Recovery of Molybdenum from Copper and Molybdenum Middlings by High-pressure Oxygen Digestion-extraction AITranslate
Abstract AITranslate
Recovery of molybdenum from copper and molybdenum middlings has been studied.The main steps are as follows:NaOH hi-pressure oxygen digestion to enable Mo to enter the solution in the form of sodium molybdate with Cu remaining in the residues,which can be used as raw matcrial for Cu recovery.Mo is recovered by extraction from Mo-containrng solution.It is shown that,under given conditions,the recovery of molybdenum and copper is 95.6% and 99% respectively.
KeyWords AITranslate
1雷贵春.铜钼分离新技术及其在德兴铜矿应用的展望[J].江西有色金属,1999,13(3):23-26. 被引量:4
2马保平.金堆城钼业公司选矿技术进展与创新[J].中国钼业,1997,21(2):59-61. 被引量:5
1徐徽,皮关华,陈白珍,石西昌,李俊丽.用溶剂萃取法从碱浸液中回收钼的研究[J].湖南师范大学自然科学学报,2007,30(1):43-46. 被引量:9
2王燕.高铜非标钼精矿处理研究进展[J].中国钼业,2008,32(2):25-27. 被引量:7
3公彦兵,沈裕军,丁喻,周新东.辉钼矿湿法冶金研究进展[J].矿冶工程,2009,29(1):78-81. 被引量:16
4宋成盈,宋会娟,王建设,赵建宏,王留成.氧气氧化法分解辉钼矿[J].金属矿山,2009(3):69-70. 被引量:5
5康绍辉,孟晋,王洪明,王平,杨剑飞.钼矿物湿法处理技术研究进展[J].湿法冶金,2012,31(6):333-337. 被引量:2
6谢铿,王海北,张邦胜.低品位钼矿及钼二次资源加压浸出工艺的研究进展[J].稀有金属与硬质合金,2014,42(3):23-27. 被引量:3
7牟文宁,张鸿彪,苏志强,宋佩.低品位钼矿钠化焙烧-水浸过程钼的转化研究[J].稀有金属,2015,39(9):854-860. 被引量:5
8杨艳.萃取法回收二硫化钼废水中的钼[J].安徽化工,2017,43(3):46-49. 被引量:1
9刘锦锐.钼酸铵生产工艺流程综述[J].云南冶金,2018,47(4):48-57. 被引量:4
10刘锦锐,任倩,刘红召.NaOH溶液体系浸出工业氧化钼试验研究[J].矿产保护与利用,2018,38(4):54-58. 被引量:1
1何树荣.工业氧化钼实用生产技术及进展[J].材料开发与应用,2013,28(1):96-101. 被引量:5
2都基峻,田刚,张凡.钼冶炼工艺的循环经济探讨[J].环境工程,2011,29(S1):381-384. 被引量:3
3李志松,李群松,舒均杰.树脂吸附法从含钼废水中回收制备三氧化钼[J].精细化工中间体,2009,39(2):60-62. 被引量:3
4吴贤,李来平,张新,张文钲.用矿浆电解法分解辉钼矿试验研究[J].现代矿业,2009(10):61-64. 被引量:1
5张文朴.加强钼资源综合利用与再生研发 促进我国生态钼业建设[J].中国钼业,2010,34(2):13-18. 被引量:3
6魏德洲,高淑玲,刘文刚,卢涛,张瑞洋,马崇振.2009年中国选矿年评[J].金属矿山,2010(9):1-12.
7都基峻,田刚,曾萍,刘宇,石应杰,张凡.富氧加压反应器焙烧辉钼矿过程研究[J].环境工程技术学报,2011,1(2):151-156.
8沈裕军,杨文魁,公彦兵,丁喻.碱性加压浸出三次氨浸渣中钼的实验研究[J].矿冶工程,2011,31(4):73-76. 被引量:5
9杨文魁,沈裕军,丁喻.镍钼矿湿法冶金研究现状[J].中国钼业,2011,35(5):11-14. 被引量:6
10张亨.钼酸铵的生产研究综述[J].杭州化工,2012,42(2):11-15. 被引量:3
1徐毅.硫化锌精矿中镓锗在高压氧浸中的浸出行为研究[J].湖南工业大学学报,2011,25(4):1-4. 被引量:8
2宋兴诚,沐彩兰,皇甫智伟.低锡高铅粗合金电解试验研究[J].中国有色冶金,1998,31(9):23-29.
3陈礼运,宋平,高晓宝.高品位原生钼矿的综合利用[J].中国钼业,2003,27(3):17-18. 被引量:21
4张荣良,谢永金.湿法处理氧化浸出洗净残渣试验研究[J].铜业工程,1995,0(2):37-40. 被引量:2
5顾珩,李洪桂,刘茂盛.辉钼矿湿法浸出新工艺研究[J].中国钼业,1997,21(5):29-32. 被引量:13
6宋兴诚,沐彩兰.低锡高铅粗合金电解试验研究[J].云锡科技,1997,24(3):18-31.
7彭造伟.氧压浸出物料粒度对工艺影响[J].世界有色金属,2016,0(8):167-167. 被引量:2
8张建新.电炉生产60Si2Mn钢过程吸氮分析及控制[J].新疆钢铁,2009(1):29-31.
9王崇琳.粉末材料在高压氧、氮气体中的结构及性能[J].粉末冶金技术,1996,14(4):297-304.
10林庆权.我国锡冶金标准样品的研制与发展[J].云南冶金,2002,31(3):158-164. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]
Citation Information:
Recovery of molybdenum from copper and molybdenum middlings has been studied.The main steps are as follows:NaOH hi-pressure oxygen digestion to enable Mo to enter the solution in the form of sodium molybdate with Cu remaining in the residues,which can be used as raw matcrial for Cu recovery.Mo is recovered by extraction from Mo-containrng solution.It is shown that,under given conditions,the recovery of molybdenum and copper is 95.6% and 99% respectively.
quote
| GB/T 7714-2015 | [1] TANG Zhong-yang, LI Hong-gui, HUO Guang-sheng. Recovery of Molybdenum from Copper and Molybdenum Middlings by High-pressure Oxygen Digestion-extraction[J]. Rare Metals and Cemented Carbides, 2003(1): 1-3. |
| MLA | [1] TANG Zhong-yang, et al., "Recovery of Molybdenum from Copper and Molybdenum Middlings by High-pressure Oxygen Digestion-extraction." Rare Metals and Cemented Carbides, no. 1, 2003, pp. 1-3. |
| APA | [1] TANG Zhong-yang, LI Hong-gui, & HUO Guang-sheng. (2003). Recovery of Molybdenum from Copper and Molybdenum Middlings by High-pressure Oxygen Digestion-extraction. Rare Metals and Cemented Carbides(1), 1-3. |
| IEEE | [1] TANG Zhong-yang, LI Hong-gui, and HUO Guang-sheng, "Recovery of Molybdenum from Copper and Molybdenum Middlings by High-pressure Oxygen Digestion-extraction," Rare Metals and Cemented Carbides, no. 1, pp. 1-3, 2003. keywords: {Cu middlings;molybdenum;NaOH digestion;extraction} |