Dynamic Mechanical Properties and Adiabatic Shear Behavior of Ultrafine-Grained Pure Titanium AITranslate

School of Metallurgical Engineering,Xi'an University of Architecture & Technology,Xi'an 710055,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The ultrafine-grained (UFG) pure titanium prepared by composite deformation process (equalchannelangularpressingandrotary swaging) has many excellent properties such as high strength, excellent fatigue strength and good corrosion resistance, which can be widely used in aerospace, marine exploration, and petrochemical fields. Pure titanium is a metal that is highly sensitive to strain rate and temperature. Under dynamic impact loading such as high-speed impacts, dynamic fracture, and explosions, pure titanium presents macroscopic mechanical properties and microstructure evolution laws that are significantly different from those of conventional quasi-static loading. The difference between parts with ultrafine microstructure subjected to dynamic loading and quasi-static loading is mainly reflected in the inhomogeneity of the material deformation, non-isothermal, inertia effects and strong shock wave effects. Meanwhile, the adiabatic shear phenomenon is usually one of the concerns of researchers when studying the dynamic mechanical behavior of UFG materials, because the formation of an adiabatic shear band (ASB) is often a precursor to the fracture failure of a material in a dynamic impact process. In order to investigate the mechanical properties and adiabatic shear behavior of UFG pure titanium under dynamic loading, dynamic impact experiments were carried out at strain rates of 2000~3000 s-1 and temperatures of 300~450 ℃ by the split Hopkinson press bar (SHPB) technique, and the microstructure after dynamic deformation was characterized using scanning electron microscopy (SEM) and electron backscattering diffraction (EBSD) techniques. The results showed that UFG pure titanium exhibitednegative temperature sensitivity and positive strain rate sensitivity, and the true stress-true strain curve showedan obvious yielding effect. The true stress-true strain curve couldbe divided into three stages:the yielding, the work-hardening, and the localized deformation stage. Furthermore, all the curves showed a significant double-stress peak characteristic, and the softening phenomena appearance caused by the dislocation annihilation, rearrangement. Heat aggregation and the subsequent formation of the ASB werethe main reasons for the two stress reductions. With the increased of temperature, the yield strength under different strain rates decreased. When the temperature rose from 300 ℃ to 350 ℃, the yield strength of UFG pure titanium decreasedby 9.98%;From 350 ℃ to 400 ℃, the yield strength decreasedby 6.95;From 400 ℃ to 450 ℃, the yield strength decreasedby 7.91%, which was only 77% of the yield strength at 300 ℃. The values of strain rate sensitivity index m of UFG pure titanium in the range of strain rate of 2000~3000 s-1 were in the range of 0.12 to 0.17, which indicatedthat the flow stresses increased with the increased of strain rate under different impact loads, and UFG pure titanium hadstrong strain rate sensitivity. When the strain rate was larger than 2500 s-1, ASBs with an angle of 45° or 135° to the impact direction appeared in the UFG pure titanium specimens. There was a clear boundary between the shear band and the matrix. The width of the shear band increasedwith the increased of the strain rate and the decreased of the temperature. The width of the shear band increasedfrom 4.3 μm to 42.8 μm with the increased of the strain rate from 2000 to 3000 s-1 when the temperature was 350 ℃. And the width of the shear band decreasedfrom 48.7 μm to 16.4 μm with the increased of the temperature 300 to 450 ℃ when the strain rate was 2500 s-1. There were many microviods along the direction of shear band expansion in the ASB, and the convergence between adjacent microviods led to the formation of crack and fracture failure. The impact fracture morphology of UFG pure titanium under dynamic loading exhibitedthe typical parabolic shear dimples, and there were some microwoids in the shear dimples. The temperature hadlittle effect on the morphology of the shear dimples. The microhardness distribution near the adiabatic shear zone of UFG pure titanium hadthe same trend after dynamic loading in different conditions. The microhardness in the center of the ASB was the highest, which was obviously higher than that in the transition zone and the matrix. With the increased of strain rate, the microhardness of the center zone in the ASB, the transition zone and the matrix increased slightly. The microhardness of the center zone in the ASB was greatly affected by the temperature. The higher the temperature was, the lower the microhardness of the center zone in the ASB was. The microstructures of the shear band were mainly composed of a large number of fine dynamic recrystallizationequiaxed grains, which was induced by local high temperature and large deformation. With the increased of the temperature, dynamic recrystallization grain size in the ASB increasedfrom 332 nm at 300 ℃ to 1159 nm at 450 ℃. As the local softening points, dynamic recrystallization grains contributed to the adiabatic shear instability under the action of thermal-mechanical coupling and ultimately led to the fracture failure of UFG pure titanium.

