Abstract AITranslate

This article introduces the concept of Ga recovery technology from In raffinate by two-stage solvent extraction and electrowinning with hydroximic acid YW-100 with high carbon chain+kerosene+isooctanol and N503+kerosene isooctanol The principle process flowsheet for Ga recovery is presented.

KeyWords AITranslate

In raffinate solvent extraction electrowining Ga recovery

1周令治.稀有金属冶金[M].北京:冶金工业出版社,1988..

1张魁芳,曹佐英,肖连生,曾理,张贵清,李青刚.采用HBL121从锌置换渣高浓度硫酸浸出液中萃取回收镓[J].中国有色金属学报,2014,24(9):2400-2409. 被引量:11

2张魁芳,刘志强,曹洪杨,朱薇,高远,金明亚.不同磷酸酯萃取剂从硫酸体系萃镓性能研究[J].有色金属:冶炼部分,2017,0(4):35-38. 被引量:5

3张伟,吴才贵,张俊峰,高艳芬,周科华,曹洪杨.从锌精矿回收制备高纯镓工艺设计与应用研究[J].有色金属:冶炼部分,2020,0(4):41-46. 被引量:5

4张魁芳,刘志强,陈少纯.镓的提取分离技术现状及发展趋势[J].材料研究与应用,2021,15(1):77-80. 被引量:1

5刘凯华.用P204从硫酸体系中萃取分离铟镓[J].湿法冶金,2021,40(5):386-389. 被引量:4

6张俊峰,张伟,张汇,宫晓丹.工艺参数对石灰乳沉淀法脱除镓电积贫液中铝的影响[J].有色金属工程,2022,12(2):56-60.

7张伟,吴才贵,饶帅,宫晓丹,张登凯,胡东风,周科华.采用P204+YW100萃取工艺制备镓精矿的生产应用[J].稀有金属与硬质合金,2022,50(5):33-39.

1朱茂兰,黄中省,衷水平,陈杭,胡志彪.镓精矿中镓的提取工艺[J].中国有色金属学报,2018,28(11):2351-2357. 被引量:2

2熊英,张莹莹,娄振宁,单炜军,宋玉林.镓的萃取分离研究进展[J].辽宁大学学报:自然科学版,2016,43(4):335-342. 被引量:6

3李银,夏举佩,刘海浪,罗中秋,杨劲.基于响应曲面法提取煤矸石中和液中镓的研究[J].硅酸盐通报,2017,36(3):953-959. 被引量:7

4廖亚龙,曹磊,王祎洋,叶朝.溶液中镓的提取与分离研究进展[J].材料导报,2017,31(15):133-138. 被引量:5

5曹洪杨,金明亚,张魁芳,陶进长,朱薇,刘志强.8-羟基喹啉锗印迹聚合物合成及选择性吸附锗研究[J].有色金属:冶炼部分,2017(9):36-40. 被引量:2

6曹洪杨,金明亚,张魁芳,朱薇,高远,刘志强.8-羟基喹啉锗印迹聚合物合成及吸附过程红外光谱分析[J].有色金属:冶炼部分,2017(12):26-30. 被引量:3

7刘付朋,刘志宏,李玉虎,刘智勇,李启厚.锌粉置换镓锗渣草酸浸出过程[J].中国有色金属学报,2017,27(10):2154-2163. 被引量:7

8朱茂兰,衷水平,黄中省,陈杭,陈晰,胡志彪.含镓明矾石梯级浸出与综合回收工艺[J].中国有色金属学报,2018,28(10):2136-2142. 被引量:1

9刘波,李佳怡,丁云集,郑环东,张深根.报废光伏板回收利用的研究现状[J].稀有金属,2019,43(9):987-996. 被引量:4

10张魁芳,刘志强,刘溢,曹洪杨.P204从硫酸体系萃取镓性能研究[J].有色金属:冶炼部分,2020,0(3):50-54. 被引量:4

1陈志成.薄板坯连铸连轧的工艺设想和经济效益[J].南方钢铁,1989(6):16-20.

2蒋新宇,周春山,汤淑芳.N235萃取色谱法分离萃铟余液中锗的研究[J].稀有金属,2002,26(2):116-119. 被引量:1

3胡益清,陈既明.N503+仲辛醇+煤油的混合萃取剂性能[J].稀有金属与硬质合金,1992,20(2):10-15.

4张秀莉.环烷酸中异辛醇的简便测定方法[J].吉林工学院学报:自然科学版,1999,20(1):37-39. 被引量:1

5童长仁,武金朋,李俊朝,张鹏,刘秀.TBP与N1923协同萃取铜电解液中的砷锑铋[J].有色金属:冶炼部分,2012(5):17-20. 被引量:20

6李亮星,黄茜琳,廖春发,童长仁,黄金堤,姜平国.N235-硫酸-助萃体系锑萃取性能研究[J].中南大学学报:自然科学版,2014,45(7):2151-2156. 被引量:1

7杨明.底吹炉处理锌浸出渣工艺设想[J].世界有色金属,2015,40(11):55-58. 被引量:1

8杨明.底吹炉处理锌浸出渣工艺设想[J].世界有色金属,2015,40(12):22-25.

9山口一良,许彦斌.未来高炉的要求和工艺设想[J].国外钢铁,1992(7):18-22.

10何贻柏.萃锗余液中有机物对锌电解的影响及其衍生物的消除[J].株冶科技,1995,23(4):23-28. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TF843.1[冶金工程—有色金属冶金]

Citation Information:

This article introduces the concept of Ga recovery technology from In raffinate by two-stage solvent extraction and electrowinning with hydroximic acid YW-100 with high carbon chain+kerosene+isooctanol and N503+kerosene isooctanol The principle process flowsheet for Ga recovery is presented.

quote

GB/T 7714-2015 [1] XIAO Hua-li. Study of Ga Recovery Technology from In Raffinate[J]. Rare Metals and Cemented Carbides, 2003(2): 5-7.
MLA [1] XIAO Hua-li. "Study of Ga Recovery Technology from In Raffinate." Rare Metals and Cemented Carbides, no. 2, 2003, pp. 5-7.
APA [1] XIAO Hua-li. (2003). Study of Ga Recovery Technology from In Raffinate. Rare Metals and Cemented Carbides(2), 5-7.
IEEE [1] XIAO Hua-li, "Study of Ga Recovery Technology from In Raffinate," Rare Metals and Cemented Carbides, no. 2, pp. 5-7, 2003. keywords: {In raffinate;solvent extraction;electrowining;Ga recovery}