Using optical microscope and JCXA-733 type electron probe microanalyse. by means of images of SEI, BEI and CXSI, the fracture behaviour of the industrial specimen Of WC-Co-Ni cemented carbide is observed and analysed, with discussion of alloy strength factors.

KeyWords AITranslate

WC-Co-Ni cemented carbide fracture behaviour fracture morphology pore impurity

1杨汉民,周建,胡中彪,余立新,张烈华.亚微细硬质合金三牙轮钻齿的使用与失效分析[J].武汉理工大学学报,2004,26(12):16-19.

2饶承毅,龙坚战,袁红梅.Ni含量对粗晶WC-Co-Ni硬质合金组织和性能的影响[J].硬质合金,2012,29(1):11-14. 被引量:9

3王娟梅,仝晓楠,高源.高性能煤化工浆料输出用硬质合金喷嘴的制备试验[J].机械研究与应用,2020,33(2):138-139.

4汪中玮,刘海军.碳含量和球磨时间对Fe-Co-Ni粘结相硬质合金性能的影响[J].硬质合金,2021,38(5):332-337.

1张忠健,龙坚战.碳化钨/金属间化合物硬质合金的研究进展[J].硬质合金,2012,29(6):378-386. 被引量:15

2龙坚战,张忠健,彭文,陆必志,周华堂,罗海辉,董亮.Ni_3Al添加量对WC-Co硬质合金中WC晶粒形状的影响[J].硬质合金,2013,30(6):308-315. 被引量:7

3龙坚战,陆必志,易茂中,陈飞.新型粘结相硬质合金的研究进展[J].硬质合金,2015,32(3):204-212. 被引量:26

4汪巍,伍文辉,方晴.AlN添加对原WC-Ni-Co-Cr合金性能和组织结构的影响[J].硬质合金,2015,32(4):242-246. 被引量:3

5马向东,刘东方,黄亮亮.烧结碳化钨增强激光熔敷涂层耐磨性研究[J].润滑与密封,2016,41(6):1-3. 被引量:2

6尚峰,付杰,乔斌,李化强,曹振伟,孙伟.WC-10Co超细晶硬质合金的注射成形工艺研究[J].稀有金属与硬质合金,2017,45(5):63-68. 被引量:5

7罗学全,于涛,温光华,朱光柱.球磨时间对WC-7%Co-3%Ni硬质合金组织和性能的影响[J].硬质合金,2020,37(3):240-247. 被引量:2

8赵玉玲,张颢,邹德良,魏修宇,金鹏,崔焱茗.钴镍比对WC-14%(Co,Ni)硬质合金力学性能和在中性NaCl溶液中耐腐蚀性能的影响[J].硬质合金,2021,38(4):236-243. 被引量:2

9孙化鑫,徐淑波,李辉,郑君姿,卢庆亮.Ni含量对WC-Co-Ni硬质合金的力学性能和耐腐蚀性能的影响[J].稀有金属与硬质合金,2022,50(6):77-82.

1何平,苏丽君.WC-Co-Ni硬质合金断裂行为的观察与分析[J].粉末冶金材料科学与工程,1996,1(2):51-54. 被引量:2

2何平.WC-Co-Ni硬质合金的微观组织和断裂强度[J].粉末冶金技术,1996,14(4):287-290. 被引量:2

3何平.WC-Co-Ni硬质合金微观组织与抗弯强度[J].硬质合金,1996,13(2):78-81.

4Laoui.,T,唐丹.添加TiC对Ti(CN)—WC—Co—Ni金属陶瓷显微结构和性能的影响[J].国外难熔金属与硬质材料,1996,12(2):63-64.

5李晋尧,何平.WC-Co硬质合金的微观组织结构与性能的研究[J].稀有金属材料与工程,1995,24(3):53-58. 被引量:13

6饶承毅,龙坚战,袁红梅.Ni含量对粗晶WC-Co-Ni硬质合金组织和性能的影响[J].硬质合金,2012,29(1):11-14. 被引量:9

7朱峰,伍超群,刘英坤.电子探针在6063铝合金均匀化处理中的应用[J].理化检验:物理分册,2013,49(1):34-38. 被引量:3

8李晋尧,何平.WC-Co硬质合金断裂源的观察与分析[J].理化检验:物理分册,1995,31(1):52-53. 被引量:8

9李晋尧,罗伯芳,黄建忠,李秋娟.W-N-Cu重合金固溶强化的机理研究[J].粉末冶金材料科学与工程,1998,3(2):81-86.

10王赛玉.薄板不锈钢制品中“麻点”缺陷分析[J].热加工工艺,2005(8):61-62. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程];TG111.91[金属学及工艺—物理冶金]

Citation Information:

Using optical microscope and JCXA-733 type electron probe microanalyse. by means of images of SEI, BEI and CXSI, the fracture behaviour of the industrial specimen Of WC-Co-Ni cemented carbide is observed and analysed, with discussion of alloy strength factors.

quote

GB/T 7714-2015 [1] WU Jian-she, HE Ping. Observation and Analysis of Fracture Behaviour of WC-Co-Ni Cemented Carbide[J]. Rare Metals and Cemented Carbides, 1998(3): 7-11.
MLA [1] WU Jian-she, and HE Ping. "Observation and Analysis of Fracture Behaviour of WC-Co-Ni Cemented Carbide." Rare Metals and Cemented Carbides, no. 3, 1998, pp. 7-11.
APA [1] WU Jian-she, & HE Ping. (1998). Observation and Analysis of Fracture Behaviour of WC-Co-Ni Cemented Carbide. Rare Metals and Cemented Carbides(3), 7-11.
IEEE [1] WU Jian-she and HE Ping, "Observation and Analysis of Fracture Behaviour of WC-Co-Ni Cemented Carbide," Rare Metals and Cemented Carbides, no. 3, pp. 7-11, 1998. keywords: {WC-Co-Ni cemented carbide;fracture behaviour;fracture morphology;pore;impurity}