A New Environmental-acceptable Process for Regeneration ofCemented Carbide Scraps AITranslate

School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Description is made of a new environmentally- acceptable process for regeneration of cemented carbide scraps developed by professor V.P.Bondarenko research group of Institute for Super-hard Materials of the National Academy of Sciences of Ukraine.The process is based on cemented carbide scraps as raw material in the steps as follows:oxidation,crushing-mixture gas-phase reduction-carbonization to obtain carbon-controlled regenerated cemented carbide, followed by pressing,CH4 and H2 mixed gas low-temperature sintering and high-temperature gas-phase sintering to produce regenerated cemented carbide, whose property conforms with Ukraine State Standard 3882-74.

KeyWords AITranslate

cemented carbide regeneration environmental protection

1Bondarenko V P,et al.Advanced technologies of production of cemented carbides and composite materials based on them[A].Kencrunger G.Proceedings of the 15th Iinternational Plansee Seminar[C].Plansee Holding AG:Routte,2001.

2Бондаренко.ВП,идр.Спеканиеволъфрамовыхтвердыхсплавоввпрецизионноконтролируемойгазовойсреде[M].Киев:НауковаДумка,1995.

3Bondarenho V P,et al.Production of tungsten-cobalt cemented carbides[J].Materials Technology,2002,17(1):30.

4Bondarenko V P,et al.Optimizing conditions for obtaining a solid solution of tungsten carbide in titanium carbide by preparing it in a precisely controlled gas medium[J].Int Journal of Hydrogen Energy,1999,24:845.

5Bondarenko V P,et al.Use of a precisely controlled methane-hydrogen gas medium when regeneratioing tungsten-base hard alloy waste[J].Int Journal of Hydrogen Energy,1999,24:853.

6Bondarenko V P.et al.The effect of temperature and holding time on the degree of regeneration of T5K10 alloy waste in hydrogen containing equilibrium amounts of methane[J].Int Journal of Hydrogen Energy,1999,24:849.

1李友生.钨资源在硬质合金刀具行业中的可持续发展[J].制造技术与机床,2012(12):107-110. 被引量:1

2刘雪梅,范金莲,冯浩,宋晓艳.WC-Co硬质合金的高温氧化过程研究[J].中国体视学与图像分析,2018,23(4):343-350. 被引量:1

3周新华,王力民,彭英健.我国硬质合金再生产业现状与发展[J].硬质合金,2016,33(5):356-364. 被引量:19

1李亮星,朱志城,贾孟熹,黄茜琳.硬质合金废料电解回收钨及W(Ⅵ)在熔盐中的电化学行为[J].材料导报,2022,36(S01):448-453.

2杨斌,陈广军,石安红,刘柏雄.废旧硬质合金短流程回收技术的研究现状[J].材料导报,2015,29(3):68-74. 被引量:15

3陈飞,龙坚战,冉丽萍,邱友绪.Al含量对WC-Fe合金的组织与性能的影响[J].硬质合金,2017,34(2):75-82.

4王超,张红梅,李岩,贾宏斌,王渐灵,孟令浩,姜正义.烧结温度对碳化钨/高强钢复合材料界面微观组织和元素扩散的影响[J].功能材料,2019,50(4):4086-4092.

5谭千榆,王鹏,时凯华,曾伟.Co-Ni-Cr复合粘结相矿用合金的研制及生产[J].四川冶金,2019,41(3):29-33. 被引量:1

6邝海,谭敦强,何文,易志强.氧化还原法回收废硬质合金[J].稀有金属与硬质合金,2019,47(4):70-75. 被引量:3

7赵中伟,孙丰龙,杨金洪,方奇,姜文伟,刘旭恒,陈星宇,李江涛.我国钨资源、技术和产业发展现状与展望[J].中国有色金属学报,2019,29(9):1902-1916. 被引量:39

8汪艳亮,王云,谢小豪,陈林芳,陈颢.稀土硬质合金研究进展[J].有色金属科学与工程,2019,10(5):106-112. 被引量:9

9谢小豪,王云,汪艳亮,陈颢.废旧硬质合金回收方法及其研究进展[J].有色金属科学与工程,2020,11(2):64-70. 被引量:11

10李刚,张红梅,赵大东,王超,李洪楠,李娜,孟令浩,姜正义.颗粒粒径对碳化钨/高强钢复合材料界面微观组织和元素扩散的影响[J].功能材料,2021,52(1):1104-1114.

1用浮选法生产再生氧化铝的工艺[J].轻金属,2005(3):64-64.

2张长理.电解法再生废硬质合金工艺进展[J].有色金属:冶炼部分,1990(2):40-42. 被引量:1

3韩培德,吴宇,黄源.锌熔法回收硬质合金质量分析[J].太原理工大学学报,1998,29(3):279-281. 被引量:3

4栾广英,关晓宇.钴渣提取氧化钴工艺的改进[J].有色金属:冶炼部分,1993(3):15-16. 被引量:3

5刘沙,刘刚,杨贵彬,黄泽兰.碳化钨粉制备新技术[J].稀有金属与硬质合金,2005,33(1):29-32. 被引量:7

6周长松,康平.电解法处理废硬质合金工艺及发展前景[J].硬质合金,1989(1):47-52. 被引量:1

7姜文伟,高晋,普崇恩,谢盛德.硫酸钠熔炼法处理废硬质合金工艺中钴的回收[J].稀有金属与硬质合金,2000,28(2):22-25. 被引量:13

8苏鸿英.废铝回收再生——美国铝工业的一大热点[J].资源再生,2008(3):31-31. 被引量:2

9张长理.电解法处理废硬质合金[J].中国物资再生,1992(8):13-15.

10曹茂盛.气相还原法制备α-Fe超细粉末试验工艺研究[J].材料科学与工艺,1995,3(4):91-95. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF805.2[冶金工程—有色金属冶金]

Citation Information:

Description is made of a new environmentally- acceptable process for regeneration of cemented carbide scraps developed by professor V.P.Bondarenko research group of Institute for Super-hard Materials of the National Academy of Sciences of Ukraine.The process is based on cemented carbide scraps as raw material in the steps as follows:oxidation,crushing-mixture gas-phase reduction-carbonization to obtain carbon-controlled regenerated cemented carbide, followed by pressing,CH4 and H2 mixed gas low-temperature sintering and high-temperature gas-phase sintering to produce regenerated cemented carbide, whose property conforms with Ukraine State Standard 3882-74.

quote

GB/T 7714-2015 [1] LIU Sha, LIU Gang, YANG Gui-bin, et al. A New Environmental-acceptable Process for Regeneration ofCemented Carbide Scraps[J]. Rare Metals and Cemented Carbides, 2004(2): 21-23.
MLA [1] LIU Sha, et al., "A New Environmental-acceptable Process for Regeneration ofCemented Carbide Scraps." Rare Metals and Cemented Carbides, no. 2, 2004, pp. 21-23.
APA [1] LIU Sha, LIU Gang, YANG Gui-bin, & HUANG Ze-lan. (2004). A New Environmental-acceptable Process for Regeneration ofCemented Carbide Scraps. Rare Metals and Cemented Carbides(2), 21-23.
IEEE [1] LIU Sha, LIU Gang, YANG Gui-bin, and HUANG Ze-lan, "A New Environmental-acceptable Process for Regeneration ofCemented Carbide Scraps," Rare Metals and Cemented Carbides, no. 2, pp. 21-23, 2004. keywords: {cemented carbide;regeneration;environmental protection}