First-principles study of the thermodynamic properties and electronic structure of compounds from Hf–Ni phase system AITranslate

Institute of Nuclear Sciences Vinča;Institute of Nuclear Sciences Vinča;Institute of Nuclear Sciences Vinča;Institute of Nuclear Sciences Vinča
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ab initio calculations of the structural, electronic and thermodynamic properties of Hf2Ni, HfNi, HfNi2 and HfNi5 are presented. Using all-electron augmented plane waves plus local orbitals (APW+lo) method the relative stability of the selected compounds was determined by calculating their enthalpies of formation and cohesive energies. In addition, their electronic structure and bonding properties were determined. The results are discussed in view of the potential application of these intermetallics as materials for hydrogen storage.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.04.019

Chinese Library Classification Number:

Citation Information:

Ab initio calculations of the structural, electronic and thermodynamic properties of Hf2Ni, HfNi, HfNi2 and HfNi5 are presented. Using all-electron augmented plane waves plus local orbitals (APW+lo) method the relative stability of the selected compounds was determined by calculating their enthalpies of formation and cohesive energies. In addition, their electronic structure and bonding properties were determined. The results are discussed in view of the potential application of these intermetallics as materials for hydrogen storage.

quote

GB/T 7714-2015 [1] Jana Radaković, Katarina Ćirić, Jelena BeloševićČavor, et al. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.04.019.
MLA [1] Jana Radaković, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.04.019.
APA [1] Jana Radaković, Katarina Ćirić, Jelena BeloševićČavor, & Vasil Koteski. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.04.019
IEEE [1] Jana Radaković, Katarina Ćirić, Jelena BeloševićČavor, and Vasil Koteski, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.04.019.