daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Bonding Phase of the Liquid phase Sintered Mo Based Alloy AITranslate

National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects of bonding phase composed of Ni and Cu on the properties of the liquid phase sintered Mo W Ni Cu alloy were studied. The results show that the sintering temperature decreases and the alloy grain is spheroidized and is refined with the increase of Ni and Cu or the ratio of Ni to Cu.Under the condition of a given ratio of Ni to Cu, the ultimate tensile strength of the alloy increases rapidly and then decreases slow with the increase of Ni and Cu. Under the condition of a given amount of Ni and Cu, the ultimate tensile strength changes with the increase in the ratio of Ni to Cu also so.When the ratio of Ni to Cu is 2.4, the amount of Ni and Cu is 6%wt, sintering temperature is above 1 380 ℃ , in the liquid phase sintered Mo based alloy there are few poles, the ultimate tensile strength can reach 1 100 MPa, the grain is cobble stone form.

KeyWords AITranslate

liquid phase sintering amount of Ni and Cu ratio of Ni to Cu bonding phase

1王伏生,梁容海,周载明,付忠.钨合金球制造工艺的研究[J].中南工业大学学报,1996,27(6):699-702. 被引量:7

2梁容海,汤金芝,刘红卫.高钨镦块材料的组织与性能[J].中国有色金属学报,1999,9(2):263-267. 被引量:2

3AmericanSocietyforMetals.Metalshandbook(8thEdition)[M].TheUnitedStatesofAmerica,1973,8:319.

4费多尔钦科NM.粉末冶金原理[M].北京:冶金工业出版社,1974.

5谢佑卿.金属固溶体及其组元的性质[J].中南矿冶学院学报,1993,24(3):332-341. 被引量:2

1何平,王志法,肖迎红.烧结温度对Mo-Cu-Ni合金性能的影响[J].中国钼业,2004,28(5):32-34. 被引量:4

1Guo, Shibo, Kang, Qiping, Cai, Chunbo, Qu, Xuanhui.Mechanical properties and expansion coefficient of Mo-Cu composites with different Ni contents[J].稀有金属:英文版,2012(4):368-371. 被引量:7

2夏扬,韩胜利,崔舜,宋月清,林晨光.高气密性Mo-Cu-Ni瓷封合金[J].真空电子技术,2006,19(4):36-39. 被引量:2

3郭世柏,康启平,蔡春波.活化元素Co对Mo-Cu合金组织和性能的影响[J].材料科学与工程学报,2011,29(1):86-89. 被引量:3

4陈宏斌,郭世柏,康启平,蔡春波.活化元素Fe对Mo-Cu合金组织和性能的影响[J].粉末冶金技术,2013,31(6):403-407. 被引量:2

1袁国洲.镍铜总量对液相烧结钼基合金性能的影响[J].粉末冶金材料科学与工程,1999,4(2):147-151.

2袁国洲.镍铜总量对液相烧结Mo-W-Ni-Cu合金性能的影响[J].稀有金属与硬质合金,1999(2):7-10. 被引量:5

3专利[J].粉末冶金技术,2001,19(2):118-119.

4黄金昌.钼基合金单晶体的加工工艺[J].稀有金属快报,1995(11):10-11.

5刘光俊.近几年来钨钼及其合金的进展[J].中国钨业,1990(10):21-25.

6李碧春.提高转炉废钢比的技术措施[J].重钢技术,1998,41(2):7-10.

7李惠萍.耐高温涂钨钼材[J].中国钼业,2004,28(6):9-9.

8张文钲,孙国英.钼化合物应用现状与发展[J].中国钼业,1990,0(2):1-12.

9王伏生,梁容海,金展鹏.W-Ni-Cu合金中粘结相对膨胀系数等性能的影响[J].粉末冶金材料科学与工程,1997,2(3):229-233. 被引量:3

10惠军,周世铎.工艺因素对W-Ni-Cu合金机械性能的影响[J].上海钢研,1993(3):36-39.

Basic Information:

DOI:

Chinese Library Classification Number:TF125.241[冶金工程—粉末冶金];TF124.54[冶金工程—粉末冶金]

Citation Information:

The effects of bonding phase composed of Ni and Cu on the properties of the liquid phase sintered Mo W Ni Cu alloy were studied. The results show that the sintering temperature decreases and the alloy grain is spheroidized and is refined with the increase of Ni and Cu or the ratio of Ni to Cu.Under the condition of a given ratio of Ni to Cu, the ultimate tensile strength of the alloy increases rapidly and then decreases slow with the increase of Ni and Cu. Under the condition of a given amount of Ni and Cu, the ultimate tensile strength changes with the increase in the ratio of Ni to Cu also so.When the ratio of Ni to Cu is 2.4, the amount of Ni and Cu is 6%wt, sintering temperature is above 1 380 ℃ , in the liquid phase sintered Mo based alloy there are few poles, the ultimate tensile strength can reach 1 100 MPa, the grain is cobble stone form.

quote

GB/T 7714-2015 [1] YUAN Guo-zhou, ZHANG Zhao-sen, LIU Hua-yi, et al. Study on Bonding Phase of the Liquid phase Sintered Mo Based Alloy[J]. Rare Metals and Cemented Carbides, 2000(4): 11-15.
MLA [1] YUAN Guo-zhou, et al., "Study on Bonding Phase of the Liquid phase Sintered Mo Based Alloy." Rare Metals and Cemented Carbides, no. 4, 2000, pp. 11-15.
APA [1] YUAN Guo-zhou, ZHANG Zhao-sen, LIU Hua-yi, & LIU Bin. (2000). Study on Bonding Phase of the Liquid phase Sintered Mo Based Alloy. Rare Metals and Cemented Carbides(4), 11-15.
IEEE [1] YUAN Guo-zhou, ZHANG Zhao-sen, LIU Hua-yi, and LIU Bin, "Study on Bonding Phase of the Liquid phase Sintered Mo Based Alloy," Rare Metals and Cemented Carbides, no. 4, pp. 11-15, 2000. keywords: {liquid phase sintering;amount of Ni and Cu;ratio of Ni to Cu;bonding phase}