daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

The Latest Development and Prospect of SiC Particle Reinforced Al-based Composite AITranslate

School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The latest development of SiC particle reinforced Al-based composite is reviewed from its prepa- ration technology, performance and application, respectively. The existing problems of the composite are analyzed during development, and its future development trend is pointed out.

KeyWords AITranslate

Al-based composite SiC particle reinforcement preparation technology performance and appli-cation the latest development

1欧阳柳章,罗承萍,隋贤栋,骆灼旋.SiC_p/Al复合材料的制造及新动向[J].铸造,2000,49(1):17-20. 被引量:22

2崔朝英.SiC_p/Al复合材料的制备方法及研究方向[J].沈阳工程学院学报:自然科学版,2002(3):53-55. 被引量:13

3杨国英,陈建华,任智森.颗粒增强铸造铝基复合材料的研究[J].轻合金加工技术,1998,26(5):39-42. 被引量:9

4樊建中,桑吉梅,石力开.颗粒增强铝基复合材料的研制、应用与发展[J].材料导报,2001,15(10):55-57. 被引量:67

5Cui Yan, Geng Lin, Yao zhongkai. A new advance in the development of high performance SiCe/A1 composite [J]. J Mater Sci, 1997, 13.- 227-231.

6乐永康,张迎元.颗粒增强铝基复合材料的研究现状[J].材料开发与应用,1997,12(5):33-39. 被引量:40

7张大童,李元元,龙雁.铝基复合材料研究进展[J].轻合金加工技术,2000,28(1):5-10. 被引量:46

8ClyneTW,Withers.金属基复合材料导论[M].北京:冶金工业出版社,1996.

9王文明,潘复生,鲁云,曾苏民.P/M制备SiC_p/Al复合材料的研究现状[J].粉末冶金技术,2004,22(6):364-368. 被引量:7

10樊建中,姚忠凯,杜善义,杨改英,孙继光,郭宏,李义春,张少明,石力开.P/M制备的SiC_p/Al复合材料的界面结构[J].中国有色金属学报,1998,8(1):20-23. 被引量:9

1纪兴华,吕昕晖,陈刚,杜之明,李倩倩.粉末冶金及热挤压制备SiC_p/铝基复合材料的磨损性能[J].特种铸造及有色合金,2019,39(1):67-70. 被引量:5

2罗燕,龙文元,罗云,周谊刚.颗粒的正态分布对颗粒增强复合材料性能的影响[J].热加工工艺,2014,43(18):109-111.

3罗燕,龙文元,罗云,周谊刚.复合材料中空心颗粒的团聚效应[J].铸造技术,2015,36(3):570-572.

4肖荣林,郑化安,付东升,李克伦,苏艳敏,吕晓丽.铝基复合材料的制备及应用进展[J].铸造技术,2015,36(5):1118-1121. 被引量:26

5陈阳,唐彬彬,王金辉,李亚耸.SiC_P添加量对铝基复合材料组织和性能的影响[J].铸造技术,2015,36(7):1636-1638. 被引量:2

6杨明晓,林继兴,童先,沈建康,牛丽媛,李光玉.变质和细化工艺对原位Mg_2Si/Al复合材料组织与性能的影响[J].热加工工艺,2015,44(14):168-171.

7刘春忠,任正宜.颗粒增强铝基复合材料的制备方法和强度的影响因素[J].辽宁大学学报:自然科学版,2016,43(2):143-149. 被引量:2

8王进峰,储开宇,赵久兰,范孝良.SiC_p/Al复合材料切削仿真及实验研究[J].人工晶体学报,2016,45(7):1756-1764. 被引量:16

9潘利科,韩建民,张颖骁,杨智勇,李志强,李卫京.高含量SiC_p/A356复合材料衍生材料的组织与性能[J].中国有色金属学报,2016,26(10):2078-2085. 被引量:7

10李剑云,谢敬佩,王爱琴,朱鹏飞.非连续相混杂增强金属基复合材料的研究进展[J].粉末冶金工业,2016,26(6):55-61. 被引量:8

1李广阳,白玉,范文学,郝海.Al-Ti-C-O的制备及其对AZ31镁合金的晶粒细化作用[J].特种铸造及有色合金,2022,42(12):1540-1547.

2周明,徐志凯,颜庆华,卢德宏.粗铝颗粒对Al_(2)O_(3p)/7075铝基复合材料力学性能影响[J].特种铸造及有色合金,2021,41(12):1549-1552.

