daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Range-Broadening Ultraviolet-Blocking Regulation of Cellulose Nanopaper via Surface Self-Absorption with Poly(methyl methacrylate)/Avobenzone AITranslate

Shaanxi University of Science &Technology; Shaanxi University of Science &Technology; Shaanxi University of Science &Technology; Shaanxi University of Science &Technology;Northwest University; China|Northwest University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cellulose nanopaper-based materials with recyclability and excellent optical properties have recently received increasing attention. A series of lignin-containing (17.2, 14.7, 7.3, 4.9, and 1.3% by wt) pristine nanopapers (LNPs) were obtained through self-absorption of poly(methyl methacrylate) (PMMA)/avobenzone (AVB) to produce cellulose nanopapers (LPANPs) with range-broadening and ultraviolet (UV) blocking extending from UVB (290–320 nm) to UVA (320–400 nm). SEM results indicated that PMMA/AVB presented a microspherical morphology (150–600 nm) on LPANP surfaces. LPANP exhibited high optical transparency (>95% in the visible region) and high haze (>77%), with good wet mechanical properties (107.5 MPa) and thermal stability. In addition, LPANP hydrophobic properties were significantly improved after PMMA/AVB particle absorption, achieving conversion from hydrophilicity to hydrophobicity. Consequently, with the properties of water resistance, optical haze, and range-broadening UV-blocking, these LPANP presented potential applications in the field of optoelectronic devices, such as in UV-blocking, supercapacitors, and electronic device substrates.

KeyWords AITranslate

haze cellulose nanopaper selfabsorption PMMA/AVB particle rangebroadening ultravioletblocking hydrophobicity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00686

Chinese Library Classification Number:

Citation Information:

Cellulose nanopaper-based materials with recyclability and excellent optical properties have recently received increasing attention. A series of lignin-containing (17.2, 14.7, 7.3, 4.9, and 1.3% by wt) pristine nanopapers (LNPs) were obtained through self-absorption of poly(methyl methacrylate) (PMMA)/avobenzone (AVB) to produce cellulose nanopapers (LPANPs) with range-broadening and ultraviolet (UV) blocking extending from UVB (290–320 nm) to UVA (320–400 nm). SEM results indicated that PMMA/AVB presented a microspherical morphology (150–600 nm) on LPANP surfaces. LPANP exhibited high optical transparency (>95% in the visible region) and high haze (>77%), with good wet mechanical properties (107.5 MPa) and thermal stability. In addition, LPANP hydrophobic properties were significantly improved after PMMA/AVB particle absorption, achieving conversion from hydrophilicity to hydrophobicity. Consequently, with the properties of water resistance, optical haze, and range-broadening UV-blocking, these LPANP presented potential applications in the field of optoelectronic devices, such as in UV-blocking, supercapacitors, and electronic device substrates.

quote

GB/T 7714-2015 [1] Xinping Li, Xin Zhang, Nan Wang, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00686.
MLA [1] Xinping Li, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00686.
APA [1] Xinping Li, Xin Zhang, Nan Wang, Hui Chang, Yaoyu Wang, & Zhao Zhang. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00686
IEEE [1] Xinping Li, Xin Zhang, Nan Wang, Hui Chang, Yaoyu Wang, and Zhao Zhang, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00686. keywords: {haze cellulose nanopaper;selfabsorption;PMMA/AVB particle;rangebroadening ultravioletblocking;hydrophobicity}