daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Tensile Deformation Behavior and Microstructure Evolution Mechanism of TC4 Alloy at High Temperature AITranslate

School of Metallurgical Engineering,Xi'an University of Architecture and Technology,Xi'an 710055,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ti-6Al-4V(TC4), as an excellent dual-phase titanium alloy, exhibits good thermal stability at high temperatures and possesses superior overall performance, leading to its extensive use in the aerospace industry. Due to the complex geometries and poor room-temperature formability of titanium alloys, hot forming processes are typically employed during manufacturing. However, TC4 alloy has a narrow hot working window, where the microstructure is highly sensitive to deformation parameters. The competition among deformation mechanisms such as dynamic recrystallization(DRX), work hardening(WH), and dynamic recovery(DRV)complicates microstructural evolution during high-temperature deformation. Therefore, investigating the effects of deformation parameters on microstructural evolution and corresponding deformation mechanisms is crucial. Traditionally, hot compression tests are used to evaluate alloy forming processes. However, in the complex process of hot stamping of intricate parts, tensile stresses may lead to accumulated damage, significantly reducing final mechanical performance. High-temperature tensile tests accurately reflect the stress state during material deformation. The tensile deformation behavior of titanium alloys differs in mechanism from hot compression, making it essential to elucidate the evolution of microstructure during high-temperature tensile deformation for a better understanding of mechanical property changes. Previous studies have indicated that high-temperature deformation of TC4 alloy involves complex microstructural changes such as processing hardening due to dynamic grain growth, deformation and high-temperature movement of intragranular dislocations, α→β phase transformation, globularization of lamellar α phase, dynamic recovery, and dynamic recrystallization. Consequently, material mechanical properties undergo intricate changes, necessitating exploration of TC4 titanium alloy's mechanical characteristics under different high-temperature conditions. The plastic deformation capability of the alloy fundamentally reflects the macro results of its internal microstructural deformation mechanism. A systematic study on the tensile deformation behavior of TC4 alloy within a broad temperature range for hot forming is currently lacking. Therefore, this paper conducted high-temperature tensile experiments at temperatures of 650, 700, 750, 800 and 850 ℃ with a strain rate of 0.02 s-1, employing electron backscatter diffraction (EBSD) to analyze the tensile microstructure characteristics and deformation mechanisms of TC4 alloy post-deformation. The formation process of recrystallized grains was reflected by changes in orientation difference angles, and individual grains were selected to analyze the globularization process of lamellar structures. The phase diagrams and image quality maps were used to reveal α-β phase transformation of TC4 alloy. The results showed that:1) TC4 alloy exhibited different deformation characteristics during high-temperature tensile processes. With increasing deformation temperature, yield stress gradually decreased. At 650 ℃, yield stress increased with loading, peaks, and then rapidly decreased until fracture, exhibiting significant work hardening characteristics. At 700 and 750 ℃, yield stress reached a maximum early in deformation, followed by dynamic softening, indicating DRV characteristics. At 800 and 850 ℃, yield stress peaked early in deformation and then decreased gradually with increasing strain, where dynamic recrystallization played a dominant role, resulting in decreased strength and significantly increased elongation. 2) Fracture surface analysis revealed that at lower temperatures, dimples were smaller and deeper, with uneven distribution and presence of microcracks and numerous voids at fracture surfaces. As temperature increased, dimples became larger and shallower, indicating increased plasticity, consistent with macro trends in elongation. 3) During high-temperature deformation of TC4 alloy, significant differences were observed in microstructural morphology. At 650 ℃, primary α phase exhibited elongated distribution with relatively low equiaxed transformation. Local recrystallization occurred in grain boundaries of α-p phase, forming "necklace-like" recrystallized grains. As temperature rose to 700 and 750 ℃, dynamic softening did not fully dissipate energy from thermal deformation, leading to dynamic precipitation of lamellar α phase, with increased thickness of lamellar α phase with temperature rise. At 800 ℃, thinner α phase lamellae transformed into finer recrystallized grains, undergoing dynamic globularization process, with average DRX grain size approximately 1.04 μm. Increasing to 850 ℃, volume fraction of recrystallized grains increased, including those formed at α-p phase grain boundaries and globularization of lamellar α phase. Overall, with increasing tensile temperature, primary α phase tended towards equiaxial transformation, decreasing aspect ratio from 1.67 to 1.35, with grain size initially increasing and then decreasing. Low-angle grain boundaries(LAGBs)gradually transformed into high-angle grain boundaries(HAGBs), with HAGBs content increasing from 11.7% to 36.1%, indicating enhanced DRX effects. High-temperature tensile process of TC4 alloy was controlled by multiple deformation mechanisms, primarily including DRV mechanism, DRX mechanism, α→β phase transformation, lamellar α phase globularization mechanism, and grain boundary sliding(GBS)mechanism. DRV and continuous dynamic recrystallization(CDRX)mainly controled flow softening process of TC4 alloy, with CDRX mechanism continuously transitioning from LAGBs to HAGBs. Discontinuous dynamic recrystallization(DDRX)phenomenon was observed even at lower temperatures(650 ℃). α→β phase transformation was a critical factor in enhancing alloy plasticity, with decreasing volume fraction of αp phase and increasing α→β phase transformation with temperature rise. Dynamic globularization of lamellar α phase initially occurred in thinner lamellar layers, eventually forming fine and uniform DRX grains.

