Abstract AITranslate
Coated P507 impregnated resin was prepared with P507 as the extractant, HZ818 macroporous resin as the matrix,polyvinyl alcohol as the coating material and boric acid as the crosslinking agent. The adsorption mechanism of the sample for indium (Ⅲ) in sulfuric acid was investigated by using saturation capacity method and constant molecular series method. Uncoated and coated P507 impregnated resin were characterized by IR spectra before and after indium (Ⅲ ) adsorption. The results show that the process of coated P507 impregnated resin adsorption for indium ( Ⅲ ) in sulfuric acid is contributed to the joint action of cation exchange and coordination reaction.
KeyWords AITranslate
1王树楷.铟的应用与提取进展[J].中国工程科学,2008,10(5):85-94. 被引量:22
2刘军深,袁延旭.P507萃淋树脂在盐酸介质中吸附铟(Ⅲ)的性能[J].稀有金属与硬质合金,2008,36(4):1-4. 被引量:11
3Nalan Kabay, Jose Luis Cortina, Andrzej Trochimczuk, et al. Soivent-impregnated resins (SIRs)--Methods of preparation and their applications[J]. Reactive & Func- tional Polymers, 2010,7 :484-496.
4Trochimczuk A W, Kabay N, Arda M, et al. Stabilization of solvent impregnated resins (SIRS) by coating with water soluble polymers and chemical crosslinking [J]. Reactive & Functional Polymers,2004,59.. 1-7.
5Yuan Yanxu, Liu Junshen, Zhou Baoxue, et al. Synthesis of coated solvent impregnated resin for the adsorption of indium (Ⅲ)[J]. Hydrometallurgy, 2010,101 : 148-155.
6顾学民,龚毅生,臧希波,等.无机化学丛书(第二版)[M].北京:科学出版社,1990.517.
7包昌年.用2-乙基己基膦酸单(2-乙基己基)酯自硫酸溶液中萃取铟的机理研究[J].化学学报,1984,42:1210-1213.
1魏士龙,刘军深,高学珍,陈晓亮.TBP浸渍树脂在氯化物介质中吸附铁(Ⅲ)的性能及机理[J].鲁东大学学报:自然科学版,2013,29(3):218-222.
2陈文,张亚雷,周雪飞,代朝猛.水中铟(Ⅲ)的分离富集及资源化回用研究进展[J].化工进展,2015,34(7):2009-2015. 被引量:3
3陈晓亮,刘军深,刘清清,徐翠萍.包覆型P507浸渍树脂的制备及吸附铟(Ⅲ)的性能[J].稀有金属,2016,40(8):825-830. 被引量:3
4高学珍,魏士龙,曹鹏,刘军深.P507/D301浸渍树脂吸附铟(Ⅲ)的性能研究[J].鲁东大学学报:自然科学版,2017,33(4):340-345. 被引量:4
1姚艳清,刘四清,董旭,刘海林.铟的富集分离工艺技术现状及展望[J].金属矿山,2016,45(9):132-136. 被引量:7
2高学珍,魏士龙,曹鹏,刘军深.P507/D301浸渍树脂吸附铟(Ⅲ)的性能研究[J].鲁东大学学报:自然科学版,2017,33(4):340-345. 被引量:4
3刘欢,华中胜,何几文,唐泽韬,张伟伟,吕辉鸿.废弃氧化铟锡中铟的回收技术综述[J].材料导报,2018,32(11):1916-1923. 被引量:5
4万媛媛,李长振,杜志林,高学珍,刘训恿,刘军深.盐酸介质中Cyanex 923浸渍树脂吸附Ga(Ⅲ)的性能研究[J].鲁东大学学报:自然科学版,2018,34(4):333-337. 被引量:1
5杜志林,李长振,万媛媛,高学珍,刘训恿,刘军深.CA-100/HZ802浸渍树脂在硫酸体系中吸附Ga(Ⅲ)[J].曲阜师范大学学报:自然科学版,2019,45(1):77-81.
6李皓,刘美林,温建康.广西某锌冶炼厂萃原液中铟的离心萃取研究[J].稀有金属,2019,43(4):420-427. 被引量:2
7周澳,李熙腾,李鑫培,巨少华,张利华.3D打印多通道微反应器用于萃取分离In^(3+)和Fe^(3+)[J].化工进展,2019,38(5):2093-2102. 被引量:5
8陈晓亮,刘军深,高学珍,魏士龙,张妍.伯胺N1923溶剂浸渍树脂吸附In(Ⅲ)的性能及机理[J].鲁东大学学报:自然科学版,2020,36(4):366-370.
