daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Addition and Correction to “Fluorocarbon Rubber-Based Inert Dry Adhesive for Applications under Harsh Conditions” AITranslate

AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01193

Chinese Library Classification Number:

Citation Information:

quote

GB/T 7714-2015 [1] Sung Ho Lee, Hyo Sung Kim, Hyun Woo Song, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01193.
MLA [1] Sung Ho Lee, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01193.
APA [1] Sung Ho Lee, Hyo Sung Kim, Hyun Woo Song, & Moon Kyu Kwak. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01193
IEEE [1] Sung Ho Lee, Hyo Sung Kim, Hyun Woo Song, and Moon Kyu Kwak, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01193.