KeyWords AITranslate

ultrafine-grained pure titanium dynamic mechanical behavior adiabatic shear band dynamic recrystallization

[1]Sun J L, Trimby P W, Yan F K, Liao X Z, Tao N R, Wang J T. Shear banding in commercial pure titanium deformed by dynamic compression [J].Acta Materialia, 2014, 79: 47.

[2]Xue Q, Meyers M A, Nesterenko V F. Self-organization of shear bands in titanium and Ti-6Al-4V alloy [J].Acta Materialia, 2002, 50(3): 575.

[3](赵永庆, 葛鹏, 辛社伟. 近五年钛合金材料研发进展 [J].中国材料进展, 2020, 39(z1): 527.)

Y Q Zhao, P Ge, W S Xing. Progresses of R&D on Ti-alloy materials in recent 5 years [J].Chinese Materials Progress, 2020, 39(z1): 527.

[4]Langdon G T. Achieving superplasticity in ultrafine-grained metals [J].Mechanics of Materials, 2013, 67: 1.

[5]Zhen G L, Ze R L. Non-aerospace application of Ti materials with a great many social and economic benefits in China [J].Materials Science & Engineering A, 2000, 280(1): 25.

[6]Elias C N, Lima J H C, Valiev R, Meyers M A. Biomedical applications of titanium and its alloys [J]. JOM, 2008, 60(3): 46.

[7](文超举, 刘春影, 舒佳玉, 陆婧, 王欢, 董强, 徐星星. 纯钛表面氧化石墨烯涂层的制备及生物学性能研究 [J].有色金属工程, 2024, 14(2): 1.)

C J Wen, C Y Liu, J Y Shu, J Lu, H Wang, Q Dong, X X Xu. Preparation and biological properties of graphene oxide coating on pure titanium surface [J].Nonferrous Metals Engineering, 2024, 14(2): 1.

[8]Li Z Z, Wang B F, Zhao S T, Valiev R Z, Vecchio K S, Meyers M A. Dynamic deformation and failure of ultrafine-grained titanium [J].Acta Materialia, 2017, 125: 210.

[9]Fintová S, Arzaghi M, Kuběna I, Sarrazin-Baudoux C. Fatigue crack propagation in UFG Ti grade 4 processed by severe plastic deformation [J].International Journal of Fatigue, 2017, 98: 187.

[10]G Y Z, Sun X Y, Wei Q, Li Y L. Compressive responses of ultrafine-grained titanium within a broad range of strain rates and temperatures [J].Mechanics of Materials, 2017, 115: 22.

[11]Khodabakhshi F, Mohammadi M, Gerlich A P. Stability of ultra-fine and nano-grains after severe plastic deformation: a critical review [J].Journal of Materials Science, 2021, 56(28): 15513.

[12]Long F W, Jiang Q W, Xiao L, Li X W. Compressive deformation behaviors of coarse-and ultrafine-grained pure titanium at different temperatures: a comparative study [J].Materials Transactions, 2011, 52(8): 1617.

[13]Meredith S C, Khan S A. Texture evolution and anisotropy in the thermo-mechanical response of UFG Ti processed via equal channel angular pressing [J].International Journal of Plasticity, 2012, 30–31: 202.

