Abstract AITranslate

This article describes the situation in the recent years of extraction and stripping technology and equipment in hydrometallurgy of Ta & Nb in China,focusing on description of the latest development and techno-economic data in HF-H2SO4-Octanol-2 extraction-stripping system as well as the existing technical problems,related measures and ideas for the improvement and solution.

KeyWords AITranslate

tantalum and niobium extraction-stripping Octano-2 technology equipment

1莘良佐,等.钽铌冶金[M].北京:冶金工业出版社,1982.

2王肇信 幸良佐 曾芳屏.钽铌冶金学[M].北京:稀有金属冶金学会,1998.232-254.

3吴贤澄,等译.有机溶剂分析手册[M].北京:化学工业出版社,1984.

4张心灵.钽铌湿法技改工程设计评述[A]..1998年稀有金属冶金分会论文集(钽铌部分)[C].石嘴山:宁夏有色金属冶炼厂,1998.88.

5韩建设,张劲.钽铌水冶分解提取工艺及设备的进展[J].稀有金属与硬质合金,2003,31(4):27-31. 被引量:14

6韩建设.氧化铌生产工艺及装备的进展[J].稀有金属与硬质合金,2003,31(1):35-38. 被引量:14

1任卿,张锦柱,赵春红.钽、铌资源现状及其分离方法研究进展[J].湿法冶金,2006,25(2):65-69. 被引量:20

2韩建设,赵明智,王才明,张劲,周勇.钽铌湿法冶炼的“三废”综合治理工艺探讨[J].稀有金属与硬质合金,2006,34(4):40-44. 被引量:12

3唐德胜,晏慧娟.钽铌氢氧化物洗水回用工艺研究[J].稀有金属与硬质合金,2010,38(4):43-45.

4韩建设,李丰,吴鹰.钽铌湿法冶炼工序成本及其核算管理探讨[J].稀有金属与硬质合金,2010,38(4):46-51.

5李光伟,许延辉,赵文怡,马升峰.富铌渣硫酸浸出液中铌的分离工艺研究[J].稀土,2013,34(4):57-62. 被引量:5

6胡根火,郭永忠,宋金华.镁粉还原-仲辛醇萃取法从钽铌矿分解液中除Sb的实验研究[J].稀有金属与硬质合金,2014,42(3):12-14. 被引量:2

7李兵,张劲松,陈云明,曹其如,黄立娟,李新政,刘东彬,鲁芸芸,张海君.不锈钢材料中微量铌的分离技术研究[J].化学研究与应用,2014,26(7):1112-1116.

8晏秋平.浅谈钽铌金属矿回收实验研究[J].科技视界,2014(22):285-285.

9马小华,高海涛.钽铌冶炼工业废水处理过程中产生废渣的综合处理及利用研究[J].化学工程与装备,2015(6):32-35.

10马小华,高海涛.钽铌冶炼工业废水处理中废渣的综合处理及利用研究[J].无机盐工业,2015,47(11):57-59. 被引量:1

1胡根火.钽铌湿法冶金分离方法评述[J].稀有金属与硬质合金,2015,43(1):29-32. 被引量:4

2杨大锦.2006年云南冶金年评[J].云南冶金,2007,36(2):39-51.

3章晋叔.钽铌资源企业在市场经济条件下的换位思维[J].有色冶金设计与研究,2008,29(1):1-2.

4王伟,李辉,郑培生.低品位钽铌原料的湿法冶金新工艺研究[J].稀有金属快报,2008,27(4):31-36. 被引量:10

5韩建设,刘建华,叶祥,凌诚.南方稀土水冶含氨废水综合回收工艺探讨[J].稀土,2008,29(6):69-75. 被引量:27

6韩建设,李丰,吴鹰.钽铌湿法冶炼工序成本及其核算管理探讨[J].稀有金属与硬质合金,2010,38(4):46-51.

7杨清宇,王琳丽,蔡锡元,韩建设.南方稀土湿法冶炼废水综合回收与治理研究(下)[J].有色冶金节能,2012,27(2):6-10. 被引量:4

8李新冬,黄万抚,肖芫华,张平.某钽铌矿钽铌资源综合回收试验研究[J].矿业研究与开发,2012,32(5):34-36. 被引量:2

9杨秀丽,王晓辉,孙青,徐娟,郑诗礼,魏昶.低浓度氢氟酸体系中MIBK萃取分离钽铌的研究[J].有色金属:冶炼部分,2012(11):26-29. 被引量:9

10黄江波,徐文炘.钽铌钨锡多金属矿冶炼项目污染防治措施探讨[J].广州化工,2013,41(3):109-111. 被引量:1

1杨继红.钽铌冶炼生产中余热资源回收和利用工艺研究[J].稀有金属与硬质合金,2013,41(4):58-61.

2熊一凡,戴和平.钽铌湿法冶炼配水洗涤监控系统设计[J].江西科学,2013,31(5):679-681.

3陈既明.浅谈钽铌湿法冶炼中稀有金属的回收[J].稀有金属与硬质合金,1997,25(4):56-58. 被引量:2

4张少辉,张碧田,何芬.紫外级氧化铪的生产工艺研究[J].稀有金属,2009,33(3):411-414. 被引量:1

5晏慧娟,唐德胜.传统工艺生产氧化钽(铌)除杂技术特点及研究进展[J].稀有金属与硬质合金,2016,44(4):14-19. 被引量:4

6杨秀丽,王晓辉,向仕彪,孙青,魏昶,郑诗礼.盐酸法富集钨渣中的钽和铌[J].中国有色金属学报,2013,23(3):873-881. 被引量:21

7吴声,廖春生,贾江涛,严纯华.P507体系反萃取条件对平衡负载稀土量的研究[J].中国稀土学报,2006,24(2):134-138. 被引量:12

8姚卫东,曹七林,伍尊中.钽铌湿法冶炼含氟废水的综合利用及其治理[J].材料研究与应用,2011,5(1):71-73. 被引量:5

9韩建设,张劲.钽铌水冶分解提取工艺及设备的进展[J].稀有金属与硬质合金,2003,31(4):27-31. 被引量:14

10郭永忠,胡根火,宋金华.离子交换法处理含氟氨氮硫酸根废水技术研究与应用[J].江西科学,2015,33(4):602-605. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF111.3[冶金工程—冶金物理化学]

Citation Information:

This article describes the situation in the recent years of extraction and stripping technology and equipment in hydrometallurgy of Ta & Nb in China,focusing on description of the latest development and techno-economic data in HF-H2SO4-Octanol-2 extraction-stripping system as well as the existing technical problems,related measures and ideas for the improvement and solution.

quote

GB/T 7714-2015 [1] HAN Jian-she, ZHOU Yong. Development of Ta & Nb Extraction and Stripping Technology and Equipment[J]. Rare Metals and Cemented Carbides, 2004(2): 15-20.
MLA [1] HAN Jian-she, and ZHOU Yong. "Development of Ta & Nb Extraction and Stripping Technology and Equipment." Rare Metals and Cemented Carbides, no. 2, 2004, pp. 15-20.
APA [1] HAN Jian-she, & ZHOU Yong. (2004). Development of Ta & Nb Extraction and Stripping Technology and Equipment. Rare Metals and Cemented Carbides(2), 15-20.
IEEE [1] HAN Jian-she and ZHOU Yong, "Development of Ta & Nb Extraction and Stripping Technology and Equipment," Rare Metals and Cemented Carbides, no. 2, pp. 15-20, 2004. keywords: {tantalum and niobium;extraction-stripping;Octano-2;technology;equipment}