daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Comparative Study on Properties of LaCoO_3 Powders Prepared by Ammonium Carbonate Precipitation and Citric Acid Complexation AITranslate

Key Laboratory of green extraction and efficient utilization of light rare earth resources of Ministry of education,Inner Mongolia University of Science and Technology;Key Laboratory of green extraction and efficient utilization of light rare earth resources of Ministry of education,Inner Mongolia University of Science and Technology;Key Laboratory of green extraction and efficient utilization of light rare earth resources of Ministry of education,Inner Mongolia University of Science and Technology;Key Laboratory of green extraction and efficient utilization of light rare earth resources of Ministry of education,Inner Mongolia University of Science and Technology;Key Laboratory of green extraction and efficient utilization of light rare earth resources of Ministry of education,Inner Mongolia University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using La(NO3)3 and Co(NO3)2 as raw materials,rare earth perovskite LaCoO3 powder was prepared by citric acid complexation and ammonium carbonate precipitation,respectively.Products were characterized by SEM,XRD,specific surface area analyzer and laser particle size analyzer.The results show that the rare earth perovskite LaCoO3 powder can be prepared by calcination above 600℃,and the surface structure is the flocculent structure of honeycomb foam.With the increase of calcination temperature,the surface will be sintered at different degrees.The sample prepared by citric acid complexation has high purity,stronger sintering resistance and smaller particle size,the efficiency of catalytic denitrification is over 90%.

KeyWords AITranslate

rare earth perovskite LaCoO3 citric acid complexation method ammonium carbonate precipitation method

1王广建,秦永宁,马智,王永成.钙钛矿型复合氧化物材料[J].化学通报,2005,68(2):117-122. 被引量:24

2于洁,王华,马文会.复合掺杂钙钛矿氧化物催化剂的研究进展[J].昆明理工大学学报:理工版,2003,28(1):19-22. 被引量:3

3冉锐,吴晓东,翁端.稀土钙钛矿催化剂制备方法的研究进展[J].稀土,2004,25(5):46-50. 被引量:26

4李莹莹.钙钛矿型复合氧化物研究进展[J].广州化工,2012,40(24):1-3. 被引量:3

5郝斌,杨铁皂,吕刚,宋崇林,宾峰.LaCoO_3钙钛矿型催化剂对柴油机NO_x净化性能研究[J].小型内燃机与摩托车,2012,41(2):62-65. 被引量:1

6王虹,赵震,徐春明,段爱军,刘坚,迟姚玲.LaBO_3钙钛矿型复合氧化物同时消除柴油机尾气炭颗粒和NO[J].催化学报(英文),2008,29(7):649-654. 被引量:37

7路良泽,代方方,孟明.负载钙钛矿型催化剂的制备、结构及其对碳烟的催化燃烧性能[J].科学通报,2014,59(26):2609-2614. 被引量:5

8明彩兵,叶代启,易慧,付名利.由贵金属取代的钙钛矿催化剂对碳烟的催化性能[J].中国环境科学,2009,29(9):924-928. 被引量:5

9毕军,吴艳波,魏斌斌,宋铁犇,韩笑梅.钙钛矿型LaCoO_3的制备及其光催化性能[J].大连交通大学学报,2014,35(4):78-81. 被引量:5

10郑兴芳.水热法制备纳米氧化物的研究进展[J].无机盐工业,2009,41(8):9-11. 被引量:22

1曹霞,鲁登云,朱彦华,贺梦冬.La_(2)O_(3)∶Eu^(3+)纳米棒的水热合成以及光学性质研究[J].湖南师范大学自然科学学报,2021,44(4):126-130.

1张传驹,李明航,谈冠希,苗杰,靳广洲.热解条件对CuCe-O/γ-Al2O3催化性能的影响[J].石油化工,2018,47(10):52-58.

2唐超兰,张伟祥,陈志茹,周德敬,李龙,楚瑞坤.3D打印用钛合金粉末制备技术分析[J].广东工业大学学报,2019,36(3):91-98. 被引量:14

3张新涛,张科翠,张娟,赵健,张东.注射成形用的金属粉末制备技术及性能研究[J].金川科技,2019,0(1):25-28.

4张新涛,张科翠,张东,赵健,樊昱,张娟.注射成形用金属粉末的制备技术及性能研究进展[J].粉末冶金工业,2019,29(2):55-59. 被引量:4

5吴梦,张大超,徐师,陈敏,王春英.废水除磷工艺技术研究进展[J].有色金属科学与工程,2019,10(2):97-103. 被引量:22

6苟晓琴,韩海生,孙伟,刘润清,亢建华.氟离子在脱硫石膏表面的吸附转化行为及高浓度含氟废水净化技术[J].矿冶工程,2019,39(2):97-101. 被引量:7

7张杰,付凤艳,王超.DPVA/Ag_3PO_4纳米复合材料的制备与表征研究[J].人工晶体学报,2019,48(4):752-756. 被引量:2

8方秀秀,廖文敏,宋建东,汪云,罗孟飞.气相催化1,1,1,3,3-五氟丙烷脱HF合成1,3,3,3-四氟丙烯研究进展[J].化工生产与技术,2019,25(1):15-17.

9徐志勇,赵文波,柴牧原,陈玲,李艳红,赵榆林.微/纳米过渡金属氧化物的液相合成及其应用[J].化工新型材料,2019,47(4):38-42. 被引量:1

10王璐璐,冯璇,沈来宏.高硫石油焦化学链燃烧特性及硫的转化[J].东南大学学报:自然科学版,2019,49(2):288-295. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TQ426[化学工程]

Citation Information:

Using La(NO3)3 and Co(NO3)2 as raw materials,rare earth perovskite LaCoO3 powder was prepared by citric acid complexation and ammonium carbonate precipitation,respectively.Products were characterized by SEM,XRD,specific surface area analyzer and laser particle size analyzer.The results show that the rare earth perovskite LaCoO3 powder can be prepared by calcination above 600℃,and the surface structure is the flocculent structure of honeycomb foam.With the increase of calcination temperature,the surface will be sintered at different degrees.The sample prepared by citric acid complexation has high purity,stronger sintering resistance and smaller particle size,the efficiency of catalytic denitrification is over 90%.

quote

GB/T 7714-2015 [1] DU Hong-wei, BAI Zhi-peng, SUN Ting, et al. Comparative Study on Properties of LaCoO_3 Powders Prepared by Ammonium Carbonate Precipitation and Citric Acid Complexation[J]. Rare Metals and Cemented Carbides, 2019(2): 1-5.
MLA [1] DU Hong-wei, et al., "Comparative Study on Properties of LaCoO_3 Powders Prepared by Ammonium Carbonate Precipitation and Citric Acid Complexation." Rare Metals and Cemented Carbides, no. 2, 2019, pp. 1-5.
APA [1] DU Hong-wei, BAI Zhi-peng, SUN Ting, XIAO Zhuo-nan, & LI Ke. (2019). Comparative Study on Properties of LaCoO_3 Powders Prepared by Ammonium Carbonate Precipitation and Citric Acid Complexation. Rare Metals and Cemented Carbides(2), 1-5.
IEEE [1] DU Hong-wei, BAI Zhi-peng, SUN Ting, XIAO Zhuo-nan, and LI Ke, "Comparative Study on Properties of LaCoO_3 Powders Prepared by Ammonium Carbonate Precipitation and Citric Acid Complexation," Rare Metals and Cemented Carbides, no. 2, pp. 1-5, 2019. keywords: {rare earth perovskite;LaCoO3;citric acid complexation method;ammonium carbonate precipitation method}