[14](张永皞, 范啟超, 孙明艳, 杨琴, 陈捷, 黄姝珂. 等径角挤压(ECAP)技术在NiTi基形状记忆合金中的研究进展 [J].稀有金属, 2023, 47(9): 1263.)

Y H Zhang, Q H Fan, M Y Sun, Q Yang, J Chen, S K Huang. Development of equal channel angular pressing in NiTi-based shape memory alloy [J].Chinese Journal of Rare Metals, 2023, 47(9): 1262.

[15](李帅康, 刘晓燕, 杨西荣, 张习祎. 超细晶材料动态力学性能及绝热剪切行为 [J].塑性工程学报, 2022, 29(6): 1.)

S K Li, X Y Liu, X R Yang, X Y Zhang. Dynamic mechanical properties and adiabatic shear behavior of ultrafine grained materials [J].Journal of Shaping Engineering, 2022, 29(6): 1.

[16](杨泽洲, 申勇峰, 冯晓伟, 薛文颖, 谢若泽, 胡艳辉. 超细晶D6A钢动态拉伸力学特性实验研究 [J].爆炸与冲击, 2022, 42(4): 65.)

Z Z Yang, Y F Shen, X W Fen, W Y Xue, R Z Xie, Y H Hu. Investigation on dynamic tensile properties of an ultrafine grained D6A steel [J].Explosions and Shocks, 2022, 42(4): 65.

[17]Long Y, Zhang W H, Peng L, Peng H Y, Li X Z, Huang X L. Mechanical behaviors of ultrafine-grained Ti-6Al-4V alloy during compression at various strain rates [J].Metallurgical and Materials Transactions, 2020, 51(9): 4765.

[18](宋鹏飞, 董新龙, 付应乾, 索涛. 基于等径通道挤压法的超细晶铜动态剪切变形行为实验研究 [J].兵工学报, 2018, 39(4): 763.)

P F Song, X L Dong, Y Q Fu, T Suo. Experimental research on dynamic shear behavior of ultrafine-grained copper prepared by equal channel angular pressing [J]. Journal of Ordnance Industry, 2018, 39(4): 763.

[19]Yang B, Zhou H G, Liu Z C, Huang H, Liu W H. Dynamic mechanical behavior and microstructure evolution of 7A52-T6 alloy at elevated temperatures [J].Journal of Physics: Conference Series, 2021, 1948(1): 012140.

[20]Zhang S X, Wang C Y, Zhilyaev P A, Korznikova E, Li S K, Raab I G, Langdon G T. Temperature and strain rate dependence of microstructural evolution and dynamic mechanical behavior in nanocrystalline Ti [J].Materials Science & Engineering A, 2015, 641: 29.

[21](刘晓燕, 强萌, 杨西荣, 罗雷. 室温ECAP变形纯钛孪生行为研究 [J].稀有金属, 2023, 47(10): 1352.)

X Y Liu, M Qiang, X R Yang, L Luo. Twinning behavior of pure titanium processed by ECAP at room temperature [J].Chinese Journal of Rare Metals, 2023, 47(10): 1352.

[22]Wang B F, Li J, Sun J Y, Wang X Y, Liu Z L. Shear localization and its related microstructural evolution in the ultrafine grained titanium processed by multi-axial compression [J].Materials Science and Engineering A, 2014, 612: 227.

[23](刘晓燕, 李帅康, 陈文文, 王子轩. TA1纯钛绝热剪切行为及变形机制 [J].有色金属工程, 2024, 14(7): 60.)

X Y Liu, S K Li, W W Chen, Z X Wang. Adiabatic shear behavior and deformation mechanism of TA1 pure titanium [J].Nonferrous Metals Engineering, 2024, 14(7): 60.

[24]Purnashis C, Singha M K, Vikrant T. Dynamic tensile and compressive behaviour of AA7475-T7351 alloy under different strain rates and temperatures [J].Structures, 2022, 46: 49.

