Mechanism Study on Selective Extraction of Nickel from Acidic Sulfate Solution by Using the Synergistic Solvent Extraction System of P204 and 4PC AITranslate
Abstract AITranslate
The mechanism of synergistic solvent extraction of nickel by P204 and 4PC from acidic sulfate solution was studied with slope method,constant molecale method and saturation extraction method,respectively. The thermodynamic equilibrium constant of the synergistic reaction was determined,and its enthalpy and entropy changes were also obtained.The results show that the combination of P204 with 4PC has a positive synergistic effect for nickel extraction,and the extracted complex is identified as NiA2L2.The synergistic solvent extraction is an endothermic reaction with enthalpy change of 29.52J/mol and entropy change of-6.53kJ/(mol·K).The synergistic solvent extraction system of P204and 4PC can obviously promote the selective extraction of nickel from acidic sulfate solution.
KeyWords AITranslate
1黄小卫,李建宁,张永奇,龙志奇,王春梅,薛向欣.P204-P507在酸性硫酸盐溶液中对Nd^3+和Sm^3+的协同萃取[J].中国有色金属学报,2008,18(2):366-371. 被引量:24
2肖超,肖连生.钴、镍萃取分离原理与方法[J].湿法冶金,2010,29(4):225-228. 被引量:10
3chu yong cheng,keith r.barnard,wensheng zhang,zhaowu zhu,yoko pranolo.Recovery of nickel,cobalt,copper and zinc in sulphate and chloride solutions using synergistic solvent extraction[J].中国化学工程学报:英文版,2016,0(2):237-248. 被引量:9
4刘大星.从镍红土矿中回收镍、钴技术的进展[J].有色金属:冶炼部分,2002(3):6-10. 被引量:116
1刘文森,雷泽,朱兆武,齐涛.含氮杂环化合物与有机酸协同体系在镍、钴萃取分离中的应用[J].过程工程学报,2020,20(4):382-389. 被引量:3
2张文凯,龚元琳,高凯歌.二-(2-乙基己基)磷酸酯与单烷基磷酸酯协同萃取湿法磷酸中铁离子的研究[J].磷肥与复肥,2021,36(4):4-6.
1邓静娴,武彪,孙启,温建康,刘学.钴对羟肟萃取剂的毒化及其抑制研究进展[J].中国有色金属学报,2021,31(7):1922-1932.
2方海嫣,刘海燕,魏宗武,沈芳,王臣.几种锰冶炼硫酸锰溶液中钴镍离子分离方法[J].科学大众:科技创新,2021(10):239-241.
3宋强,童雄,谢贤,张文杰,许宝松,范培强,彭世文.溶剂萃取法分离提取镍和钴的研究现状及展望[J].中国有色金属学报,2023,33(6):1957-1971.
1李敏,李英波,罗海燕,咸漠,梁向峰,刘会洲.1,2,4-丁三醇稀溶液缩醛反应的热力学和动力学特征(英文)[J].过程工程学报,2017,17(6):1265-1273.
2万建新,任学昌,蒋煜峰,郭效军,彭波.P204-熔融石蜡固液萃取废水中铜、钴、镍[J].环境化学,2018,37(12):2688-2693.
3杜瑾,齐芳云.测定硫酸根浓度如何确定钡镁合剂用量[J].电力勘测设计,2019,31(1):42-45. 被引量:1
4黄月华,张铭阑,章志云,王怡,杨飞,刁晓平.蚯蚓粪对扑热息痛的吸附特性[J].江苏农业科学,2019,47(1):268-273.
5张雪凯,周康根,陈伟,雷清源,黄颖,彭长宏.酸浸-分步萃取法从赤泥中回收铁和稀土(英文)[J].中南大学学报:英文版,2019,26(2):458-466. 被引量:26
6唐晓玲.容量法测定铝土矿中三氧化二铝含量[J].冶金与材料,2018,38(4):71-72. 被引量:5
7刘宇程,陈媛媛,梁晶晶,吕忠祥,刘骞.复合溶剂萃取法处理油基钻屑实验研究[J].应用化工,2019,48(1):93-96. 被引量:9
8周国涛,李青刚,刘永畅,张贵清,曹佐英,曾理,关文娟.从钨渣硫酸浸出液中萃取钪的研究[J].稀有金属与硬质合金,2018,46(6):1-9. 被引量:7
9王钊,张诚春.蔗糖总有机碳标准物质的研制[J].工业计量,2018,28(6):98-101. 被引量:4
10代阿芳,杨俊,孙月婷.硝酸汞滴定法测定复混肥料中氯离子的含量[J].中国土壤与肥料,2018(6):202-206. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]
Citation Information:
The mechanism of synergistic solvent extraction of nickel by P204 and 4PC from acidic sulfate solution was studied with slope method,constant molecale method and saturation extraction method,respectively. The thermodynamic equilibrium constant of the synergistic reaction was determined,and its enthalpy and entropy changes were also obtained.The results show that the combination of P204 with 4PC has a positive synergistic effect for nickel extraction,and the extracted complex is identified as NiA2L2.The synergistic solvent extraction is an endothermic reaction with enthalpy change of 29.52J/mol and entropy change of-6.53kJ/(mol·K).The synergistic solvent extraction system of P204and 4PC can obviously promote the selective extraction of nickel from acidic sulfate solution.
quote
| GB/T 7714-2015 | [1] SUN Zhen, ZENG Li, GUAN Wen-juan, et al. Mechanism Study on Selective Extraction of Nickel from Acidic Sulfate Solution by Using the Synergistic Solvent Extraction System of P204 and 4PC[J]. Rare Metals and Cemented Carbides, 2018(6): 25-31. |
| MLA | [1] SUN Zhen, et al., "Mechanism Study on Selective Extraction of Nickel from Acidic Sulfate Solution by Using the Synergistic Solvent Extraction System of P204 and 4PC." Rare Metals and Cemented Carbides, no. 6, 2018, pp. 25-31. |
| APA | [1] SUN Zhen, ZENG Li, GUAN Wen-juan, ZHANG Gui-qing, & WANG Ying-song. (2018). Mechanism Study on Selective Extraction of Nickel from Acidic Sulfate Solution by Using the Synergistic Solvent Extraction System of P204 and 4PC. Rare Metals and Cemented Carbides(6), 25-31. |
| IEEE | [1] SUN Zhen, ZENG Li, GUAN Wen-juan, ZHANG Gui-qing, and WANG Ying-song, "Mechanism Study on Selective Extraction of Nickel from Acidic Sulfate Solution by Using the Synergistic Solvent Extraction System of P204 and 4PC," Rare Metals and Cemented Carbides, no. 6, pp. 25-31, 2018. keywords: {nickel;synergistic solvent extraction;selectivity;P204;4PC;mechanism;thermodynamics} |