Tellurium Recovery by Solvent Extraction from Copper Telluride Prepared with Copper Anode Slime AITranslate
Abstract AITranslate
Tellurium was enriched as copper telluride from copper anode slime. Tellurium and selenium were separated from chlorination leaching solution of copper telluride by solvent extraction, and tellurium was recovered. The results show that with 20% TOA+20% octanol+60% sulfonated kerosene (volume fraction) as the extractant,2 mol/L H2SO4 +HCl as the detergent and 200 g/L NH4 Cl solution as the stripping agent, tellurium can be effectively separated from selenium and copper. After stripping solution is reduced by sulfur dioxide or hydrazine hydrate,high purity tellurium powder is obtained.
KeyWords AITranslate
1张博亚,王吉坤,彭金辉.铜阳极泥中碲的回收[J].有色金属再生与利用,2006(5):14-15. 被引量:5
2Пашков Г Л. Гиганов Г П, Цереков Т Х. и др. Экстракция четырехвалентного теллура три-н-октилам ином из соляно - сернокислых растворов [J]. Сборник Научных Трудов ВНИИЦВЕТМЕТа.1968 .12: 28-32.
1廖先杰,杨绍利.加快攀西地区碲铋战略资源科学开发利用[J].材料保护,2013,46(S2):172-175. 被引量:1
2陈昆昆,郑雅杰.采用H_2SO_4-H_2O_2溶液从含贵金属的富碲渣中选择性提取碲[J].稀有金属,2013,37(6):946-951. 被引量:7
3邵丽雄,刁江,冀成庆.从含碲溶液中分离富集碲的研究进展[J].四川冶金,2018,40(3):9-12. 被引量:5
4何几文,刘欢,胡智东,张福元,华中胜.铜阳极泥中碲的回收研究进展[J].稀有金属与硬质合金,2018,46(4):20-28. 被引量:11
5李玉东,夏挺,叶钟林,李英伟,王鹏程.碲化铜物料提取精碲的试验研究[J].云南冶金,2019,48(1):49-52. 被引量:2
6刘波,李佳怡,丁云集,郑环东,张深根.报废光伏板回收利用的研究现状[J].稀有金属,2019,43(9):987-996. 被引量:4
7李超,刘述平,徐凌飞,黄雯孝,梁冠杰,何兰军.铜阳极泥中综合回收硒、碲、金等金属的研究[J].广州化工,2019,47(24):90-92. 被引量:3
8葛素志.废液中低含量稀贵稀散金属回收工艺[J].有色冶金设计与研究,2020,41(1):11-14. 被引量:1
9俞超杰,朱昊辰,黄菊文,贺文智,李光明.废弃光伏面板资源化利用的技术进展[J].上海节能,2021(1):13-19. 被引量:1
1罗正波,谭代娣,张圣南,李林,李家元.从铋渣中回收碲的工业试验[J].世界有色金属,2020(10):195-197.
2郑春到,林东和,黄冰,吴晓莉.从铂钯置换后液中回收碲工艺探索[J].铜业工程,2015(2):11-14. 被引量:1
3郭学益,许志鹏,李栋,田庆华.基于AOP协同氧化浸出碲渣中的碲和有价金属[J].中国有色金属学报,2018,28(1):167-174. 被引量:3
4郭学益,许志鹏,李栋,田庆华,张镇.从碲渣中选择性分离与回收碲的新工艺[J].中国有色金属学报,2018,28(5):1008-1015. 被引量:9
5邵丽雄,刁江,冀成庆.从含碲溶液中分离富集碲的研究进展[J].四川冶金,2018,40(3):9-12. 被引量:5
6宁瑞,余珊,房孟钊,李伟,李飞燕.提高分金工序中碲浸出率的试验研究[J].湖南有色金属,2019,35(2):39-41. 被引量:2
7吴展,李云峰,王亚东,胡琴.铜阳极泥回收碲的工艺优化研究[J].中国有色冶金,2019,48(6):6-9. 被引量:5
8刘静,柳成,曲永印.基于遗传算法优化BP神经网络的电解碲电源[J].北华大学学报:自然科学版,2020,21(2):257-262. 被引量:1
9廖春发,彭珊,邹耕,曾颜亮.基于RSM超声波-微波协同氧化浸出铜阳极泥分铜渣中碲的研究[J].稀有金属与硬质合金,2020,48(2):10-17. 被引量:4
10范兴祥,李英伟,杨坤彬,王家和.冶炼碱性渣制备高纯碲联产粗硒试验[J].有色金属:冶炼部分,2020(8):72-77. 被引量:1
1张慧宁,赖朝彬,崔健.电炉渣在NH_4Cl溶液浸出过程的自阻模型[J].有色金属科学与工程,2014,5(2):39-43. 被引量:3
2陆跃华,水承静.硫化银的氯盐浸出[J].贵金属,1998,19(2):23-27. 被引量:4
3李明建.洗涤剂用 4A 沸石合成的晶化导向剂制备及应用研究[J].广东工业大学学报,1997,0(3):34-37. 被引量:4
4韦建华,肖连生,曾理.碱性条件下钨萃取过程中铝的行为研究[J].中国钨业,2016,31(2):43-48.