KeyWords AITranslate

high temperature tensile TC4 alloy mechanical properties microstructure evolution deformation mechanism

[1]Sun D,Zhang Y Q,Jiang S Y,Yu J B,Yan B Y. Investigation on hot workability of Ti-37 at pct Nb alloy based on processing map and microstructural evolution [J]. Metallurgical and Materials Transactions A,2021,52(7):2830.

[2]Shi S X,Ge J Y,Lin Y C,Zhang X Y,Zhou K C. High-temperature deformation behavior and recrystallization mechanism of a near beta titanium alloy Ti-55511 in β phase region [J]. Materials Science and Engineering A,2022,847:143335.

[3](张猛. TC4钛合金高温拉伸变形行为及微观组织演变研究 [D]. 武汉:华中科技大学,2023. 1.)

M Zhang. Study on Tensile Deformation Behavior and Microstructure Evolution of TC4 Titanium Alloy at High Temperature [D]. Wuhan:Huazhong University of Science and Technology,2023. 1.

[4]Paghandeh M,Zarei-Hanzaki A,Abedi H R,Vahidshad Y,Kawałko J,Dietrich D,lampke T. Compressive/tensile deformation behavior and the correlated microstructure evolution of Ti-6Al-4V titanium alloy at warm temperatures [J]. Journal of Materials Research and Technology,2021,10:1291.

[5]Jha J S,Toppo S P,Singh R,Tewari A,Mishra S K. Flow stress constitutive relationship between lamellar and equiaxed microstructure during hot deformation of Ti-6Al-4V [J]. Journal of Materials Processing Technology,2019,270:216.

[6]Li H,Zhao Z L,Guo H Y,Yao Z K,Ning Y Q,Miao X P,Ge M M. Effect of initial alpha lamellar thickness on deformation behavior of a near-α high-temperature alloy during thermomechanical processing [J]. Materials Science and Engineering A,2017,682:345.

[7]Zhang Z X,Qu S J,Feng A H,Hu X,Shen J. Microstructural mechanisms during multidirectional isothermal forging of as-cast Ti-6Al-4V alloy with an initial lamellar microstructure [J]. Journal of Alloys and Compounds,2019,773:277.

[8]Li Z Y,Wang Q J,Du X D,Yang C C,Wang K S. Thermal deformation behavior and microstructural evolution mechanism of TC4 titanium alloy based on hot processing map [J]. JOM,2024,76:5233.

