Effects of Triton X-100 and OP-10 on Dispersivity of Nano-Sized Tungsten Carbide Powder in Absolute Ethanol AITranslate

School of Civil Engineering and Architecture,Wuhan Polytechnic University;School of Civil Engineering and Architecture,Wuhan Polytechnic University;School of Civil Engineering and Architecture,Wuhan Polytechnic University;School of Civil Engineering and Architecture,Wuhan Polytechnic University;School of Civil Engineering and Architecture,Wuhan Polytechnic University;School of Civil Engineering and Architecture,Wuhan Polytechnic University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nano-sized tungsten carbide powder is an important raw material for the preparation of ultrafine nano-cemented carbide.However,due to its large specific surface area,agglomeration is easy to occur,hindering the full play of its inherent excellent performance.To reduce the agglomeration of the nano-sized tungsten carbide powder,two surfactants,Triton X-100 and OP-10,were used for dispersion.Sedimentation experiment,absorbance test,particle size analysis and transmission electron microscope were used to study the dispersion performance of nano-sized tungsten carbide in absolute ethanol.The results show that when the mass fractions of Triton X-100 and OP-10 are 2% and 1.5% with ultrasonic times of 30 min and 50 min,respectively,the dispersion effect of the nano-sized tungsten carbide suspension reaches the best.Under the same ultrasonic time and with the same concentrations,OP-10 exhibits better dispersion effect than Triton X-100.Infrared analysis shows that Triton X-100 and OP-10 mainly reduce the agglomeration by adsorbing onto the surface of nano-sized tungsten carbide.

KeyWords AITranslate

nano-sized tungsten carbide Triton X-100 OP-10 surfactant dispersion

1赵玉超,唐建成,叶楠,周威威,韦朝龙,刘定军.添加剂及纳米WC粉含量对电镀WC-Cu复合材料性能的影响[J].中国有色金属学报:英文版,2020,30(6):1594-1604. 被引量:1

2吴霞,巫辉.Facile Preparation and Formation Mechanism of Uniform Silver Nanoparticles Using OP-10 as Emulsifier in Reverse Microemulsion[J].武汉理工大学学报:材料科学英文版,2011,26(1):38-42. 被引量:1

1袁军文,曾瑞霖,徐涛,尹超,董涛.含钒添加剂对纳米硬质合金性能的影响[J].硬质合金,2023,40(1):1-7.

2王红英,黄高明,刘澜涛,别安涛.适用于烧结环保砖的纳米TiO_(2)前驱体研究[J].江西建材,2023(5):67-70.

3王日升,吴岩佩,和学衡.矿用水力分级设备选型优化研究[J].黄金,2023,44(8):15-20.

4Weidong Huang,Linxia Zhang,Qiuping Yang,Zhimin Wang.Polyvinylpyrrolidone as an Efficient Stabilizer for Silver Nanoparticles[J].中国化学:英文版,2014,32(9):909-913.

5何继坤,马赛,曾惠钦,陆必志.碳化工艺对细晶碳化钨粉末特性与硬质合金晶粒异常长大的影响[J].硬质合金,2023,40(4):279-287.

6马晓燕,赵志西,谢青青,艾迪娅·阿不来提,夏米西亚·奴尔买买提,王丽萍.磁性复合材料的制备及其对二甲基胂酸的吸附[J].工业水处理,2023,43(8):66-73.

7张如杰,周广东,王建博,翁光东,雷东,龚文辉.氟化脱细胞兔主动脉制备人工小血管的可行性研究[J].上海交通大学学报:医学版,2023,43(7):814-820.

8徐依,张兵,杨艳,陈乐,赵田丽,王奇,张志娟,杨奔,昝斌,蔡军,王快社.GH4169合金在冷轧和热处理过程中的组织演变和力学性能[J].稀有金属材料与工程,2023,52(7):2385-2395.

9徐立乾,张芳,徐留俊,相建凯.数码绘图技术在古代彩画复原中的应用探索——以公输堂门板彩画复刻为例[J].西北美术:西安美术学院学报,2023(2):115-120.

10杜乐,胡娅洁,胡健,孙滔,云雪艳,董同力嘎.UV固化制备聚(L-乳酸)/壳聚糖薄膜及其热学、力学及抑菌性能研究[J].中国塑料,2023,37(8):38-44.

Basic Information:

DOI:

Chinese Library Classification Number:TB34[一般工业技术—材料科学与工程]

Citation Information:

Nano-sized tungsten carbide powder is an important raw material for the preparation of ultrafine nano-cemented carbide.However,due to its large specific surface area,agglomeration is easy to occur,hindering the full play of its inherent excellent performance.To reduce the agglomeration of the nano-sized tungsten carbide powder,two surfactants,Triton X-100 and OP-10,were used for dispersion.Sedimentation experiment,absorbance test,particle size analysis and transmission electron microscope were used to study the dispersion performance of nano-sized tungsten carbide in absolute ethanol.The results show that when the mass fractions of Triton X-100 and OP-10 are 2% and 1.5% with ultrasonic times of 30 min and 50 min,respectively,the dispersion effect of the nano-sized tungsten carbide suspension reaches the best.Under the same ultrasonic time and with the same concentrations,OP-10 exhibits better dispersion effect than Triton X-100.Infrared analysis shows that Triton X-100 and OP-10 mainly reduce the agglomeration by adsorbing onto the surface of nano-sized tungsten carbide.

quote

GB/T 7714-2015 [1] ZOU Lie, TAN Xiao-ming, LIU Jie-sheng, et al. Effects of Triton X-100 and OP-10 on Dispersivity of Nano-Sized Tungsten Carbide Powder in Absolute Ethanol[J]. Rare Metals and Cemented Carbides, 2023(4): 39-46.
MLA [1] ZOU Lie, et al., "Effects of Triton X-100 and OP-10 on Dispersivity of Nano-Sized Tungsten Carbide Powder in Absolute Ethanol." Rare Metals and Cemented Carbides, no. 4, 2023, pp. 39-46.
APA [1] ZOU Lie, TAN Xiao-ming, LIU Jie-sheng, FU Wan-wan, FENG Bo-wen, & ZHANG Man. (2023). Effects of Triton X-100 and OP-10 on Dispersivity of Nano-Sized Tungsten Carbide Powder in Absolute Ethanol. Rare Metals and Cemented Carbides(4), 39-46.
IEEE [1] ZOU Lie, TAN Xiao-ming, LIU Jie-sheng, FU Wan-wan, FENG Bo-wen, and ZHANG Man, "Effects of Triton X-100 and OP-10 on Dispersivity of Nano-Sized Tungsten Carbide Powder in Absolute Ethanol," Rare Metals and Cemented Carbides, no. 4, pp. 39-46, 2023. keywords: {nano-sized tungsten carbide;Triton X-100;OP-10;surfactant;dispersion}