[25](陈荣, 卢芳云, 林玉亮, 赵鹏铎, 李俊玲, 夏开文. 分离式Hopkinson压杆实验技术研究进展 [J].力学进展, 2009, 39(5): 576.)

R Chen, F Y Lu, Y L Lin, P D Zhao, J L Li, K W Xia. Critical review of split hopkinson pressure bar technique [J]. Progress in Mechanics, 2009, 39(5): 576.

[26]Wang L, Wang Y C, Zhilyaev A P, Korznikov A V, Li S K, Korznikov E, Langdon G T. Dynamic compressive behavior of ultrafine-grained pure Ti at elevated temperatures after processing by ECAP [J].Journal of Materials Science, 2014, 49(19): 46.

[27]Zhu Y C, Fan J X, LI Z L, Luo Y Y, Yong N. Study of strain rate sensitivity exponent and strain hardening exponent of Stypical titanium alloys [J].Materials Today Communications, 2022, 30: 103060.

[28]Shi W D, Lu S Y, Shen J H, Chen B, Umeda J, Wei Q M, Kondoh K, Li Y L. ASB induced phase transformation in high oxygen doped commercial purity Ti [J].Materials Science & Engineering A, 2022, 830: 142321.

[29](朱宁远, 陈秋明, 陈世豪, 左寿彬. TC11钛合金动态回复与动态再结晶高温本构模型研究 [J].有色金属科学与工程, 2024, 15(1): 58.)

N Y Zhu, Q M Chen, S H Chen, S B Zuo. Study on high-temperature constitutive model of TC11 titanium alloy dynamic recovery and dynamic recrystallization [J].Nonferrous Metals Science and Engineering, 2024, 15(1): 58.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY23080007

Chinese Library Classification Number:TG146.23

Citation Information:

The ultrafine-grained (UFG) pure titanium prepared by composite deformation process (equalchannelangularpressingandrotary swaging) has many excellent properties such as high strength, excellent fatigue strength and good corrosion resistance, which can be widely used in aerospace, marine exploration, and petrochemical fields. Pure titanium is a metal that is highly sensitive to strain rate and temperature. Under dynamic impact loading such as high-speed impacts, dynamic fracture, and explosions, pure titanium presents macroscopic mechanical properties and microstructure evolution laws that are significantly different from those of conventional quasi-static loading. The difference between parts with ultrafine microstructure subjected to dynamic loading and quasi-static loading is mainly reflected in the inhomogeneity of the material deformation, non-isothermal, inertia effects and strong shock wave effects. Meanwhile, the adiabatic shear phenomenon is usually one of the concerns of researchers when studying the dynamic mechanical behavior of UFG materials, because the formation of an adiabatic shear band (ASB) is often a precursor to the fracture failure of a material in a dynamic impact process. In order to investigate the mechanical properties and adiabatic shear behavior of UFG pure titanium under dynamic loading, dynamic impact experiments were carried out at strain rates of 2000~3000 s-1 and temperatures of 300~450 ℃ by the split Hopkinson press bar (SHPB) technique, and the microstructure after dynamic deformation was characterized using scanning electron microscopy (SEM) and electron backscattering diffraction (EBSD) techniques. The results showed that UFG pure titanium exhibitednegative temperature sensitivity and positive strain rate sensitivity, and the true stress-true strain curve showedan obvious yielding effect. The true stress-true strain curve couldbe divided into three stages:the yielding, the work-hardening, and the localized deformation stage. Furthermore, all the curves showed a significant double-stress peak characteristic, and the softening phenomena appearance caused by the dislocation annihilation, rearrangement. Heat aggregation and the subsequent formation of the ASB werethe main reasons for the two stress reductions. With the increased of temperature, the yield strength under different strain rates decreased. When the temperature rose from 300 ℃ to 350 ℃, the yield strength of UFG pure titanium decreasedby 9.98%;From 350 ℃ to 400 ℃, the yield strength decreasedby 6.95;From 400 ℃ to 450 ℃, the yield strength decreasedby 7.91%, which was only 77% of the yield strength at 300 ℃. The values of strain rate sensitivity index m of UFG pure titanium in the range of strain rate of 2000~3000 s-1 were in the range of 0.12 to 0.17, which indicatedthat the flow stresses increased with the increased of strain rate under different impact loads, and UFG pure titanium hadstrong strain rate sensitivity. When the strain rate was larger than 2500 s-1, ASBs with an angle of 45° or 135° to the impact direction appeared in the UFG pure titanium specimens. There was a clear boundary between the shear band and the matrix. The width of the shear band increasedwith the increased of the strain rate and the decreased of the temperature. The width of the shear band increasedfrom 4.3 μm to 42.8 μm with the increased of the strain rate from 2000 to 3000 s-1 when the temperature was 350 ℃. And the width of the shear band decreasedfrom 48.7 μm to 16.4 μm with the increased of the temperature 300 to 450 ℃ when the strain rate was 2500 s-1. There were many microviods along the direction of shear band expansion in the ASB, and the convergence between adjacent microviods led to the formation of crack and fracture failure. The impact fracture morphology of UFG pure titanium under dynamic loading exhibitedthe typical parabolic shear dimples, and there were some microwoids in the shear dimples. The temperature hadlittle effect on the morphology of the shear dimples. The microhardness distribution near the adiabatic shear zone of UFG pure titanium hadthe same trend after dynamic loading in different conditions. The microhardness in the center of the ASB was the highest, which was obviously higher than that in the transition zone and the matrix. With the increased of strain rate, the microhardness of the center zone in the ASB, the transition zone and the matrix increased slightly. The microhardness of the center zone in the ASB was greatly affected by the temperature. The higher the temperature was, the lower the microhardness of the center zone in the ASB was. The microstructures of the shear band were mainly composed of a large number of fine dynamic recrystallizationequiaxed grains, which was induced by local high temperature and large deformation. With the increased of the temperature, dynamic recrystallization grain size in the ASB increasedfrom 332 nm at 300 ℃ to 1159 nm at 450 ℃. As the local softening points, dynamic recrystallization grains contributed to the adiabatic shear instability under the action of thermal-mechanical coupling and ultimately led to the fracture failure of UFG pure titanium.

