Na-Rich Disordered Rock Salt Oxyfluoride Cathode Materials for Sodium Ion Batteries AITranslate
Abstract AITranslate
The existing classes of Na-based cathode materials and their chemistries are still limited, mainly with respect to the increasing demand for alternative post-Li technologies. In this letter, a newly synthesized Na-rich disordered rock salt (DRS) oxyfluoride with the nominal composition Na2MnO2F is reported as a cathode candidate for Na-ion batteries (SIBs). Rietveld refinement analysis confirmed that the synthesized compound has a DRS structure with larger lattice compared to Li-rich homologues. During the first cycle, up to 1.7 Na+/f.u. can be extracted at a slow rate, while a better capacity retention and cycling stability are obtained at high rate, reminiscent of electrode–electrolyte interaction. Further, X-ray absorption fine structure (operando and ex situ) confirmed the Mn oxidation state evolution upon cycling in agreement with the cyclic voltammetry redox profile, emphasizing the reversible Na+ (de)insertion and change of the Mn local ordering. This work is an additional input to the limited series of cathode candidates for SIBs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.2c00906
Chinese Library Classification Number:
Citation Information:
The existing classes of Na-based cathode materials and their chemistries are still limited, mainly with respect to the increasing demand for alternative post-Li technologies. In this letter, a newly synthesized Na-rich disordered rock salt (DRS) oxyfluoride with the nominal composition Na2MnO2F is reported as a cathode candidate for Na-ion batteries (SIBs). Rietveld refinement analysis confirmed that the synthesized compound has a DRS structure with larger lattice compared to Li-rich homologues. During the first cycle, up to 1.7 Na+/f.u. can be extracted at a slow rate, while a better capacity retention and cycling stability are obtained at high rate, reminiscent of electrode–electrolyte interaction. Further, X-ray absorption fine structure (operando and ex situ) confirmed the Mn oxidation state evolution upon cycling in agreement with the cyclic voltammetry redox profile, emphasizing the reversible Na+ (de)insertion and change of the Mn local ordering. This work is an additional input to the limited series of cathode candidates for SIBs.
quote
| GB/T 7714-2015 | [1] Yasaman Shirazi Moghadam, Abdel El Kharbachi, Yang Hu, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c00906. |
| MLA | [1] Yasaman Shirazi Moghadam, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c00906. |
| APA | [1] Yasaman Shirazi Moghadam, Abdel El Kharbachi, Yang Hu, Kai Wang, Stéphanie Belin, & Maximilian Fichtner. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c00906 |
| IEEE | [1] Yasaman Shirazi Moghadam, Abdel El Kharbachi, Yang Hu, Kai Wang, Stéphanie Belin, and Maximilian Fichtner, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c00906. |