Effect of Pre-Annealing Time on Crystallization of Sm2Fe17ZrNb0.4Cu0.2B0.2 Amorphous Alloy AITranslate
Abstract AITranslate
Sm2Fe17ZrNb0.4Cu0.2B0.2amorphous alloy ribbons were prepared by fast quenching at the speed of 40 m/s in a high vacuum arc melting and single-roll rotary quenching integrated furnace.In order to realize the explosive nucleation of amorphous alloy ribbons at relatively low crystallization temperature,and refine grains and together improve the uniformity of microstructure,it is necessary to improve the order degree of atoms before crystallization.Therefore,the amorphous alloy ribbons were pre-annealed at 500℃for different time to study the crystallization evolution of the amorphous alloy with different pre-annealing time.The results analyzed by X-ray diffractometer(XRD)and high-resolution transmission microscope(HRTEM)show that long-term pre-annealing treatment has a great influence on the precipitation ofα-Fe phase.When the pre-annealing temperature is 500°C,the pre-annealing time should not exceed 90 min.Too long pre-annealing time leads to the early precipitation of crystal phase and uneven crystallization microstructure.
KeyWords AITranslate
1田霖,李春燕,翟建树,卢煜,寇生中.非晶合金的功能性研究进展[J].稀有金属,2021,45(8):998-1009. 被引量:6
2王春伟,黄秋雨.金属晶态-非晶态相变材料的热力学与动力学研究进展[J].热加工工艺,2020,49(14):16-19. 被引量:1
3张晓立,王金相,孙宇新,刘家骢.块体非晶合金的应用与研究进展[J].科学技术与工程,2007,7(24):6383-6390. 被引量:13
4伍尚南,肖方明,唐仁衡.我国稀土永磁材料的发展和需求分析[J].材料研究与应用,2006(4):275-279. 被引量:3
5时彧,刘义伦,陈安华.稀土永磁体在机械工程领域的应用与展望[J].矿山机械,2006,34(6):100-103. 被引量:1
6李容军,甘家毅,谢美玲,梁红梅,陈建彬.稀土永磁材料的发展及在电机中的应用分析[J].大众科技,2019,21(9):23-25. 被引量:4
7邹欣伟,张敏刚,孙刚,马勤.稀土永磁材料的研究进展[J].科技情报开发与经济,2008,18(12):113-116. 被引量:9
8叶金文,刘颖,郑华雄,陈先富,廖立.Sm_2Fe_(17)N_x的结构精修分析[J].稀有金属材料与工程,2011,40(6):1015-1018. 被引量:6
9谭明,严达利,谈清华,王玲玲,郝延明.Sm2Fe17化合物的吸氮反应研究[J].天津师范大学学报:自然科学版,2008,28(3):27-29. 被引量:2
10王小红,刘颖,叶金文,涂铭旌.合金元素对Sm_2Fe_(17)N_x微观结构和性能的影响[J].材料导报,2007,21(F05):304-306. 被引量:2
1云路股份公布第三季度报告[J].磁性元件与电源,2022(11):86-86.
2王成,王伟,丁士杰,宫鹏辉,高原.激光熔覆铁基耐磨涂层的制备及摩擦学性能研究[J].中国激光,2022,49(22):131-141. 被引量:1
3陈超,杨梦梅,孙康,毕海明,王傲,刘颖,徐茹婷.木质素与纤维素热解炭结构特性对其高温石墨化过程的影响机制[J].林业工程学报,2022,7(6):124-131.
4刘金玉,卢明亮,范凤兰,焦连升,王丽.桉木基硬碳用作钠离子电池负极材料[J].化学工程,2023,51(3):24-29. 被引量:1
5李昌新,张庆武,李立.高炉渣基沸石分子筛材料的制备及其响应面优化[J].安全与环境学报,2023,23(2):521-529.
6张乐乐,郭英健,沈鹏,孙齐松,朱明刚.高Ce含量的速凝带及其磁性能[J].粉末冶金工业,2023,33(1):45-50.
7杨依婕,刘莹,张伟,刘娜,桂超,蔡正达,孙鲁闽,陈玉保.TiO_(2)催化剂改性方法对光热催化麻疯树籽油制备生物燃油的影响[J].中国油脂,2023,48(1):53-59.
8陕西国防工业职业技术学院最具转化潜力科技成果项目推介——黄陵矿区煤泥制备4A型分子筛研究项目[J].陕西国防职教研究,2023,33(1).
9任行涛.SAPO-11分子筛合成及丁烯异构化性能研究[J].精细与专用化学品,2023,31(2):8-13.
Basic Information:
DOI:
Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]
Citation Information:
Sm2Fe17ZrNb0.4Cu0.2B0.2amorphous alloy ribbons were prepared by fast quenching at the speed of 40 m/s in a high vacuum arc melting and single-roll rotary quenching integrated furnace.In order to realize the explosive nucleation of amorphous alloy ribbons at relatively low crystallization temperature,and refine grains and together improve the uniformity of microstructure,it is necessary to improve the order degree of atoms before crystallization.Therefore,the amorphous alloy ribbons were pre-annealed at 500℃for different time to study the crystallization evolution of the amorphous alloy with different pre-annealing time.The results analyzed by X-ray diffractometer(XRD)and high-resolution transmission microscope(HRTEM)show that long-term pre-annealing treatment has a great influence on the precipitation ofα-Fe phase.When the pre-annealing temperature is 500°C,the pre-annealing time should not exceed 90 min.Too long pre-annealing time leads to the early precipitation of crystal phase and uneven crystallization microstructure.
quote
| GB/T 7714-2015 | [1] WANG Wan-ting, WANG Shu-huan, LIU Kun, et al. Effect of Pre-Annealing Time on Crystallization of Sm2Fe17ZrNb0.4Cu0.2B0.2 Amorphous Alloy[J]. Rare Metals and Cemented Carbides, 2023(1): 65-69. |
| MLA | [1] WANG Wan-ting, et al., "Effect of Pre-Annealing Time on Crystallization of Sm2Fe17ZrNb0.4Cu0.2B0.2 Amorphous Alloy." Rare Metals and Cemented Carbides, no. 1, 2023, pp. 65-69. |
| APA | [1] WANG Wan-ting, WANG Shu-huan, LIU Kun, & ZHANG Yi-kun. (2023). Effect of Pre-Annealing Time on Crystallization of Sm2Fe17ZrNb0.4Cu0.2B0.2 Amorphous Alloy. Rare Metals and Cemented Carbides(1), 65-69. |
| IEEE | [1] WANG Wan-ting, WANG Shu-huan, LIU Kun, and ZHANG Yi-kun, "Effect of Pre-Annealing Time on Crystallization of Sm2Fe17ZrNb0.4Cu0.2B0.2 Amorphous Alloy," Rare Metals and Cemented Carbides, no. 1, pp. 65-69, 2023. keywords: {Sm-Fe based permanent magnet material;amorphous alloy ribbon;pre-annealing time;crystallization;α-Fe} |