Enhanced Mechanical Properties of Natural Rubber by Block Copolymer-Based Porous Carbon Fibers AITranslate
Abstract AITranslate
Nanosized particles have a large surface area to facilitate interfacial contact and thus are promising fillers for polymers. However, poor dispersion of nanoparticles limits the reinforcement effect. Herein, by rationally tailoring the internal porous structures, specific surface area, and surface chemistry, we prepared porous carbon fiber (PCF) filler from poly(acrylonitrile-block-methyl methacrylate) (PAN-b-PMMA) block copolymers. PCF had a three-dimensional porous network and provided improved filler–matrix interactions. Owing to the enhanced filler–matrix interlocking, large interfacial contact area, and strong interfacial affinity induced by nitrogen and oxygen doping, PCF was uniformly dispersed in rubber. Uncured nature rubber composites containing 5 parts of PCF per hundred parts of rubber (phr) showed 4.3 times higher Young’s modulus and twice the tensile strength at 300% strain compared to the neat rubber. PCF represents an effective reinforcing filler for polymers.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01329
Chinese Library Classification Number:
Citation Information:
Nanosized particles have a large surface area to facilitate interfacial contact and thus are promising fillers for polymers. However, poor dispersion of nanoparticles limits the reinforcement effect. Herein, by rationally tailoring the internal porous structures, specific surface area, and surface chemistry, we prepared porous carbon fiber (PCF) filler from poly(acrylonitrile-block-methyl methacrylate) (PAN-b-PMMA) block copolymers. PCF had a three-dimensional porous network and provided improved filler–matrix interactions. Owing to the enhanced filler–matrix interlocking, large interfacial contact area, and strong interfacial affinity induced by nitrogen and oxygen doping, PCF was uniformly dispersed in rubber. Uncured nature rubber composites containing 5 parts of PCF per hundred parts of rubber (phr) showed 4.3 times higher Young’s modulus and twice the tensile strength at 300% strain compared to the neat rubber. PCF represents an effective reinforcing filler for polymers.
quote
| GB/T 7714-2015 | [1] Wenqi Zhao, Zhen Xu, John Elliott, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01329. |
| MLA | [1] Wenqi Zhao, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01329. |
| APA | [1] Wenqi Zhao, Zhen Xu, John Elliott, Cindy S. Barrera, Zacary L. Croft, Haibo Zhao, Janice Tardiff, & Guoliang Liu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01329 |
| IEEE | [1] Wenqi Zhao, Zhen Xu, John Elliott, Cindy S. Barrera, Zacary L. Croft, Haibo Zhao, Janice Tardiff, and Guoliang Liu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01329. keywords: {block copolymer;porous carbon fiber;polymer composite;rubber;carbon black;interface} |