3韦玉堂,孙婷婷.扩散温度对车用Al2O3/Sn0.3Ag0.7Cu合金粉末组织及物理性能的影响[J].粉末冶金工业,2020,0(1):73-76.

4段春争,刘玉敏,孙伟.切削参数对SiC_p/Al复合材料切削变形的影响[J].工具技术,2019,53(1):20-24. 被引量:1

5王洪涛,姚海龙,易志海,白小波,陈清宇,纪岗昌.冷喷涂SiC/Al纳米复合涂层的组织结构与性能[J].中国表面工程,2018,31(6):98-108. 被引量:1

6潘利文,唐景凡,杨娟,吴晓文,林维捐,胡治流.超声波辅助液态法制备铝基复合材料的研究进展[J].轻合金加工技术,2016,44(2):16-20.

7刘德波,张萍.热挤压对SiC_W-Cu复合材料塑性的影响[J].铸造技术,2016,37(4):765-767.

8李刚,张井波,张明,刘云婷,安亚君.激光诱导自蔓延烧结Al_(80)-(Fe-Cr)_(20)合金组织及性能研究[J].材料导报,2016,30(18):104-107.

9潘利文,林维捐,唐景凡,吴晓文,杨娟,胡治流.颗粒增强铝基复合材料制备方法及研究现状[J].材料导报:纳米与新材料专辑,2016,30(1):511-515. 被引量:14

10姚强,王琼,路通,王燕,朱宇宏.金属基复合材料增强体体积含量检测方法概述[J].中国冶金,2016,26(12):6-8.

1张烈银.复合材料用功能性胶粘剂的性能与应用[J].塑料包装,1998,8(4):29-35.

2丁保华,李文超.梯度功能材料的研究现状与展望[J].耐火材料,1998,32(5):295-298. 被引量:10

3江炎兰,张金春,王杰,张勇.纳米材料的性能与应用——金属及其合金[J].兵器材料科学与工程,2001,24(6):64-66. 被引量:8

4谢允斌,黄美荣,李新贵.聚吡咯纳米粒子的制备与应用[J].胶体与聚合物,2005,23(2):34-36. 被引量:2

5江炎兰,张金春,等.纳米材料的性能与应用-金属及其合金[J].兵器材料科学与工程,2002,25(6):64-66.

6杨慧华,郝刚领,李先雨.泡沫镁的制备及其性能与应用[J].价值工程,2015,34(23):141-142. 被引量:4

7张大童,李元元,龙雁.铝基复合材料研究进展[J].轻合金加工技术,2000,28(1):5-10. 被引量:46

8李克平,张同俊.新型梯度功能材料的研究现状与展望[J].材料导报,1996,10(3):11-15. 被引量:17

9强颖怀,王晓虹,冯培忠.SiCp增强金属基复合材料的研究进展[J].轻金属,2003(7):49-51. 被引量:24

10王君,韩建涛,张杨.肿瘤声动力化学疗法研究现状与展望[J].中国肿瘤,2003,12(6):339-341. 被引量:7

Basic Information:

DOI:

Chinese Library Classification Number:TB333[一般工业技术—材料科学与工程]

Citation Information:

The latest development of SiC particle reinforced Al-based composite is reviewed from its prepa- ration technology, performance and application, respectively. The existing problems of the composite are analyzed during development, and its future development trend is pointed out.

quote

GB/T 7714-2015 [1] WANG Xing, XIE Jing-pei, HAO Shi-ming, et al. The Latest Development and Prospect of SiC Particle Reinforced Al-based Composite[J]. Rare Metals and Cemented Carbides, 2013(3): 50-53.
MLA [1] WANG Xing, et al., "The Latest Development and Prospect of SiC Particle Reinforced Al-based Composite." Rare Metals and Cemented Carbides, no. 3, 2013, pp. 50-53.
APA [1] WANG Xing, XIE Jing-pei, HAO Shi-ming, & WANG Ai-qin. (2013). The Latest Development and Prospect of SiC Particle Reinforced Al-based Composite. Rare Metals and Cemented Carbides(3), 50-53.
IEEE [1] WANG Xing, XIE Jing-pei, HAO Shi-ming, and WANG Ai-qin, "The Latest Development and Prospect of SiC Particle Reinforced Al-based Composite," Rare Metals and Cemented Carbides, no. 3, pp. 50-53, 2013. keywords: {Al-based composite;SiC particle reinforcement;preparation technology;performance and appli-cation;the latest development}