daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Effects of Nb Content on Mechanical Properties of the High Phosphorus-bearing Weathering Steel AITranslate

Key Laboratory of Comprehensive Utilization of Polymetals, Inner Mongolia University of Science and Technology, Bayan Obo, Inner Mongolia Autonomous Region;Key Laboratory of Comprehensive Utilization of Polymetals, Inner Mongolia University of Science and Technology, Bayan Obo, Inner Mongolia Autonomous Region;Key Laboratory of Comprehensive Utilization of Polymetals, Inner Mongolia University of Science and Technology, Bayan Obo, Inner Mongolia Autonomous Region;Key Laboratory of Comprehensive Utilization of Polymetals, Inner Mongolia University of Science and Technology, Bayan Obo, Inner Mongolia Autonomous Region
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Investigation was made of the effects of Nb content on microstructure, strength and impact toughness of the high phosphorus bearing weathering steel by microstructure analysis, tensile test and impact test. The results show that with the increase of Nb content, the microstructure of the high phosphorus-bearing weathering steel becomes more uniform with weaker band like distribution, yield strength and tensile strength are improved at first and tend to be stable, and longitudinal impact energy in creases at first and then decreases, while transverse impact energy is the opposite. The high phosphorus bearing weathering steel with 0. 042 % Nb has the microstructure of obviously weakened band-like distribu tion,with the smallest average grain size,the maximum yield strength, tensile strength and longitudinal impact energy,and the minimum transverse impact energy. The high phosphorus-bearing weathering steel containing 0. 090% Nb,with no obvious band-like distributed microstructure, has the same strength, the narrowed anisotropy of impact toughness,compared with the one containing 0. 042% Nb.

KeyWords AITranslate

high phosphorus-bearing weathering steel Nb microstructure yield strength tensile strength impact toughness

1李德强,周宏伟.铁道车辆用09CuPTiRE耐候钢在本钢的开发试制[J].本钢技术,2001(4):11-15. 被引量:2

2郭艳,郭华,左军,常军,徐建中,王丹.攀钢09CuPRE热轧耐候板的工艺及性能[J].钢铁钒钛,1998,19(1):32-37. 被引量:6

3Johnson J B. Short-term atmospheric corrosion of steel at two weather and pollution monitored sites[J]. Corrosion Science, 1997,17 = 691-700.

4陈小平,王向东,江社明,李春艳.晶粒尺寸对耐候钢抗大气腐蚀性能的影响[J].材料保护,2005,38(7):14-17. 被引量:15

5于千.耐候钢发展现状及展望[J].钢铁研究学报,2007,19(11):1-4. 被引量:76

6梁彩凤,侯文泰.合金元素对碳钢和低合金钢在大气中耐腐蚀性的影响[J].中国腐蚀与防护学报,1997,17(2):87-92. 被引量:38

7DeardoAJ.铌科学与技术[M].北京:冶金工业出版社,2003.271-313..

1张贺佳,张俊粉,李吉伟,王宝华,李国民,魏亮亮.Cu合金化对Cr9Mo1钢耐腐蚀及力学性能的影响[J].材料科学与工艺,2018,26(4):73-79. 被引量:6

2张贺佳,张春雷,王琪,张俊粉.含Cu超耐腐蚀钢筋Cr9Mo1的实验研究[J].北方钒钛,2019,0(1):51-56.

1焦海东,刘丽霞,彭军,郑丽丽,吴世杰.国内钢的显微组织耐蚀性研究概述[J].中国铸造装备与技术,2020,55(1):5-12. 被引量:1

2闫志波,陈红卫,贺会敏,王向明.Ni-Cu-Nb复合60Si2Cr弹簧钢的奥氏体连续冷却转变[J].石家庄职业技术学院学报,2020,32(2):5-9.

3于驰,王宏岩,高秀华,王宏伟.冷却工艺对货油舱用耐蚀钢组织性能的影响[J].材料科学与工艺,2020,28(4):31-40. 被引量:1

4于晗.热处理工艺对高强高导铜合金组织级性能的影响[J].材料科学与工艺,2020,28(5):31-37. 被引量:3

5闫志波,赵海涛,陈红卫.301不锈钢螺栓断裂原因分析[J].锻压技术,2020,45(10):7-12. 被引量:2

6侯元盛,左景辉,刘忱,刘常升.货油舱上甲板用耐蚀钢的腐蚀行为[J].腐蚀与防护,2022,43(2):43-47.

