Optical Second-Harmonic Polarimetry on Hf0.5Zr0.5O2/La0.67Sr0.33MnO3 Interfaces Optical Second-Harmonic Polarimetry on Hf0.5Zr0.5O2/La0.67Sr0.33MnO3 Interfaces AITranslate
Abstract AITranslate
The interface-induced second-harmonic generation from ferroelectric hafnium–zirconium oxide (Hf0.5Zr0.5O2) epitaxial thin films, buffered with a La0.67Sr0.33MnO3 bottom electrode, is analyzed as a function of input and output polarization angles and the azimuthal angle of the sample for several film thicknesses. It is shown that the signal is generated mainly from the buffer side of the interface, rather than from the ferroelectric side. However, the ferroelectric film affects significantly the nonlinear optical properties of the underlying ferromagnetic buffer electrode. Several mechanisms accounting for these observations are discussed, from oxygen migration, to an electrostatic effect, including a possible modulation of the La0.67Sr0.33MnO3 magnetization by the upper ferroelectric film.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00197
Chinese Library Classification Number:
Citation Information:
The interface-induced second-harmonic generation from ferroelectric hafnium–zirconium oxide (Hf0.5Zr0.5O2) epitaxial thin films, buffered with a La0.67Sr0.33MnO3 bottom electrode, is analyzed as a function of input and output polarization angles and the azimuthal angle of the sample for several film thicknesses. It is shown that the signal is generated mainly from the buffer side of the interface, rather than from the ferroelectric side. However, the ferroelectric film affects significantly the nonlinear optical properties of the underlying ferromagnetic buffer electrode. Several mechanisms accounting for these observations are discussed, from oxygen migration, to an electrostatic effect, including a possible modulation of the La0.67Sr0.33MnO3 magnetization by the upper ferroelectric film.
quote
| GB/T 7714-2015 | [1] Qiucheng Yu, Rohit Kumar, Deepak Kumar, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00197. |
| MLA | [1] Qiucheng Yu, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00197. |
| APA | [1] Qiucheng Yu, Rohit Kumar, Deepak Kumar, Alessia Sambri, Fabio Miletto Granozio, Ignasi Fina, Florencio Sánchez, Domenico Paparo, & Andrea Rubano. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00197 |
| IEEE | [1] Qiucheng Yu, Rohit Kumar, Deepak Kumar, Alessia Sambri, Fabio Miletto Granozio, Ignasi Fina, Florencio Sánchez, Domenico Paparo, and Andrea Rubano, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00197. keywords: {secondharmonic generation 2D ferroelectrics hafnium oxide thin films nonlinear optics} |