The Synthesis of Crystalline Rare Earth (La、Ce、Pr、Nd) Carbonates AITranslate
Abstract AITranslate
The crystalline rare earth (La、Ce、Pr、Nd) carbonates were precipitated using ammonium bicarbonate as precipitant. Chemical analysis of the composition of these compounds has been carried out. X-ray powder diffractomtry, IR spectrum and TGA、DTA of these compounds have been studied. The compositions of the rare earth carbonates have been determined to be RE2(CO3)3 ·xH2O(RE=La2、Ce、Pr、Nd, x=2、3 、4 ).
KeyWords AITranslate
1喻庆华,李先柏.晶型碳酸稀土与稀土配分[J].稀有金属与硬质合金,1997,25(3):8-12. 被引量:5
2刘翠翠,李梅,胡艳宏,柳召刚.聚苯乙烯磺酸钠调控制备球状碳酸铈颗粒研究[J].无机盐工业,2012,44(8):13-15.
3贺伦燕,李南萍.用碳酸氢铵沉淀制备晶状碳酸钇的机理研究[J].稀有金属与硬质合金,2002,30(1):1-5. 被引量:8
4周晓宏.中重稀土碳酸钆晶型沉淀工艺研究[J].福建冶金,2022,51(1):22-25. 被引量:1
1闫勇,朱伟长,李辉生.氧化钇纳米粉体材料的制备[J].化工新型材料,2004,32(7):11-12. 被引量:5
2闻雷,其鲁,孙旭东,徐国祥.碳酸盐沉淀法制备Y_2O_3纳米粉及透明陶瓷[J].中国有色金属学报,2006,16(2):235-240. 被引量:10
3潘艳,李玮楠,陆敏.稀土掺杂的纳米晶材料化学制备方法的研究[J].武汉理工大学学报,2007,29(E01):150-153.
4霍地,孙旭东,修稚萌,李晓东.制备工艺对超细氧化钇粉体形态与烧结性的影响[J].中国稀土学报,2007,25(5):566-572. 被引量:12
5陈少静,辛庆辉,王宝利,沙镇虎,孙绍波,曹大力.混合碳酸稀土对泡沫陶瓷过滤器性能的影响[J].沈阳化工学院学报,2008,22(2):149-152.
6郭易芬,马伟民,闻雷,沈世妃,王华栋,尹凯.碳酸氢铵共沉淀法制备(Y,Gd)2O3:Eu^3+纳米材料及光谱特性[J].人工晶体学报,2009,38(3):746-750. 被引量:5
7岑治,夏长林,姬志强,许朝辉,杨海涛,郭英.高浓度溶液共沉技术制备晶型碳酸镨钕工业化生产试验研究[J].稀土,2010,31(4):92-95. 被引量:5
8李永超,谭亚军.纳米YAG粉体的制备与表征[J].贵州大学学报:自然科学版,2011,28(5):45-48. 被引量:1
9刘宇晖,余荣旻,欧阳宇平,苏正夫,邵春欣,王志坚,刘吉波.粒度可控氧化钇粉体的制备[J].有色金属科学与工程,2015,6(3):22-25.
10尹少华,林国,彭金辉,谢峰,李世伟,张利波.响应曲面法优化微波干燥碳酸稀土的实验研究[J].稀有金属,2016,40(4):350-355. 被引量:6
1冯天泽.稀土碳酸盐的制法、性质和组成[J].稀土,1989(3):45-49. 被引量:18
2一种处理含铝稀土料液的碳酸稀土结晶沉淀方法[J].无机盐工业,2014,46(9):61-61.
3李先柏,喻庆华.晶态镝、钬、铒、钇碳酸盐的制备[J].稀有金属,1994,18(5):360-364. 被引量:1
4柳松,马荣骏.RE^(3+)-NH_4^+-CO_3^(2-)体系的研究[J].矿冶工程,1997,17(1):59-61.
5一种低氯根稀土碳酸盐加工方法[J].无机盐工业,2013,45(10):38-38.
6林静,孙利清.碳酸稀土及工业生产[J].纯碱工业,2001(1):44-45.
7秦玉楠.稀土精细无机盐产品的开发及应用[J].精细与专用化学品,1996,0(8):7-10.
8一种处理含铝稀土料液的碳酸稀土结晶沉淀方法[J].有色冶金节能,2015,31(2):62-62.
9秦玉楠.稀土无机盐的开发及应用[J].无机盐工业,1995,9(4):20-21.
10毕祥.不锈钢黑磷化后石墨烯封闭工艺及性能研究[J].石油化工腐蚀与防护,2017,34(1):23-25.
Basic Information:
DOI:
Chinese Library Classification Number:TQ133.3[化学工程—无机化工]
Citation Information:
The crystalline rare earth (La、Ce、Pr、Nd) carbonates were precipitated using ammonium bicarbonate as precipitant. Chemical analysis of the composition of these compounds has been carried out. X-ray powder diffractomtry, IR spectrum and TGA、DTA of these compounds have been studied. The compositions of the rare earth carbonates have been determined to be RE2(CO3)3 ·xH2O(RE=La2、Ce、Pr、Nd, x=2、3 、4 ).
quote
| GB/T 7714-2015 | [1] LI Xian-bai, YU Qing-hua. The Synthesis of Crystalline Rare Earth (La、Ce、Pr、Nd) Carbonates[J]. Rare Metals and Cemented Carbides, 1994(3): 1-6. |
| MLA | [1] LI Xian-bai, and YU Qing-hua. "The Synthesis of Crystalline Rare Earth (La、Ce、Pr、Nd) Carbonates." Rare Metals and Cemented Carbides, no. 3, 1994, pp. 1-6. |
| APA | [1] LI Xian-bai, & YU Qing-hua. (1994). The Synthesis of Crystalline Rare Earth (La、Ce、Pr、Nd) Carbonates. Rare Metals and Cemented Carbides(3), 1-6. |
| IEEE | [1] LI Xian-bai and YU Qing-hua, "The Synthesis of Crystalline Rare Earth (La、Ce、Pr、Nd) Carbonates," Rare Metals and Cemented Carbides, no. 3, pp. 1-6, 1994. keywords: {rare earth, rare earth(La、Ce、Pr、Nd) carbonates, crystalline precipitation} |