[9](杜丹妮. TC4钛合金超塑性的研究 [D]. 南昌:南昌大学,2016. 1.)

D N Du. Study on Superplasticity of TC4 Titanium Alloy [D]. Nanchang:Nanchang University,2016. 1.

[10]Liu Z G,Li P J,Xiong L T,Liu T Y,He L J. High-temperature tensile deformation behavior and microstructure evolution of Ti55 titanium alloy [J].  Materials Science and Engineering A,2016,680:259.

[11](杨聪聪. 双相Ti-1023合金力学特性及变形机制研究 [D]. 西安:西安建筑科技大学,2023. 1.)

C C Yang. Study on Mechanical Properties and Deformation Mechanism of Dual-Phase Ti-1023 Alloy [D]. Xi'an:Xi'an University of Architecture and Technology,2023. 1.

[12]Yue H Y,Peng H,Su Y J,Wang X P,Chen Y Y. Microstructure and high-temperature tensile property of TiAl alloy produced by selective electron beam melting[J]. Rare Metals,2021,40(12):3635.

[13]Lu K L,Luo B,Wang G D,Huang H T,Chen F G. High-temperature mechanical properties and dynamic recrystallization of Mo-14Re alloy [J]. Materials Characterization,2024,208:113617.

[14](商国强,张晓泳,王新南,李超,朱知寿,甘雪萍. 显微组织类型对TB17钛合金力学性能的影响 [J]. 稀有金属,2024,48(2):153.)

G Q Shang,X Y Zhang,X N Wang,C Li,Z S Zhu,X P Gan. Effect of microstructure types on mechanical properties of TB17 titanium alloy [J]. Chinese Journal of Rare Metals,2018,48(2):153.

[15]Lin X J,Huang H J,Yuan X G,Zheng B Z,Wang Y X,Zuo X J,Zhou G. Microstructure change characteristic and fracture mechanism of Ti-47.5Al-2.5V-1.0Cr-0.2Zr alloy during high temperature tensile deformation [J].  Journal of Alloys and Compounds,2023,952:169963.

[16](飞尚才,蒋小霞. 冷变形 SUS304 奥氏体不锈钢再结晶行为 [J]. 锻压技术,2025,50(1):215.)

S C Fei,X X Jiang. Recrystallization behavior of cold deformed SUS304 austenitic stainless steel [J]. Forging & Stamping Technology,2025,50(1):215.

[17]Shao B,Su H,Tang W,Wan S X,Wang W K,Liu J B,Wang J W,Zong Y Y,Shan D B. Tensile deformation behavior and dynamic recrystallization of TA15 alloy over a wide temperature range [J]. Advanced Engineering Materials,2022,24(12):2200675.

[18]Zhao Q Y,Yang F,Torrens R,Bolzoni L. Comparison of hot deformation behavior and microstructural evolution for Ti-5Al-5V-5Mo-3Cr alloys prepared by powder metallurgy and ingot metallurgy approaches [J]. Materials & Design,2019,169:107682.

[19]Chen K,Luo J,Han W C,Li M Q. Formation and evolution of new α grain boundary and its influence on globularization of α lamellae in TC17 alloy [J]. Journal of Alloys and Compounds,2020,848:156141.

[20]Li C M,Huang L,Zhao M J,Guo S Q,Yang S,Li J J. Characterization of hot workability of Ti-6Cr-5Mo-5V-4Al alloy based on hot processing map and microstructure evolution [J]. Journal of Alloys and Compounds,2022,905:164161.

[21]Sun J Z,Li M Q,Li H. Deformation behavior of TC17 titanium alloy with basketweave microstructure during isothermal compression [J]. Journal of Alloys and Compounds,2018,730:533.

[22]Liu Y,Li Z Q,Zhao B,Sun C Y,Feng Y H. Microstructure evolution characteristics of near-α TA32 titanium alloy during superplastic tensile deformation [J].  Materials Science and Engineering A,2023,879:145264.

