Effect Comparison of Joining Way between Tungsten Alloy Anvil and Base Seat AITranslate

National Key Laboratory of Powder Metallurgy of Central South China University of Technology;National Key Laboratory of Powder Metallurgy of Central South China University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The working characteristics of tungsten alloy hammaring block are introduced. The Jinning ways between tungsten alloy anvil and base seat are analysed. Among them the 'V' type joining can get the contact close-connected with auto-lock effect, which results in good conductibility and heat radiation of anvil, greatly improving the life of utensil system.

KeyWords AITranslate

tungsten alloy anvil seat joining way hot upset

1王伏生,赵慕岳.高密度钨合金及其在军事工业中的应用[J].粉末冶金材料科学与工程,1997,2(2):114-120. 被引量:19

2成都科学技术大学,彭少方.钨冶金学[M]冶金工业出版社,1981.

1梁容海,汤金芝,刘红卫.高钨镦块材料的组织与性能[J].中国有色金属学报,1999,9(2):263-267. 被引量:2

1龚伟平,陈腾飞,龚育平.钼合金耐火材料液相烧结性能热力学研究[J].矿冶工程,2006,26(3):65-67. 被引量:3

2袁国洲,张兆森,刘华佾,刘槟.液相烧结钼基合金粘结相的研究[J].稀有金属与硬质合金,2000,28(4):11-15. 被引量:1

1丁宝利,韩至成,王善道,卢国华,陈亚爱.双锭电磁铸造实验研究[J].铸造技术,1995,20(6):11-13. 被引量:4

2王伏生,梁容海,刘栓柱.砧块与基座新型联结方式探讨[J].内燃机配件,1995(4):27-29.

3胡亚民,郑恒杰.国内外电热镦粗工艺的发展[J].模具技术,1989(3):72-80. 被引量:9

4胡斌.RT17辊道改造与实践[J].浙江冶金,2010(4):40-42.

5梁容海,汤金芝,刘红卫.高钨镦块材料的组织与性能[J].中国有色金属学报,1999,9(2):263-267. 被引量:2

6梁容海,钟国明.高钨合金砧模材料的研究[J].稀有金属与硬质合金,1998,26(2):31-34.

7李大海.自锁式试压盖的设计及应用[J].一重技术,2008(4):67-68.

8吕长山,邵友竹.气动自锁式三爪卡盘的研制[J].钻镗床,1994(2):6-7.

9颜月娥,黄振德,梁容海,周载明.钨合金砧块与基座联结性能的改善[J].粉末冶金材料科学与工程,1996,1(1):82-84. 被引量:1

10王伏生,陈乾坤.电镦砧块与基座联结方式探讨[J].内燃机配件,1993(2):24-28. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TG315.12[金属学及工艺—金属压力加工]

Citation Information:

The working characteristics of tungsten alloy hammaring block are introduced. The Jinning ways between tungsten alloy anvil and base seat are analysed. Among them the 'V' type joining can get the contact close-connected with auto-lock effect, which results in good conductibility and heat radiation of anvil, greatly improving the life of utensil system.

quote

GB/T 7714-2015 [1] LIANG Rong-hai, XIONG Xiang-jun. Effect Comparison of Joining Way between Tungsten Alloy Anvil and Base Seat[J]. Rare Metals and Cemented Carbides, 1998(3): 4-7.
MLA [1] LIANG Rong-hai, and XIONG Xiang-jun. "Effect Comparison of Joining Way between Tungsten Alloy Anvil and Base Seat." Rare Metals and Cemented Carbides, no. 3, 1998, pp. 4-7.
APA [1] LIANG Rong-hai, & XIONG Xiang-jun. (1998). Effect Comparison of Joining Way between Tungsten Alloy Anvil and Base Seat. Rare Metals and Cemented Carbides(3), 4-7.
IEEE [1] LIANG Rong-hai and XIONG Xiang-jun, "Effect Comparison of Joining Way between Tungsten Alloy Anvil and Base Seat," Rare Metals and Cemented Carbides, no. 3, pp. 4-7, 1998. keywords: {tungsten alloy anvil;seat;joining way;hot upset}