Single Crystal Growth of Cyclopenta-Fused Polycyclic Aromatic Hydrocarbon by the Naphthalene Flux Method: 2D Ambipolar Charge Transport Properties and NIR Absorption Single Crystal Growth of Cyclopenta-Fused Polycyclic Aromatic Hydrocarbon by the Naphthalene Flux Method: 2D Ambipolar Charge Transport Properties and NIR Absorption AITranslate
Abstract AITranslate
Compared to simple p- and n-type organic field-effect transistors, it is very difficult to achieve high performance in ambipolar transistors because both HOMO–HOMO and LUMO–LUMO interactions in the crystal must be large and multidimensional. We have experimentally and theoretically investigated three types of cyclopenta-fused polycyclic aromatic hydrocarbon molecules with narrow HOMO–LUMO gaps and found that one of them is a two-dimensional ambipolar material. Although the crystal structures of these molecules have not been reported due to their low solubility in common organic solvents, we have succeeded in revealing their crystal structures using the naphthalene flux method. 1,2,6,7-Tetraphenyldicyclopenta[cd,jk]pyrene crystals have a brick-work structure, which is expected to be promising for two-dimensional charge transport. Theoretical calculations using the obtained molecular arrangement suggested that there are two-dimensional interactions for both HOMO–HOMO and LUMO–LUMO. Experimental investigation confirmed ambipolar operation in a single-crystal FET. In addition, near-infrared absorption due to intermolecular charge-transfer interactions was observed despite the single-component nature of the material, suggesting its potential for use in photoelectric conversion devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c01148
Chinese Library Classification Number:
Citation Information:
Compared to simple p- and n-type organic field-effect transistors, it is very difficult to achieve high performance in ambipolar transistors because both HOMO–HOMO and LUMO–LUMO interactions in the crystal must be large and multidimensional. We have experimentally and theoretically investigated three types of cyclopenta-fused polycyclic aromatic hydrocarbon molecules with narrow HOMO–LUMO gaps and found that one of them is a two-dimensional ambipolar material. Although the crystal structures of these molecules have not been reported due to their low solubility in common organic solvents, we have succeeded in revealing their crystal structures using the naphthalene flux method. 1,2,6,7-Tetraphenyldicyclopenta[cd,jk]pyrene crystals have a brick-work structure, which is expected to be promising for two-dimensional charge transport. Theoretical calculations using the obtained molecular arrangement suggested that there are two-dimensional interactions for both HOMO–HOMO and LUMO–LUMO. Experimental investigation confirmed ambipolar operation in a single-crystal FET. In addition, near-infrared absorption due to intermolecular charge-transfer interactions was observed despite the single-component nature of the material, suggesting its potential for use in photoelectric conversion devices.
quote
| GB/T 7714-2015 | [1] Hirohiko Tanoguchi, Takuma Yuki, Seiya Yokokura, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01148. |
| MLA | [1] Hirohiko Tanoguchi, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01148. |
| APA | [1] Hirohiko Tanoguchi, Takuma Yuki, Seiya Yokokura, Takashi Yanase, Mingoo Jin, Hajime Ito, Taro Nagahama, & Toshihiro Shimada. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01148 |
| IEEE | [1] Hirohiko Tanoguchi, Takuma Yuki, Seiya Yokokura, Takashi Yanase, Mingoo Jin, Hajime Ito, Taro Nagahama, and Toshihiro Shimada, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01148. keywords: {organic field effect transistors ambipolar charge transport single crystal growth cyclopentafused polycyclic aromaticShow More} |