[23]Ma L X,Wan M,Li W D,Shao J,Han X N,Zhang J C. On the superplastic deformation mechanisms of near-α TNW700 titanium alloy [J]. Journal of Materials Science Technology,2022,108:173.

[24]Guo B Q,Jonas J J. Dynamic transformation during the high temperature deformation of titanium alloys [J].  Journal of Alloys and Compounds,2021,884:161179.

[25]Wang L H,Zhang Y,Zeng Z,Zhou H,He J,Liu P,Chen M W,Han J,Srolovitz D J,Teng J,Guo Y Z,Yang G,Kong D L,Ma E,Hu Y L,Yin B C,Huang X X,Zhang Z,Zhu T,Han X D. Tracking the sliding of grain boundaries at the atomic scale [J]. Science,2022,375(6586):1261.

[26]Yang J Z,Wu J J. Grain rotation accommodated GBS mechanism for the Ti-6Al-4V alloy during superplastic deformation [J]. Crystals,2021,11:991.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY24070009

Chinese Library Classification Number:TG146.2

Citation Information:

Ti-6Al-4V(TC4), as an excellent dual-phase titanium alloy, exhibits good thermal stability at high temperatures and possesses superior overall performance, leading to its extensive use in the aerospace industry. Due to the complex geometries and poor room-temperature formability of titanium alloys, hot forming processes are typically employed during manufacturing. However, TC4 alloy has a narrow hot working window, where the microstructure is highly sensitive to deformation parameters. The competition among deformation mechanisms such as dynamic recrystallization(DRX), work hardening(WH), and dynamic recovery(DRV)complicates microstructural evolution during high-temperature deformation. Therefore, investigating the effects of deformation parameters on microstructural evolution and corresponding deformation mechanisms is crucial. Traditionally, hot compression tests are used to evaluate alloy forming processes. However, in the complex process of hot stamping of intricate parts, tensile stresses may lead to accumulated damage, significantly reducing final mechanical performance. High-temperature tensile tests accurately reflect the stress state during material deformation. The tensile deformation behavior of titanium alloys differs in mechanism from hot compression, making it essential to elucidate the evolution of microstructure during high-temperature tensile deformation for a better understanding of mechanical property changes. Previous studies have indicated that high-temperature deformation of TC4 alloy involves complex microstructural changes such as processing hardening due to dynamic grain growth, deformation and high-temperature movement of intragranular dislocations, α→β phase transformation, globularization of lamellar α phase, dynamic recovery, and dynamic recrystallization. Consequently, material mechanical properties undergo intricate changes, necessitating exploration of TC4 titanium alloy's mechanical characteristics under different high-temperature conditions. The plastic deformation capability of the alloy fundamentally reflects the macro results of its internal microstructural deformation mechanism. A systematic study on the tensile deformation behavior of TC4 alloy within a broad temperature range for hot forming is currently lacking. Therefore, this paper conducted high-temperature tensile experiments at temperatures of 650, 700, 750, 800 and 850 ℃ with a strain rate of 0.02 s-1, employing electron backscatter diffraction (EBSD) to analyze the tensile microstructure characteristics and deformation mechanisms of TC4 alloy post-deformation. The formation process of recrystallized grains was reflected by changes in orientation difference angles, and individual grains were selected to analyze the globularization process of lamellar structures. The phase diagrams and image quality maps were used to reveal α-β phase transformation of TC4 alloy. The results showed that:1) TC4 alloy exhibited different deformation characteristics during high-temperature tensile processes. With increasing deformation temperature, yield stress gradually decreased. At 650 ℃, yield stress increased with loading, peaks, and then rapidly decreased until fracture, exhibiting significant work hardening characteristics. At 700 and 750 ℃, yield stress reached a maximum early in deformation, followed by dynamic softening, indicating DRV characteristics. At 800 and 850 ℃, yield stress peaked early in deformation and then decreased gradually with increasing strain, where dynamic recrystallization played a dominant role, resulting in decreased strength and significantly increased elongation. 2) Fracture surface analysis revealed that at lower temperatures, dimples were smaller and deeper, with uneven distribution and presence of microcracks and numerous voids at fracture surfaces. As temperature increased, dimples became larger and shallower, indicating increased plasticity, consistent with macro trends in elongation. 3) During high-temperature deformation of TC4 alloy, significant differences were observed in microstructural morphology. At 650 ℃, primary α phase exhibited elongated distribution with relatively low equiaxed transformation. Local recrystallization occurred in grain boundaries of α-p phase, forming "necklace-like" recrystallized grains. As temperature rose to 700 and 750 ℃, dynamic softening did not fully dissipate energy from thermal deformation, leading to dynamic precipitation of lamellar α phase, with increased thickness of lamellar α phase with temperature rise. At 800 ℃, thinner α phase lamellae transformed into finer recrystallized grains, undergoing dynamic globularization process, with average DRX grain size approximately 1.04 μm. Increasing to 850 ℃, volume fraction of recrystallized grains increased, including those formed at α-p phase grain boundaries and globularization of lamellar α phase. Overall, with increasing tensile temperature, primary α phase tended towards equiaxial transformation, decreasing aspect ratio from 1.67 to 1.35, with grain size initially increasing and then decreasing. Low-angle grain boundaries(LAGBs)gradually transformed into high-angle grain boundaries(HAGBs), with HAGBs content increasing from 11.7% to 36.1%, indicating enhanced DRX effects. High-temperature tensile process of TC4 alloy was controlled by multiple deformation mechanisms, primarily including DRV mechanism, DRX mechanism, α→β phase transformation, lamellar α phase globularization mechanism, and grain boundary sliding(GBS)mechanism. DRV and continuous dynamic recrystallization(CDRX)mainly controled flow softening process of TC4 alloy, with CDRX mechanism continuously transitioning from LAGBs to HAGBs. Discontinuous dynamic recrystallization(DDRX)phenomenon was observed even at lower temperatures(650 ℃). α→β phase transformation was a critical factor in enhancing alloy plasticity, with decreasing volume fraction of αp phase and increasing α→β phase transformation with temperature rise. Dynamic globularization of lamellar α phase initially occurred in thinner lamellar layers, eventually forming fine and uniform DRX grains.

