Research Progress in Zirconium Metallurgical Technology AITranslate
Abstract AITranslate
Zirconium is an indispensable structural material of nuclear reactors for its very low thermal neutron absorption cross section,which will not absorb and waste thermal neutrons during the nuclear reaction process.The production process of zirconium metal is mainly introduced.The advantages and disadvantages of such zirconium metal production methods as metal thermal reduction,molten salt electrolysis and thermal dissociation of zirconium iodide are compared and analyzed,and the development trend of zirconium metal production process is put forward.
KeyWords AITranslate
1杨锋,尉北玲,王旭峰.核级锆合金研究现状及我国核级锆材发展方向[J].金属世界,2016(3):24-28. 被引量:17
2郑明光,叶成,韩旭.新能源中的核电发展[J].核技术,2010,33(2):81-86. 被引量:40
3李岱松.海绵锆生产工艺的节能环保分析[J].资源节约与环保,2011,26(4):47-51. 被引量:3
4WU Yanke XU Zhigao CHEN Song WANG Lijun LI Guoxun.Electrochemical behavior of zirconium in molten NaCl-KCl-K_2ZrF_6 system[J].稀有金属:英文版,2011,30(1):8-13. 被引量:15
5叶奇蓁.中国核电发展战略研究[J].电网与清洁能源,2010,26(1):3-8. 被引量:50
6孙彦华,杨钢,周林,吴云峰.锆粉制备工艺的研究进展[J].云南冶金,2015,44(1):49-52. 被引量:7
7郭春芳,董云会,于先进,李德刚,张丽鹏.直接电脱氧法制备金属锆[J].中国有色金属学报,2007,17(6):1019-1023. 被引量:17
8刘美凤,卢世刚,阚素荣.熔盐电解固态氧化物制备难熔金属及合金的最新进展[J].稀有金属,2008,32(5):668-673. 被引量:7
9谢珊珊,李慧,张士宪,刘晓,霍东兴.金属锆的制备工艺[J].热加工工艺,2017,46(4):27-29. 被引量:4
10王峰,王快社,马林生,张兵,孔亮,林兆霞.核级锆及锆合金研究状况及发展前景[J].兵器材料科学与工程,2012,35(1):107-110. 被引量:29
1董朝望,赵金龙,夏阳,郭学益,刘汉宁.氢气辅助镁还原-烧结制备Zr-2.5Nb合金[J].中国有色金属学报,2022,32(11):3306-3314.
2何伟,马红征,苗壮,王松茂,杨军红.Zr-1锆锭缺陷形成原因[J].理化检验:物理分册,2023,59(3):28-30.
1叶俊良,柯智耀.应用Fe2O3和TiO2金属热还原进行添加TiB2和TiC的FeAl/Al2O3复合材料的燃烧合成[J].中国有色金属学报:英文版,2020,30(9):2510-2517. 被引量:2
2王天,王耀武,王宇,贺晓军.金属钛冶炼研究进展[J].中国有色冶金,2020,49(3):1-6. 被引量:7
3张利凡,丁满堂,何翠萍,林海,雷莹莹,何玉琼.含钛高炉渣火法提钛[J].中国资源综合利用,2020,38(10):94-96. 被引量:2
4沈自强,狄跃忠,彭建平,王耀武,冯乃祥.真空热还原法制备金属锂的研究进展[J].矿产保护与利用,2020,40(5):10-16.
5李红莉,张宇.不同制备工艺对金属钛粉微观性质及应用的影响研究[J].钛工业进展,2020,37(6):29-33. 被引量:1
6冉剑锋,吕鹏,姚家舒,李亚丽,张良静,尹少华,张利波.微波加热在稀土冶金与新材料合成的研究进展[J].矿产保护与利用,2020,40(5):37-43. 被引量:3
7徐晓辉,吴荣俊,李晓玲,李强,贾靖轩,陈艳,程翀.重金属-稀土高分子复合材料屏蔽性能的MCNP模拟[J].舰船科学技术,2020,42(11):72-75.
8王孝娃,杜宁,王岚.上海市质子碳离子放射治疗设施辐射源关键点分析[J].中国医疗器械杂志,2020,44(6):476-480. 被引量:3
9王珍,凌永一,王子昊,张婧,贾全利,刘新红.熔盐辅助法制备碳化钛材料的研究进展[J].工程科学学报,2021,43(1):97-107. 被引量:2
10郭珺文.浅谈金镶玉工艺嵌金银丝嵌宝石的历史及发展[J].文物鉴定与鉴赏,2020(20):102-103. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF841.4[冶金工程—有色金属冶金]
Citation Information:
Zirconium is an indispensable structural material of nuclear reactors for its very low thermal neutron absorption cross section,which will not absorb and waste thermal neutrons during the nuclear reaction process.The production process of zirconium metal is mainly introduced.The advantages and disadvantages of such zirconium metal production methods as metal thermal reduction,molten salt electrolysis and thermal dissociation of zirconium iodide are compared and analyzed,and the development trend of zirconium metal production process is put forward.
quote
| GB/T 7714-2015 | [1] ZHANG Kai, XU Liang. Research Progress in Zirconium Metallurgical Technology[J]. Rare Metals and Cemented Carbides, 2020(6): 30-37. |
| MLA | [1] ZHANG Kai, and XU Liang. "Research Progress in Zirconium Metallurgical Technology." Rare Metals and Cemented Carbides, no. 6, 2020, pp. 30-37. |
| APA | [1] ZHANG Kai, & XU Liang. (2020). Research Progress in Zirconium Metallurgical Technology. Rare Metals and Cemented Carbides(6), 30-37. |
| IEEE | [1] ZHANG Kai and XU Liang, "Research Progress in Zirconium Metallurgical Technology," Rare Metals and Cemented Carbides, no. 6, pp. 30-37, 2020. keywords: {zirconium metallurgy;metal thermal reduction;molten salt electrolysis;thermal dissociation of zirconium iodide;research progress} |