Study on the Density of NdF_3-LiF-Nd_2O_3 System AITranslate
Abstract AITranslate
The density of NdF 3 LiF melts was measured by Archimedes method in the present paper.The regression equation of the density dependence on the concentration of NdF 3 and temperature was gained by means of two factor quadratic regression orthogonal design.And the effects of the concentration of NdF 3 and temperature on the density of the melts were discussed.Moreover,the influences of the addition of Nd 2O 3 on the density were investigated.
KeyWords AITranslate
1别列耶夫AM.熔盐物理化学[M].北京:中国工业出版社,1963.79.
2路贵民,张日强.NdF_3—LiF系融盐密度的数学模型及BaF_2添加剂对其影响的研究[J].有色矿冶,1990(3):35-39. 被引量:4
3郭春泰,杜森林,李洁,鲁化一,赵连山,唐定骧.NdF_3-LiF-BaF_2熔盐体系的密度和粘度[J].中国稀土学报,1989,7(1):7-11. 被引量:8
4许文江,潘伦桃,王向东,舒永春,毛襄萍,施文峰.氟钽酸钾及其相关熔盐体系的密度[J].稀有金属,1999,23(5):349-352. 被引量:6
1张亚楠,李静,柴登鹏,高玉莹,王成智,侯光辉,于强,刘利英,张芬萍,刘秀.PrF3-NdF3-LiF-Pr6O11-Nd2O3体系熔盐电导率性能研究[J].稀土,2020,0(1):92-96. 被引量:2
2石富.稀土电解槽的研究现状及发展趋势[J].中国稀土学报,2007,25(S1):70-76. 被引量:22
3刘中兴,齐素慈.3kA钕电解槽流场的数值模拟[J].稀有金属材料与工程,2007,36(2):194-196. 被引量:19
4刘中兴,张桢,伍永福,洪昌勇,刘宇慧,张惠,王亮亮.稀土钕氧化物电解槽内液—液两相流动研究[J].有色金属:冶炼部分,2011(5):27-30. 被引量:3
5刘宇新,刘中兴,杨立军.稀土电解槽气液两相流动数值模拟[J].有色金属:冶炼部分,2011(10):27-30. 被引量:15
6王军,张作良,涂赣峰,吴文远.10kA底部阴极稀土熔盐电解槽流场的模拟[J].稀土,2012,33(2):64-68. 被引量:5
7郑鑫,朱卫花,彭光怀,梁金,张小联.NdF_3-LiF-Nd_2O_3体系熔盐电导率的研究[J].中国钨业,2013,28(1):30-33. 被引量:7
8朱桥,王秀峰.高温熔体密度测量研究进展[J].硅酸盐通报,2013,32(6):1087-1091. 被引量:5
9刘中兴,董云芳,伍永福,何金辉,许立勇.60kA底部阴极稀土电解槽阳极倾角对流场影响的数值模拟[J].稀土,2013,34(4):21-24. 被引量:11
10董云芳,刘中兴,伍永福,许立勇,何金辉.60kA底部阴极稀土电解槽极距的模拟优化[J].有色金属:冶炼部分,2013(10):32-35. 被引量:9
1王权,王玉峰,赵海营,夏云.20钢与Monel400合金在NdF_(3)-LiF熔盐环境中的耐蚀性研究[J].稀土,2022,43(1):127-133.
2廖春发,郭超,林觉远,蔡伯清,王旭.电流密度对稀土熔盐电解影响的研究进展[J].稀土,2021(1):122-128. 被引量:4
3张亚楠,李静,柴登鹏,高玉莹,王成智,侯光辉,于强,刘利英,张芬萍,刘秀.PrF3-NdF3-LiF-Pr6O11-Nd2O3体系熔盐电导率性能研究[J].稀土,2020,0(1):92-96. 被引量:2
4笪宗扬,李二斗,候少春,丁艳蓉.稀土氧化物电解过程氟化氢尾气干法吸附实验研究[J].环境工程,2023,41(S01):372-376.
5石富.钕电解的能耗及优化设计研究[J].中国稀土学报,2007(S1):37-39.