quote

GB/T 7714-2015 [1] Xiaoyan Liu, Yuliang Zhou, Shuaikang Li, et al. Dynamic Mechanical Properties and Adiabatic Shear Behavior of Ultrafine-Grained Pure Titanium[J]. Chinese Journal of Rare Metals, 2025, 49(11): 1659-1668. DOI:10.13373/j.cnki.cjrm.XY23080007.
MLA [1] Xiaoyan Liu, et al., "Dynamic Mechanical Properties and Adiabatic Shear Behavior of Ultrafine-Grained Pure Titanium." Chinese Journal of Rare Metals, vol. 49, no. 11, 2025, pp. 1659-1668, https://doi.org/10.13373/j.cnki.cjrm.XY23080007.
APA [1] Xiaoyan Liu, Yuliang Zhou, Shuaikang Li, Xirong Yang, Jingzhong Wang, & Lei Luo. (2025). Dynamic Mechanical Properties and Adiabatic Shear Behavior of Ultrafine-Grained Pure Titanium. Chinese Journal of Rare Metals, 49(11), 1659-1668. https://doi.org/10.13373/j.cnki.cjrm.XY23080007
IEEE [1] Xiaoyan Liu, Yuliang Zhou, Shuaikang Li, Xirong Yang, Jingzhong Wang, and Lei Luo, "Dynamic Mechanical Properties and Adiabatic Shear Behavior of Ultrafine-Grained Pure Titanium," Chinese Journal of Rare Metals, vol. 49, no. 11, pp. 1659-1668, 2025, doi: 10.13373/j.cnki.cjrm.XY23080007. keywords: {ultrafine-grained pure titanium;dynamic mechanical behavior;adiabatic shear band;dynamic recrystallization}