daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Recovery of Sulfuric Acid from TiO_2 Hydrolysis Waste Acid by Solvent Extraction AITranslate

Department of Environmental Engineering, College of Biological and Environmental Engineering, Jiangsu University;School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of the process extraction of sulfuric acid from TiO2 hydrolysis waste acid with tri-isoctylamine as extractant and H2O as stripping reagent.Investgation is made on the impaction of extractant concentration,phase modifier concentration,phase ratio and temperature on the extraction and stripping.Simulation test is made.The results showed that under given condition,the H2SO4 recovery can reach 91.8% and acid concentration in the product is 119.73 g/L.

KeyWords AITranslate

extraction recovery titanium dioxide wase acid sulfuric acid

1徐铜文,杨伟华,刘兆明,李善清,李旭娣,何炳林.膜法回收钛白废液中硫酸的实验研究[J].水处理技术,1999,25(4):204-208. 被引量:17

2葛龙桂.静态浓差渗析法回收钛白废酸中的硫酸.化工环保,1988,7(6):350-350.

3于淑秋 等.萃取除铁在湿法冶金中的应用--(Ⅰ)胺类及中性萃取剂.化工冶金,1988,9(3):66-66.

1唐建军,张伟,周康根,张启修.膜法回收稀土冶金过程中废酸的可行性研究[J].矿冶工程,2007,27(6):54-57. 被引量:3

2许惠,傅敏.钛白废液的治理与综合利用研究进展[J].矿产综合利用,2006(4):34-37. 被引量:16

3唐建军,周康根,张启修.Sulfuric acid recovery from rare earth sulphate solutions by diffusion dialysis[J].中国有色金属学会会刊:英文版,2006,16(4):951-955. 被引量:3

4张永刚,赵西往,靳晓霞.钢铁酸洗废液资源化的膜处理技术[J].工业水处理,2006,26(12):18-20. 被引量:18

5王建伟,任秀莲,魏琦峰,杨东,吴成龙.钛白废酸的综合利用研究现状及展望[J].无机盐工业,2009,41(9):4-7. 被引量:26

6宋宇,李婷,邓燕,邱佳.硫酸法钛白浓废酸的综合治理[J].大众科技,2011,13(9):100-102. 被引量:10

7杨海琼,董海刚,赵家春,李博捷,范兴祥,吴跃东,吴晓峰,童伟锋.钪的回收技术研究进展[J].有色金属:冶炼部分,2014(3):29-33. 被引量:13

8王文宝,龚圣,谭惠忠,秦力,欧永聪,周新华.电极箔化成磷酸处理液的循环利用研究[J].广东化工,2016,43(6):42-44. 被引量:3

9李望,赵恒,朱晓波.钛白废液制备黄钾铁矾的实验研究[J].稀有金属与硬质合金,2018,46(3):35-37. 被引量:1

10陶荣荣,牛泽鹏,朱晓波,李望,张治国.利用钛白废液制备草酸亚铁实验研究[J].稀有金属与硬质合金,2022,50(1):6-9.

1朱晓波,牛泽鹏,李望,白云涛,王涛,任博.溶剂萃取法回收钛白废液中钒的实验研究[J].稀有金属与硬质合金,2020(1):9-12. 被引量:4

2宗园,王洁,孙石,王恒颖,杨常亮,邓辅唐.含金属离子硫酸液的膜分离技术及其应用[J].云南大学学报:自然科学版,2008,30(S2):370-376. 被引量:1

