The ability to detect early damage is of great significance in load bearing composite materials used for high performance applications. Microdamages if left unchecked can grow under subsequent stress, leading to catastrophic structural failure. The sensing of early stage damage via nondestructive methods is therefore critically important for the safe use of these materials. Herein a supramolecular approach to self-diagnosis of early stage damage in a carbon fiber epoxy composite material, via the incorporation of a CB[8] based ternary complex as an additive is reported. The complex comprising a fluorescent probe and a quencher encapsulated by the CB[8] is introduced into the epoxy resin of the composite as a supramolecular cross-linking agent, whose stress-induced dissociation results in the turn on of fluorescence of the probe. In this way, detection of irreversible mechanical strain and fatigue at an early stage is attainable, enabling the assessment of microdamage in the material.

KeyWords AITranslate

damage reporting composites carbon fiber epoxy resin composites CB[8] ternary complexes fluorescence strain and fatigue Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00694

Chinese Library Classification Number:

Citation Information:

The ability to detect early damage is of great significance in load bearing composite materials used for high performance applications. Microdamages if left unchecked can grow under subsequent stress, leading to catastrophic structural failure. The sensing of early stage damage via nondestructive methods is therefore critically important for the safe use of these materials. Herein a supramolecular approach to self-diagnosis of early stage damage in a carbon fiber epoxy composite material, via the incorporation of a CB[8] based ternary complex as an additive is reported. The complex comprising a fluorescent probe and a quencher encapsulated by the CB[8] is introduced into the epoxy resin of the composite as a supramolecular cross-linking agent, whose stress-induced dissociation results in the turn on of fluorescence of the probe. In this way, detection of irreversible mechanical strain and fatigue at an early stage is attainable, enabling the assessment of microdamage in the material.

quote

GB/T 7714-2015 [1] Anjali Devi Das, Giulia Mannoni, Andreas E. Früh, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00694.
MLA [1] Anjali Devi Das, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00694.
APA [1] Anjali Devi Das, Giulia Mannoni, Andreas E. Früh, Davide Orsi, Roberta Pinalli, & Enrico Dalcanale. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00694
IEEE [1] Anjali Devi Das, Giulia Mannoni, Andreas E. Früh, Davide Orsi, Roberta Pinalli, and Enrico Dalcanale, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00694. keywords: {damage reporting composites;carbon fiber epoxy resin composites;CB[8] ternary complexes;fluorescence;strain and fatigue;Show More}