9唐洋洋,李林波,王超,杨潘,冯璐.含铟锌渣湿法回收铟工艺进展[J].有色金属工程,2021,11(4):55-62. 被引量:3
10冯建,戴松桓,徐羽靓,谢蒙,李敏.UiO-66-(COOH)2对水溶液中In(Ⅲ)的吸附性能[J].安全与环境学报,2021,21(1):365-372. 被引量:1
1谌英武.用P507萃取剂分离磷矿石中的稀土元素研究[J].武汉化工学院学报,1999,21(2):1-3. 被引量:2
2张瑞英,郝茜,孙晔.离子色谱法测定碳酸稀土和氯化稀土中硫酸根[J].稀土,2007,28(1):52-54. 被引量:5
3王月,王运东,靖宇,陈继,刘郁.Microcapsules containing ionic liquid [A336][P507] for La^(3+)/Sm^(3+)/Er^(3+)recovery from dilute aqueous solution[J].稀土学报:英文版,2016,34(12):1260-1268. 被引量:2
4汤惠民,刘慧中.伯胺N1923从硫酸溶液中萃取钪(Ⅲ)的机理研究[J].同济大学学报:自然科学版,1991,19(1):103-108.
5张邦劳,张昕,杨祖培,樊锁强,荆雪育.二(2-乙基已基)亚砜萃取钼的机理研究[J].陕西师大学报:自然科学版,1995,23(2):51-54. 被引量:1
6韩维和,张安运,钱博,李芳,余志峰.1,4-双(1′-苯基-3′-甲基-5′-氧代吡唑-4′-基)丁二酮-〔1,4〕萃取稀土的研究[J].陕西师范大学学报:自然科学版,1996,24(2):5-5. 被引量:1
7张梅,刘振祥,谢侃,杜雪岩,李文超.CeO_2包覆TiO_2的XPS研究[J].北京科技大学学报,1999,21(4):331-333. 被引量:2
8曾平,胡净宇.伯胺N1923萃取钼的机理研究[J].高等学校化学学报,1994,15(11):1588-1591. 被引量:7
9张荣馀,秦秀清.烷氧基甲基膦酸单烷基酯萃取稀土元素[J].稀土,1995,16(6):19-24.
10崔丹,段淑红,孙铁.CuSO_4-氨化P_(507)-n-C_6H_(14)体系平衡常数的计算[J].高等学校化学学报,1998,19(4):598-602.
Basic Information:
DOI:
Chinese Library Classification Number:O647.3[理学—物理化学]
Citation Information:
Coated P507 impregnated resin was prepared with P507 as the extractant, HZ818 macroporous resin as the matrix,polyvinyl alcohol as the coating material and boric acid as the crosslinking agent. The adsorption mechanism of the sample for indium (Ⅲ) in sulfuric acid was investigated by using saturation capacity method and constant molecular series method. Uncoated and coated P507 impregnated resin were characterized by IR spectra before and after indium (Ⅲ ) adsorption. The results show that the process of coated P507 impregnated resin adsorption for indium ( Ⅲ ) in sulfuric acid is contributed to the joint action of cation exchange and coordination reaction.
quote
| GB/T 7714-2015 | [1] GAO Xue-zhen, LIU Jun-shen, LI Hai-mei, et al. Adsorption Mechanism of Coated Impregnated Resin for Indium (Ⅲ) in Sulfuric Acid[J]. Rare Metals and Cemented Carbides, 2012(4): 4-6. |
| MLA | [1] GAO Xue-zhen, et al., "Adsorption Mechanism of Coated Impregnated Resin for Indium (Ⅲ) in Sulfuric Acid." Rare Metals and Cemented Carbides, no. 4, 2012, pp. 4-6. |
| APA | [1] GAO Xue-zhen, LIU Jun-shen, LI Hai-mei, & WEI Shi-long. (2012). Adsorption Mechanism of Coated Impregnated Resin for Indium (Ⅲ) in Sulfuric Acid. Rare Metals and Cemented Carbides(4), 4-6. |
| IEEE | [1] GAO Xue-zhen, LIU Jun-shen, LI Hai-mei, and WEI Shi-long, "Adsorption Mechanism of Coated Impregnated Resin for Indium (Ⅲ) in Sulfuric Acid," Rare Metals and Cemented Carbides, no. 4, pp. 4-6, 2012. keywords: {P507 extractant coated impregnated resinindium ( Ⅲ );adsorption mechanism} |