细钨粉均匀性的影响[J].稀有金属材料与工程,2001,30(6):453-456. 被引量:23

4廖寄乔,黄志锋,肖彩林.超细钨粉的制取及其氧化钨原料和钨粉的粒度测量[J].粉末冶金材料科学与工程,1999,4(4):322-329. 被引量:2

5廖寄乔,石刚,王华.超细钨粉的制取及其氧化钨原料和钨粉的粒度测量[J].理化检验:物理分册,2002,38(8):337-341. 被引量:11

6钟毓斌,孙娟,涂洁,郝立伟.超细、纳米晶硬质合金的原料制备研究[J].中国钨业,2016,31(6):35-40. 被引量:6

7陈树茂,廖小英,张秋和,熊小明,王文华,袁宜红.传统流程生产超细钨粉的工艺优化[J].中国钨业,2005,20(2):36-39. 被引量:5

8林高安.钨粉形貌与粒度分布对成形性和压坯强度的影响[J].粉末冶金材料科学与工程,2009,14(4):260-264. 被引量:30

Basic Information:

DOI:

Chinese Library Classification Number:TF123.24[冶金工程—粉末冶金]

Citation Information:

The raw materials of various tungsten oxides strongly affect the particle size of tungsten powder. Therefore, it is highly important to make the right production and choice of the tungsten raw material in the production of tungsten powder. The fine tungsten powder has been effectively obtained by hydrogen reduction of purple tungsten oxide.

quote

GB/T 7714-2015 [1] CHEN Shao-yi. Effect of Raw Materials of Tungsten Oxide on the Particle Size of Tungsten Powder[J]. Rare Metals and Cemented Carbides, 1994(3): 10-14.
MLA [1] CHEN Shao-yi. "Effect of Raw Materials of Tungsten Oxide on the Particle Size of Tungsten Powder." Rare Metals and Cemented Carbides, no. 3, 1994, pp. 10-14.
APA [1] CHEN Shao-yi. (1994). Effect of Raw Materials of Tungsten Oxide on the Particle Size of Tungsten Powder. Rare Metals and Cemented Carbides(3), 10-14.
IEEE [1] CHEN Shao-yi, "Effect of Raw Materials of Tungsten Oxide on the Particle Size of Tungsten Powder," Rare Metals and Cemented Carbides, no. 3, pp. 10-14, 1994. keywords: {tungsten oxide, tungsten powder, particle size.}