3范兵,李志广,李昭,刘士琪,任保增.硫酸法钛白废酸的处理[J].河南化工,2013,30(6):12-15. 被引量:16

4王会.不锈钢管制造业废水处理的工程实践[J].环境保护科学,2008,34(2):48-49. 被引量:1

5钱强.含钒转炉渣中和钛白废酸的试验研究[J].钢铁,2009,44(2):80-82. 被引量:2

6钱强.废弃钢渣资源新型利用研究进展[J].中国资源综合利用,2009,27(4):22-23. 被引量:3

7李俊峰.硫酸法钛白粉生产废酸液的综合利用[J].广州化工,2010,38(2):185-186. 被引量:4

8王昌松,钱红亮,姚文俊,吉远辉,陆小华.钛白工业节能减排研究进展及新思路探讨[J].无机盐工业,2010,42(4):8-10. 被引量:3

9李亮.钛白废酸喷雾浓缩装置的研发[J].湿法冶金,2010,29(2):130-133. 被引量:4

10王洁,孙癿石,方富林,毕晓伊,杨常亮,邓辅唐,乔莉.纳滤膜处理含金属离子酸性废液[J].膜科学与技术,2010,30(3):35-38. 被引量:11

1张贵清,张启修,周康根.N1923萃取回收钛白水解废酸中的钛——反萃取参数的研究[J].矿冶工程,2003,23(2):66-68. 被引量:7

2李春,李自强,刘小平,王丽雄.溶剂萃取法从锌电积废液中分离钙镁的研究[J].有色金属:冶炼部分,2000(6):20-22. 被引量:17

3靖雪晶,李木杰.钢包渣还原处理[J].冶金丛刊,1998(4):37-39. 被引量:2

4Logest,M,陈壮志.用三异辛胺作萃取脐从钴液中萃取分离铜[J].重冶科技,1990(12):24-31.

5何学斌,王建芳,杨和平.从高氟氯布袋尘中回收铟的工艺技术[J].商洛学院学报,2012,26(6):44-46.

6李宇亮,彭悦欣,徐永胜.萃取-反萃取以提取酸溶液中的镓[J].科学技术与工程,2014,22(27):173-176. 被引量:8

7杨晓,张一敏.从石煤提钒酸浸液中萃取分离硫酸[J].有色金属:冶炼部分,2016(11):28-31. 被引量:3

8陈朝梅,李军旗,金会心,龙琼.织金磷矿酸浸液萃取分离稀土试验研究[J].湿法冶金,2015,34(1):39-42. 被引量:3

9G.A.Meszaros,项锦云.美国钢公司蒙·瓦利厂利用渣处理提高炼钢产量[J].武钢技术,1997,35(10):21-25.

10贾云芝.酸浸-萃取-电积法从氧化铜矿中提取铜的研究[J].云南冶金,1997,26(6):35-41.

Basic Information:

DOI:

Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]

Citation Information:

Study is made of the process extraction of sulfuric acid from TiO2 hydrolysis waste acid with tri-isoctylamine as extractant and H2O as stripping reagent.Investgation is made on the impaction of extractant concentration,phase modifier concentration,phase ratio and temperature on the extraction and stripping.Simulation test is made.The results showed that under given condition,the H2SO4 recovery can reach 91.8% and acid concentration in the product is 119.73 g/L.

quote

GB/T 7714-2015 [1] LI Qian, ZHANG Qi-xiu. Study on Recovery of Sulfuric Acid from TiO_2 Hydrolysis Waste Acid by Solvent Extraction[J]. Rare Metals and Cemented Carbides, 2003(1): 4-7.
MLA [1] LI Qian, and ZHANG Qi-xiu. "Study on Recovery of Sulfuric Acid from TiO_2 Hydrolysis Waste Acid by Solvent Extraction." Rare Metals and Cemented Carbides, no. 1, 2003, pp. 4-7.
APA [1] LI Qian, & ZHANG Qi-xiu. (2003). Study on Recovery of Sulfuric Acid from TiO_2 Hydrolysis Waste Acid by Solvent Extraction. Rare Metals and Cemented Carbides(1), 4-7.
IEEE [1] LI Qian and ZHANG Qi-xiu, "Study on Recovery of Sulfuric Acid from TiO_2 Hydrolysis Waste Acid by Solvent Extraction," Rare Metals and Cemented Carbides, no. 1, pp. 4-7, 2003. keywords: {extraction;recovery;titanium dioxide;wase acid;sulfuric acid}