Research on Kinetics of Oxidation Leaching of Stone Coal Vanadium Ore by Manganese Dioxide AITranslate

College of Chemistry and Chemical Engineering,Jishou University;College of Chemistry and Chemical Engineering,Jishou University;College of Chemistry and Chemical Engineering,Jishou University;College of Chemistry and Chemical Engineering,Jishou University;College of Chemistry and Chemical Engineering,Jishou University;College of Chemistry and Chemical Engineering,Jishou University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The manganese dioxide was used to oxidize and leach vanadium from raw material of the stone coal vanadium ore from Zhangjiajie.The effects of MnO2dosage,liquid-solid ratio,leaching time,H2SO4 dosage and leaching temperature on vanadium leaching rate were investigated.The results show that the leaching rate of vanadium reaches 94.17%under the conditions as follows:MnO2dosage of 3%,liquid-solid ratio of 0.8∶1,H2SO4dosage of 35%,leaching temperature of 95℃and leaching time of 10h.The vanadium leaching rate Rhas a good linear relationship with the leaching time t in the form of 1-(1-R)1/3.The apparent activation energy of the leaching reaction is approximately 54.62kJ/mol according to the Arrhenius equation,indicating that the reaction is controlled by a chemical reaction.

KeyWords AITranslate

stone coal vanadium ore oxidization leaching MnO2 vanadium leaching rate kinetics

1郑琍玉,于少明,刘彬,陈亮,黄伶俐.石煤提钒碱浸过程动力学研究[J].稀有金属,2011,35(1):101-105. 被引量:21

2黄晓毅,马玄恒,高爱民,罗小新.石煤提钒工艺研究进展[J].甘肃冶金,2010,32(4):27-29. 被引量:5

3戴子林,张恩普.从石煤钒矿中浸钒技术的研究现状[J].矿冶工程,2015,35(6):85-88. 被引量:17

4陈放,张一敏,黄晶,刘涛,薛楠楠.二氧化锰对石煤提钒直接酸浸的影响[J].化工进展,2017,36(3):1126-1133. 被引量:12

5杨大锦,廖元双,刘瑜.石煤钒矿提钒新工艺研究[J].云南冶金,2014,43(1):41-44. 被引量:7

6陈庆根.石煤钒矿提钒工艺技术的研究进展[J].矿产综合利用,2009(2):30-34. 被引量:35

7高峰,石美莲,周再兴,华骏,颜文斌.湘西含钒石煤提钒工艺研究[J].矿冶工程,2011,31(3):93-96. 被引量:10

8李莹,颜文斌,华骏,方玉,刘阳文.软锰矿氧化石煤钒矿的湿法浸出研究[J].应用化工,2013,42(7):1170-1173. 被引量:9

9蒋京航,叶国华,张世民,张爽.石煤直接酸浸提钒工艺研究进展[J].矿冶,2016,25(6):35-39. 被引量:12

10杜军,王娜,陶长元,刘作华,范兴.石煤矿氧化焙烧料酸浸过程的动力学[J].化工进展,2010,29(S1):491-493. 被引量:3

1周思雨,兰帅,赖发英,刘凡,秦张杰.钒(V^(3+))与水钠锰矿共沉淀的相互作用及对Pb^(2+)和Zn^(2+)的去除研究[J].江西农业大学学报,2021,43(6):1423-1431.

2曹欢,吴天骄,程倩,宁新霞,赵笑益.硅质钒矿硫酸熟化常温水浸提钒[J].有色金属:冶炼部分,2022(1):67-72.

1叶国华,谢禹,胡艺博,左琪,乔吉波,童雄.低品位石煤钒矿低温硫酸化焙烧-水浸提钒研究[J].稀有金属,2020,44(7):753-761. 被引量:16

2隋丽丽,张俊,马明阳,翟玉春,董微,常红.浓硫酸焙烧钛渣后的滤渣碱浸动力学研究[J].稀有金属与硬质合金,2020,48(6):20-23. 被引量:1

3凡杰,谢刚,田林,李小英,王冰冰,朱炳桥.闪锌矿加压酸浸工艺及动力学试验研究[J].湿法冶金,2020,39(6):483-489. 被引量:8

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

The manganese dioxide was used to oxidize and leach vanadium from raw material of the stone coal vanadium ore from Zhangjiajie.The effects of MnO2dosage,liquid-solid ratio,leaching time,H2SO4 dosage and leaching temperature on vanadium leaching rate were investigated.The results show that the leaching rate of vanadium reaches 94.17%under the conditions as follows:MnO2dosage of 3%,liquid-solid ratio of 0.8∶1,H2SO4dosage of 35%,leaching temperature of 95℃and leaching time of 10h.The vanadium leaching rate Rhas a good linear relationship with the leaching time t in the form of 1-(1-R)1/3.The apparent activation energy of the leaching reaction is approximately 54.62kJ/mol according to the Arrhenius equation,indicating that the reaction is controlled by a chemical reaction.

quote

GB/T 7714-2015 [1] LI Li-jie, SHI Mei-lian, HUA Jun, et al. Research on Kinetics of Oxidation Leaching of Stone Coal Vanadium Ore by Manganese Dioxide[J]. Rare Metals and Cemented Carbides, 2020(6): 24-29.
MLA [1] LI Li-jie, et al., "Research on Kinetics of Oxidation Leaching of Stone Coal Vanadium Ore by Manganese Dioxide." Rare Metals and Cemented Carbides, no. 6, 2020, pp. 24-29.
APA [1] LI Li-jie, SHI Mei-lian, HUA Jun, YAN Wen-bin, GAO Feng, & HUANG Chao. (2020). Research on Kinetics of Oxidation Leaching of Stone Coal Vanadium Ore by Manganese Dioxide. Rare Metals and Cemented Carbides(6), 24-29.
IEEE [1] LI Li-jie, SHI Mei-lian, HUA Jun, YAN Wen-bin, GAO Feng, and HUANG Chao, "Research on Kinetics of Oxidation Leaching of Stone Coal Vanadium Ore by Manganese Dioxide," Rare Metals and Cemented Carbides, no. 6, pp. 24-29, 2020. keywords: {stone coal vanadium ore;oxidization leaching;MnO2;vanadium leaching rate;kinetics}