Process and Kinetics Study of Se Preparation by SO2 Reduction of SeO2 AITranslate

Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects of reaction temperature,H2SO4 concentration,SO2 flow rate and reaction time on the preparation process of Se by SO2 reduction of SeO2 were investigated,the kinetics of the process was stu-died,and the optimal process conditions and kinetic restrictive control links were obtained.The results show that under the conditions of the reaction temperature of 40 ℃,H2SO4 concentration of 1 mol/L,SO2 flow rate of 60 mL/min,and reaction time of 30 min,the reduction rate of Se reaches 99.73%,preparing Se with a purity of 99.85%.By controlling the conditions,different forms of Se can be obtained:amorphous red Se at low temperatures and well-crystallized black Se at high temperatures.The preparation process of Se by SO2 reduction of SeO2 conforms to the Avrami model,controlled by diffusion with an apparent activation energy of 1.98 kJ/mol,and described by the kinetics equation of-ln(1-X)=0.178×e-238/Tt1.276.

KeyWords AITranslate

Se SeO2 SO2 reduction kinetics process condition

1翟明国,吴福元,胡瑞忠,蒋少涌,李文昌,王汝成,王登红,齐涛,秦克章,温汉捷.战略性关键金属矿产资源:现状与问题[J].中国科学基金,2019,33(2):106-111. 被引量:196

2陈静静.硒粉密度的快速测定[J].玻璃与搪瓷,2001,29(2):40-41. 被引量:1

3孙悦,曲斌,全保刚.碳纳米管/二硒化钼有机玻璃的非线性吸收、非线性散射和光限幅特性[J].物理学报,2018,67(23):182-189. 被引量:2

4李栋,徐润泽,许志鹏,郭学益.硒资源及其提取技术研究进展[J].有色金属科学与工程,2015,6(1):18-23. 被引量:16

5杨洪英,李雪娇,佟琳琳,金哲男,殷璐,陈国宝.硝/硫混酸浸出铜阳极泥中硒的动力学(英文)[J].中国有色金属学报:英文版,2018,28(1):186-192. 被引量:6

6简锡明,谢永金.卡尔多炉处理铜阳极泥工艺评述[J].有色金属:冶炼部分,2014(10):20-23. 被引量:32

7涂百乐,张源,王爱荣.卡尔多炉处理铜阳极泥技术及应用实践[J].黄金,2011,32(3):45-48. 被引量:32

8路殿坤,畅永锋,杨红英,谢锋.高镍铜阳极泥中硒和碲的依次脱除(英文)[J].中国有色金属学报:英文版,2015,25(4):1307-1314. 被引量:11

9郭学益,许志鹏,田庆华,李栋.Optimization on selenium and arsenic conversion from copper anode slime by low-temperature alkali fusion process[J].中南大学学报:英文版,2017,24(7):1537-1543. 被引量:8

10李华健,刘秉国,宇文超,刘鹏,胡婷.响应曲面法优化微波硫酸化焙烧铜阳极泥脱硒[J].矿冶,2019,28(3):54-59. 被引量:7

1曾颜亮,彭珊,廖春发,刘付朋.水浸分铜渣超声波外场强化碱浸分碲动力学研究[J].稀有金属与硬质合金,2023,51(3):30-36. 被引量:1

2张学杨,徐浩亮,戴欢涛,游新秀,韦赵龙,曹苓玉.微波辐照木质素浸渍生物炭吸附CO_(2)性能[J].中国环境科学,2023,43(8):4427-4436.

3佘永明,冯笑,肖杰,张旭锋.复合材料锚杆成型用环氧树脂基体抗静电及力学性能研究[J].中国胶粘剂,2023,32(8):37-42.

4张雪婷,胡激江,卜志扬,李伯耿.DMC法聚氧化丙烯二醇的降解特性研究[J].聚氨酯工业,2023,38(4):14-19.

5杨智翔,殷海成,王金荣.硒化枯草芽孢杆菌肽聚糖的结构表征及体外抗氧化活性研究[J].河南工业大学学报:自然科学版,2023,44(4):84-91.

6张啟云,张武萍.微波密闭消解-乙醇增敏-串联质谱(ICP-MS/MS)法测定生物样品中的硒[J].中国无机分析化学,2023,13(10):1149-1153.

7陈雪凤,刘增亮,吴圣进,张雯龙,祁亮亮,潘庆流.秀珍菇富硒菌株筛选及其子实体富硒规律研究[J].中国食用菌,2023,42(4):34-40.

8姚怀智,刘放,余刚毅,郑雪楷,杨言,魏文清.液压启闭机-弧形闸门耦合动力学仿真与抑振研究[J].机械科学与技术,2023,42(8):1178-1183.

9胡中元,唐旭静,邢磊,张晓玲,刘彦龙.阿加曲班杂质的合成[J].精细化工中间体,2023,53(3):38-40.

10戴懿.自动发电控制系统数据采集同源性分析与研究[J].电力设备管理,2023(16):103-105.

Basic Information:

DOI:

Chinese Library Classification Number:TF843.5[冶金工程—有色金属冶金]

Citation Information:

The effects of reaction temperature,H2SO4 concentration,SO2 flow rate and reaction time on the preparation process of Se by SO2 reduction of SeO2 were investigated,the kinetics of the process was stu-died,and the optimal process conditions and kinetic restrictive control links were obtained.The results show that under the conditions of the reaction temperature of 40 ℃,H2SO4 concentration of 1 mol/L,SO2 flow rate of 60 mL/min,and reaction time of 30 min,the reduction rate of Se reaches 99.73%,preparing Se with a purity of 99.85%.By controlling the conditions,different forms of Se can be obtained:amorphous red Se at low temperatures and well-crystallized black Se at high temperatures.The preparation process of Se by SO2 reduction of SeO2 conforms to the Avrami model,controlled by diffusion with an apparent activation energy of 1.98 kJ/mol,and described by the kinetics equation of-ln(1-X)=0.178×e-238/Tt1.276.

quote

GB/T 7714-2015 [1] ZENG Yan-liang, ZOU Jian-bo, LIAO Chun-fa, et al. Process and Kinetics Study of Se Preparation by SO2 Reduction of SeO2[J]. Rare Metals and Cemented Carbides, 2023(4): 33-38.
MLA [1] ZENG Yan-liang, et al., "Process and Kinetics Study of Se Preparation by SO2 Reduction of SeO2." Rare Metals and Cemented Carbides, no. 4, 2023, pp. 33-38.
APA [1] ZENG Yan-liang, ZOU Jian-bo, LIAO Chun-fa, & LIU Fu-peng. (2023). Process and Kinetics Study of Se Preparation by SO2 Reduction of SeO2. Rare Metals and Cemented Carbides(4), 33-38.
IEEE [1] ZENG Yan-liang, ZOU Jian-bo, LIAO Chun-fa, and LIU Fu-peng, "Process and Kinetics Study of Se Preparation by SO2 Reduction of SeO2," Rare Metals and Cemented Carbides, no. 4, pp. 33-38, 2023. keywords: {Se;SeO;SO;reduction;kinetics;process condition}