quote

GB/T 7714-2015 [1] Zhiyi Li, Qingjuan Wang, Xudong Du, et al. Tensile Deformation Behavior and Microstructure Evolution Mechanism of TC4 Alloy at High Temperature[J]. Chinese Journal of Rare Metals, 2026, 50(8): 1239-1248. DOI:10.13373/j.cnki.cjrm.XY24070009.
MLA [1] Zhiyi Li, et al., "Tensile Deformation Behavior and Microstructure Evolution Mechanism of TC4 Alloy at High Temperature." Chinese Journal of Rare Metals, vol. 50, no. 8, 2026, pp. 1239-1248, https://doi.org/10.13373/j.cnki.cjrm.XY24070009.
APA [1] Zhiyi Li, Qingjuan Wang, Xudong Du, Tongyao Yang, Wen Wang, & Kuaishe Wang. (2026). Tensile Deformation Behavior and Microstructure Evolution Mechanism of TC4 Alloy at High Temperature. Chinese Journal of Rare Metals, 50(8), 1239-1248. https://doi.org/10.13373/j.cnki.cjrm.XY24070009
IEEE [1] Zhiyi Li, Qingjuan Wang, Xudong Du, Tongyao Yang, Wen Wang, and Kuaishe Wang, "Tensile Deformation Behavior and Microstructure Evolution Mechanism of TC4 Alloy at High Temperature," Chinese Journal of Rare Metals, vol. 50, no. 8, pp. 1239-1248, 2026, doi: 10.13373/j.cnki.cjrm.XY24070009. keywords: {high temperature tensile;TC4 alloy;mechanical properties;microstructure evolution;deformation mechanism}