1陈俊,周国平,刘振宇,邱以清,王国栋.退火时间对0.15%P铸轧耐候钢冷轧薄带组织性能的影响[J].材料研究学报,2011,25(3):268-272.

2周国平,王斌,陈俊,刘振宇,邱以清,王国栋.铸轧高磷耐候钢薄带低温冲击韧性[J].物理测试,2010,28(2):10-15. 被引量:1

3周国平,于世川,刘振宇,陈俊,邱以清,王国栋.高磷耐候钢铸轧薄带的组织和深拉伸性能[J].钢铁研究学报,2011,23(1):36-41. 被引量:1

4刘赓,张深根,刘波.加热速率对不同状态低合金高强钢Q&P处理后组织和性能的影响[J].机械工程材料,2016,40(12):92-98. 被引量:2

5S.M.ABBASI,A.MOMENI.热加工和后处理对Ti-6Al-4V合金显微组织和拉伸性能的影响(英文)[J].中国有色金属学报:英文版,2011,21(8):1728-1734. 被引量:5

6许剑伟,黄旭,曹京霞.固溶温度与轧制温度对Ti_3Al基合金的组织与性能的影响[J].稀有金属,2004,28(1):50-53. 被引量:1

7白兴国,梅丽,陈建伟,宗卫兵,张传友.淬火温度对石油套管用钢27MnCrV冲击韧性的影响[J].特殊钢,2010,31(2):63-65. 被引量:2

8韩孝永.浅谈压力容器用钢的生产[J].梅山科技,2005(1):6-9. 被引量:1

9裴悦凯,马党参,刘宝石,陈再枝,周荣,周健.锻造比对H13钢组织和力学性能的影响[J].钢铁,2012,47(2):81-86. 被引量:18

10杨海林,杨秀芹.82mm 14Cr1MoR钢板工业性热处理工艺试验[J].特殊钢,2005,26(3):48-50. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TG141[金属学及工艺—金属材料]

Citation Information:

Investigation was made of the effects of Nb content on microstructure, strength and impact toughness of the high phosphorus bearing weathering steel by microstructure analysis, tensile test and impact test. The results show that with the increase of Nb content, the microstructure of the high phosphorus-bearing weathering steel becomes more uniform with weaker band like distribution, yield strength and tensile strength are improved at first and tend to be stable, and longitudinal impact energy in creases at first and then decreases, while transverse impact energy is the opposite. The high phosphorus bearing weathering steel with 0. 042 % Nb has the microstructure of obviously weakened band-like distribu tion,with the smallest average grain size,the maximum yield strength, tensile strength and longitudinal impact energy,and the minimum transverse impact energy. The high phosphorus-bearing weathering steel containing 0. 090% Nb,with no obvious band-like distributed microstructure, has the same strength, the narrowed anisotropy of impact toughness,compared with the one containing 0. 042% Nb.

quote

GB/T 7714-2015 [1] DONG Chen, ZHAO Zeng-wu, LI Yan, et al. Effects of Nb Content on Mechanical Properties of the High Phosphorus-bearing Weathering Steel[J]. Rare Metals and Cemented Carbides, 2014(2): 59-63.
MLA [1] DONG Chen, et al., "Effects of Nb Content on Mechanical Properties of the High Phosphorus-bearing Weathering Steel." Rare Metals and Cemented Carbides, no. 2, 2014, pp. 59-63.
APA [1] DONG Chen, ZHAO Zeng-wu, LI Yan, & LI Bao-wei. (2014). Effects of Nb Content on Mechanical Properties of the High Phosphorus-bearing Weathering Steel. Rare Metals and Cemented Carbides(2), 59-63.
IEEE [1] DONG Chen, ZHAO Zeng-wu, LI Yan, and LI Bao-wei, "Effects of Nb Content on Mechanical Properties of the High Phosphorus-bearing Weathering Steel," Rare Metals and Cemented Carbides, no. 2, pp. 59-63, 2014. keywords: {high phosphorus-bearing weathering steel;Nb;microstructure;yield strength;tensile strength;impact toughness}