6石富.稀土电解槽的研究现状及发展趋势[J].中国稀土学报,2007,25(S1):70-76. 被引量:22
7伍永福,刘中兴,李姝婷,朱虹.稀土熔盐电解槽内多相流动数值模拟[J].过程工程学报,2009,9(S1):410-414. 被引量:5
8刘中兴,韩文帅,伍永福,胡永胜,鞠阳.60kA底部阴极稀土电解槽电场数值模拟[J].稀有金属与硬质合金,2015,43(1):26-28. 被引量:4
9刘中兴,齐素慈.3kA钕电解槽流场的数值模拟[J].稀有金属材料与工程,2007,36(2):194-196. 被引量:19
10闫晓明,刘中兴,伍永福,刘宇新,张海玲.10kA全埋式稀土电解槽的电场模拟[J].内蒙古科技大学学报,2010,29(3):214-217. 被引量:5
1刘奎仁,陈建设,魏绪钧,郑天仓,谢丽英,孔向民.NdF_3-LiF-Nd_2O_3体系表面张力的研究[J].稀土,2000,21(6):37-39. 被引量:10
2杨中兵,刘奎仁,刘民.NdF_3-LiF-Nd_2O_3体系表面张力数学模型的研究[J].黄金学报,2001,3(1):40-42.
3郑天仓,任永红,毛裕文.NdF_3-LiF-Nd_2O_3体系粘度的研究[J].稀土,2000,21(6):33-36. 被引量:19
4陈纪光,蔡志双.制取金属钕全流程工艺新技术[J].江西有色金属,1989,3(1):1-5. 被引量:2
5比.,伏德,贾天有.关于炉渣熔体密度的计算[J].科技译丛(重庆),1994(1):54-57. 被引量:6
6路贵民,张曰强.NdF_3-LiF-BaF_2系融盐电导率的测定研究[J].有色金属:冶炼部分,1992(1):31-34. 被引量:1
7刘奎仁,陈建设,魏绪钧.钕电解相关物质理论分解电压的计算[J].稀土,2001,22(2):30-33. 被引量:8
8饶勇,姜亚龙.大松装比氟化钕的研制[J].江西冶金,2001,21(1):24-26.
9尹祖平,琚建勇,刘云义.氟化氢气体法制备氟化钕热力学计算及实验[J].包钢科技,2010,36(1):32-35. 被引量:3
10郑鑫,朱卫花,彭光怀,梁金,张小联.NdF_3-LiF-Nd_2O_3体系熔盐电导率的研究[J].中国钨业,2013,28(1):30-33. 被引量:7
Basic Information:
DOI:
Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]
Citation Information:
The density of NdF 3 LiF melts was measured by Archimedes method in the present paper.The regression equation of the density dependence on the concentration of NdF 3 and temperature was gained by means of two factor quadratic regression orthogonal design.And the effects of the concentration of NdF 3 and temperature on the density of the melts were discussed.Moreover,the influences of the addition of Nd 2O 3 on the density were investigated.
quote
| GB/T 7714-2015 | [1] LIU Kui-ren, CHEN Jian-she, WEI Xu-jun, et al. Study on the Density of NdF_3-LiF-Nd_2O_3 System[J]. Rare Metals and Cemented Carbides, 2000(4): 7-10. |
| MLA | [1] LIU Kui-ren, et al., "Study on the Density of NdF_3-LiF-Nd_2O_3 System." Rare Metals and Cemented Carbides, no. 4, 2000, pp. 7-10. |
| APA | [1] LIU Kui-ren, CHEN Jian-she, WEI Xu-jun, ZHANG Zhi-hong, WANG Xiao-qing, XIE Li-ying, ZHENG Tian-cang, & KONG Xiang-min. (2000). Study on the Density of NdF_3-LiF-Nd_2O_3 System. Rare Metals and Cemented Carbides(4), 7-10. |
| IEEE | [1] LIU Kui-ren, CHEN Jian-she, WEI Xu-jun, ZHANG Zhi-hong, WANG Xiao-qing, XIE Li-ying, ZHENG Tian-cang, and KONG Xiang-min, "Study on the Density of NdF_3-LiF-Nd_2O_3 System," Rare Metals and Cemented Carbides, no. 4, pp. 7-10, 2000. keywords: {neodymium fluoride;neodymium oxide;melt;densityt} |