Study on Preparation Process of W-Al_2O_3 Composite Powder AITranslate
Abstract AITranslate
Al2 O3-doped W powder was prepared by sol-gel, azeotropic distillation and hydrothermal synthesis to produce W-Al2 O3 composite powder by calcination and two-step H2 reduction. Based on XRD analysis and SEM observation, stable monoclinic WOa and metastable hexagonal WO3 were obtained by calcination of Al2 O3-doped W powder prepared with the above-mentioned three methods. The morphology of the powder prepared by hydrothermal synthesis is regular, uniform and spherical. WO3 is reduced to low-valence WO2 and unsaturated-valence WO3-x by the primary H2 reduction,and fine W-Al2 O3 composite powder is obtained by the secondary H2 reduction. Compared with the other two methods, sol-gel method has more obvious refinement effect and it can prepare W-Al2O3 composite powder with nanoscale particle size, since Al2 O3 coated on the surfaces of W particles inhibits the deposition of tungsten atom during subsequent reduction.
KeyWords AITranslate
1种法力,陈勇,吴玉程,陈俊凌.La_2O_3弥散增强钨合金面对等离子体材料及其高热负荷性能[J].材料科学与工程学报,2009,27(3):415-417. 被引量:11
2陈勇,吴玉程,于福文,陈俊凌.La_2O_3弥散强化钨合金的组织性能研究[J].稀有金属材料与工程,2007,36(5):822-824. 被引量:25
1郭震,陈文琳.固溶处理对Al-13.0Si-4.5Cu-1.0Mg-2.0Ni合金组织和性能的影响[J].铸造,2017,66(3):273-276. 被引量:6
2杨芳,郭春霞.热化学反应法镁合金陶瓷涂层的制备及性能的影响[J].热加工工艺,2006,35(8):48-49. 被引量:16
3肖心萍,王淑英,崔永强.累积叠轧法制备纳米晶AZ91板材的研究[J].热加工工艺,2013,42(7):123-124. 被引量:1
4徐琳,丁建宁,许晓静,何远清,雷小春.钛基表面TiO_2-HA生物陶瓷膜层的血液相容性研究[J].稀有金属材料与工程,2017,46(5):1299-1304. 被引量:1
5王新征.2450℃小型高温烧结炉的研制[J].真空,2017,54(3):63-65.
6董天顺,王拓,郑晓东,周秀锴,刘金海,李国禄,崔春翔.细晶Mg-Ce中间合金的制备及其对AZ91D组织和性能的影响[J].材料导报,2017,31(12):73-78. 被引量:3
7张展飞,袁子洲,郭廷彪,张香云.金属型中温度梯度和浇注温度对ZL205A合金充型和组织性能的影响[J].铸造技术,2017,38(6):1410-1415.
8刘成刚,鞠富,李翠薇,武志勇,郝素斌,于秀霞,谭建波.水含量对162型中温蜡成型质量的影响[J].河北工业科技,2017,34(4):294-299.
9胡平,郑磊.热输入对管线钢热模拟焊缝粗晶热影响区冲击韧性的影响[J].焊管,2017,40(6):9-19. 被引量:3
10向文丽,徐媛,祝菲霞,司民真,孙坤.石墨烯的微波法快速制备及其降解罗丹明B性能的研究[J].云南大学学报:自然科学版,2017,39(4):573-578. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]
Citation Information:
Al2 O3-doped W powder was prepared by sol-gel, azeotropic distillation and hydrothermal synthesis to produce W-Al2 O3 composite powder by calcination and two-step H2 reduction. Based on XRD analysis and SEM observation, stable monoclinic WOa and metastable hexagonal WO3 were obtained by calcination of Al2 O3-doped W powder prepared with the above-mentioned three methods. The morphology of the powder prepared by hydrothermal synthesis is regular, uniform and spherical. WO3 is reduced to low-valence WO2 and unsaturated-valence WO3-x by the primary H2 reduction,and fine W-Al2 O3 composite powder is obtained by the secondary H2 reduction. Compared with the other two methods, sol-gel method has more obvious refinement effect and it can prepare W-Al2O3 composite powder with nanoscale particle size, since Al2 O3 coated on the surfaces of W particles inhibits the deposition of tungsten atom during subsequent reduction.
quote
| GB/T 7714-2015 | [1] ZHAO Yang, WEI Shi-zhong, PAN Kun-ming, et al. Study on Preparation Process of W-Al_2O_3 Composite Powder[J]. Rare Metals and Cemented Carbides, 2017(3): 25-30. |
| MLA | [1] ZHAO Yang, et al., "Study on Preparation Process of W-Al_2O_3 Composite Powder." Rare Metals and Cemented Carbides, no. 3, 2017, pp. 25-30. |
| APA | [1] ZHAO Yang, WEI Shi-zhong, PAN Kun-ming, DAN Kang-ning, YAO Li-ying, & SONG Xiang-yang. (2017). Study on Preparation Process of W-Al_2O_3 Composite Powder. Rare Metals and Cemented Carbides(3), 25-30. |
| IEEE | [1] ZHAO Yang, WEI Shi-zhong, PAN Kun-ming, DAN Kang-ning, YAO Li-ying, and SONG Xiang-yang, "Study on Preparation Process of W-Al_2O_3 Composite Powder," Rare Metals and Cemented Carbides, no. 3, pp. 25-30, 2017. keywords: {W-Al2O3 composite powder;sol-gel method;azeotropic distillation;hydrothermal synthesis;calcination;two-step H2 reduction} |