Study and Application of Technology for Violet Tungstic Oxide Preparation AITranslate
Abstract AITranslate
Study is made of the process of violet tungstic oxide preparation and the influnce of APT raw material on the production of violet tungstic oxide are studied.Phase compositions of the products are analyzed by X-ray diffraction;morphology of powder is studied by SEM;microproperties of powder is studied by TEM.Properties of fine tungsten powder and fine tungsten carbide powder from violet tungstic oxide are studied.The result shows that the process of violet tungstic oxide preparation is advanced and reasonable,tungsten powder and tungsten carbide powder from violet tungstic oxide is fine and uniform with good dispersion property and good raw material for the high-performence cemented carbide.
KeyWords AITranslate
1陈绍衣.紫色氧化钨制取钨粉[J].中南矿冶学院学报,1994,25(5):607-611. 被引量:19
2陈绍衣.氧化钨原料对钨粉粒度的影响[J].稀有金属与硬质合金,1994,22(3):10-14. 被引量:15
3陈绍衣,钱崇梁.氧化钨氢还原过程中的物相转变[J].中南工业大学学报,1995,26(5):605-609. 被引量:16
1张冬梅,王文华.扫描电镜在钨制品生产中的应用[J].江西有色金属,2005,19(1):41-44.
2陈树茂,廖小英,张秋和,熊小明,王文华,袁宜红.传统流程生产超细钨粉的工艺优化[J].中国钨业,2005,20(2):36-39. 被引量:5
3徐迎春,姜萍.紫色氧化钨的生产、检测及应用[J].江西冶金,2007,27(3):29-31. 被引量:2
4李新春,易茂中,罗崇玲,谭兴龙,戴煜.带式无舟皿连续还原炉制备粒度均匀的细颗粒钨粉[J].粉末冶金技术,2008,26(3):163-167. 被引量:8
5晏慧娟,熊艰.传统流程制备超细钨粉的研究进展[J].上饶师范学院学报,2008,28(3):50-54. 被引量:3
6张秋和,谢中华,陈树茂,王文华,钟映兰,赵会团.超细碳化钨粉工业生产实践[J].中国钨业,2009,24(6):32-34. 被引量:3
7张彩霞,周阳.高性能超细钨粉的制备工艺研究[J].上海有色金属,2010,31(4):189-193. 被引量:2
8宋志华,郭亨群,吴冲浒,吴其山.以紫钨为原料制备纳米钨粉体的研究[J].稀有金属材料与工程,2011,40(12):2216-2220. 被引量:9
9张卫兵,颜练武,赵声志,杜承功.超细WC粉末微观缺陷的研究[J].硬质合金,2012,29(5):283-288. 被引量:9
10项培云,张华民.紫钨晶型对超细碳化钨粉粒度的影响[J].稀有金属与硬质合金,2018,46(5):75-78. 被引量:6
1丁辉,李潇.碳化钨、碳化钼的制取及研究进展[J].产业科技创新,2020(15):37-38.
2左铁镛.树立科学发展观 实现我国钨业可持续发展[J].中国钨业,2008,23(1):6-9. 被引量:11
3李新春,易茂中,罗崇玲,谭兴龙,戴煜.带式无舟皿连续还原炉制备粒度均匀的细颗粒钨粉[J].粉末冶金技术,2008,26(3):163-167. 被引量:8
4王岗,李海华,黄忠伟,陈美华,王庆康,钟伟良.蓝钨与紫钨氢还原法生产超细钨粉的比较[J].稀有金属材料与工程,2009,38(A01):548-552. 被引量:17
5汤昌仁,易茂中,谭兴龙.喷雾干燥-直接碳化法制备WC-Co复合粉末[J].粉末冶金技术,2010,28(4):279-283. 被引量:7
6傅小明.钨酸铵循环氧化还原法制备亚微米钨粉[J].粉末冶金技术,2011,29(1):50-53. 被引量:4
7王长基,刘鸿,谢璐,杜香珍,李军,华娟霞,龙水秀.钨制品的扫描电镜分析[J].中国钨业,2012,27(5):36-39. 被引量:1
8朱玲旭,燕青芝,郎少庭,徐磊,葛昌纯.钨基面向等离子体材料的研究进展[J].中国有色金属学报,2012,22(12):3522-3528. 被引量:20
9阳冬元,周春成.WC块球磨工艺对WC粉及其合金性能的影响[J].硬质合金,2013,30(3):141-146. 被引量:5
10崔云涛,王金淑,刘伟.亚微米级压制型钪钨阴极粉末的研究[J].北京工业大学学报,2013,39(9):1420-1424.