5张小林,李伟,宁瑞.用Na_2SO_3与NH_3分银实验研究[J].有色金属科学与工程,2014,5(1):63-67. 被引量:10
6郭学益,康思琦,傅崇说,张多默,崔京守.氯化铵溶液中还原浸出海洋锰结核[J].有色金属,1996,48(2):50-53. 被引量:6
7巨佳.水合肼还原铜氨废液制取纳米铜粉[J].中国材料进展,2010,29(7):53-56. 被引量:1
8倪迎瑞,李中玺,李海涛,秦靖,张圣杰,薛振宇.从金电解阳极泥中湿法回收金银试验研究[J].湿法冶金,2014,33(2):115-117. 被引量:6
9张华.从富银渣中回收银的方法研究[J].四川有色金属,2000(1):32-36. 被引量:12
10刘建,闫英桃,邵海欣,陈长江.CL-TBP萃淋树脂吸附分离镓(Ga)研究[J].化学通报,2001,64(2):119-121. 被引量:10
Basic Information:
DOI:
Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]
Citation Information:
Tellurium was enriched as copper telluride from copper anode slime. Tellurium and selenium were separated from chlorination leaching solution of copper telluride by solvent extraction, and tellurium was recovered. The results show that with 20% TOA+20% octanol+60% sulfonated kerosene (volume fraction) as the extractant,2 mol/L H2SO4 +HCl as the detergent and 200 g/L NH4 Cl solution as the stripping agent, tellurium can be effectively separated from selenium and copper. After stripping solution is reduced by sulfur dioxide or hydrazine hydrate,high purity tellurium powder is obtained.
quote
| GB/T 7714-2015 | [1] ZHAO Jian, DING Cheng-fang, HU Hai-nan, et al. Tellurium Recovery by Solvent Extraction from Copper Telluride Prepared with Copper Anode Slime[J]. Rare Metals and Cemented Carbides, 2012(4): 1-3. |
| MLA | [1] ZHAO Jian, et al., "Tellurium Recovery by Solvent Extraction from Copper Telluride Prepared with Copper Anode Slime." Rare Metals and Cemented Carbides, no. 4, 2012, pp. 1-3. |
| APA | [1] ZHAO Jian, DING Cheng-fang, HU Hai-nan, & ZHAO Qin-sheng. (2012). Tellurium Recovery by Solvent Extraction from Copper Telluride Prepared with Copper Anode Slime. Rare Metals and Cemented Carbides(4), 1-3. |
| IEEE | [1] ZHAO Jian, DING Cheng-fang, HU Hai-nan, and ZHAO Qin-sheng, "Tellurium Recovery by Solvent Extraction from Copper Telluride Prepared with Copper Anode Slime," Rare Metals and Cemented Carbides, no. 4, pp. 1-3, 2012. keywords: {tellurium;copper telluride;chlorination;extraction separation;separation of selenium and tellurium;TOA tellurium metal powder} |