1徐迎春,姜萍.紫色氧化钨的生产、检测及应用[J].江西冶金,2007,27(3):29-31. 被引量:2
2魏以和,罗廉明,朱立国.一种新的硫酸铜制取工艺──萃取法[J].国外金属矿选矿,1996,33(4):53-55. 被引量:2
3张永会,傅声华,李飞.紫色氧化钨的制备及工艺研究[J].中国钨业,2011,26(3):47-49. 被引量:8
4陈树茂,廖小英,张秋和,熊小明,王文华,袁宜红.传统流程生产超细钨粉的工艺优化[J].中国钨业,2005,20(2):36-39. 被引量:5
5金志和.羰基铁粉的制造工艺和特殊性能[J].粉末冶金工业,1995,5(5):169-173. 被引量:8
6Hans Wohlfromm,Martin Blmacher,Dieter Weinand,曹勇家.粉末注射成形不锈钢——制取工艺、性能、应用——[J].粉末冶金工业,2002,12(4):7-15. 被引量:14
7方少垣.碳硫分析专用助熔剂的原料选择与制备[J].冶金分析,1991,11(3):34-36. 被引量:2
8黄金昌.碳化钛和碳化钨等离子粉末及其混合物的制取工艺[J].稀有金属快报,2000,19(3):12-14.
9黄飞.紫色氧化钨氢还原制取微晶硬质合金用超细钨粉的研究[J].湖南有色金属,2002,18(1):32-34. 被引量:12
10潘叶金,叶俊英.钼粉制取工艺模型化[J].中南矿冶学院学报,1993,24(2):217-220. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TF111.12[冶金工程—冶金物理化学]
Citation Information:
Study is made of the process of violet tungstic oxide preparation and the influnce of APT raw material on the production of violet tungstic oxide are studied.Phase compositions of the products are analyzed by X-ray diffraction;morphology of powder is studied by SEM;microproperties of powder is studied by TEM.Properties of fine tungsten powder and fine tungsten carbide powder from violet tungstic oxide are studied.The result shows that the process of violet tungstic oxide preparation is advanced and reasonable,tungsten powder and tungsten carbide powder from violet tungstic oxide is fine and uniform with good dispersion property and good raw material for the high-performence cemented carbide.
quote
| GB/T 7714-2015 | [1] PENG Ze-hui, LI Ling. Study and Application of Technology for Violet Tungstic Oxide Preparation[J]. Rare Metals and Cemented Carbides, 2003(2): 8-11. |
| MLA | [1] PENG Ze-hui, and LI Ling. "Study and Application of Technology for Violet Tungstic Oxide Preparation." Rare Metals and Cemented Carbides, no. 2, 2003, pp. 8-11. |
| APA | [1] PENG Ze-hui, & LI Ling. (2003). Study and Application of Technology for Violet Tungstic Oxide Preparation. Rare Metals and Cemented Carbides(2), 8-11. |
| IEEE | [1] PENG Ze-hui and LI Ling, "Study and Application of Technology for Violet Tungstic Oxide Preparation," Rare Metals and Cemented Carbides, no. 2, pp. 8-11, 2003. keywords: {violet tungstic oxide;preparation technology;powder morphology;tungsten powder;WC powder} |