Flexible, Wearable, and Ultralow-Power-Consumption Electronic Skins Based on a Thermally Reduced Graphene Oxide/Carbon Nanotube Composite Film Flexible, Wearable, and Ultralow-Power-Consumption Electronic Skins Based on a Thermally Reduced Graphene Oxide/Carbon Nanotube Composite Film AITranslate
Abstract AITranslate
Based on a thermally reduced graphene oxide (rGO)/carbon nanotube (CNT) composite film, two kinds of flexible, wearable, and ultralow-power-consumption electronic skins (E-skins) are prepared. They have been used to successfully perceive the signals of stretch, flexion, temperature, and pressure, and their gauge factors (GFs) are 233, 2.37 rad–1, 5.53 × 10–4 °C–1, and 1.58 kPa–1, as the mass fraction of graphene is 20% in the composite film. Compared with the E-skins based on pure rGO film, our E-skins have larger stretching stain (ε) and bending angle (θ) ranges and higher temperature- and pressure-based GF values. Furthermore, the prepared E-skins have been successfully applied in various fields, and their ultralow power consumption has also been confirmed to be below 72 nW in wearable device applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00651
Chinese Library Classification Number:
Citation Information:
Based on a thermally reduced graphene oxide (rGO)/carbon nanotube (CNT) composite film, two kinds of flexible, wearable, and ultralow-power-consumption electronic skins (E-skins) are prepared. They have been used to successfully perceive the signals of stretch, flexion, temperature, and pressure, and their gauge factors (GFs) are 233, 2.37 rad–1, 5.53 × 10–4 °C–1, and 1.58 kPa–1, as the mass fraction of graphene is 20% in the composite film. Compared with the E-skins based on pure rGO film, our E-skins have larger stretching stain (ε) and bending angle (θ) ranges and higher temperature- and pressure-based GF values. Furthermore, the prepared E-skins have been successfully applied in various fields, and their ultralow power consumption has also been confirmed to be below 72 nW in wearable device applications.
quote
| GB/T 7714-2015 | [1] Guangjie Yuan, Shaoguang Lv, Rui Zhang, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00651. |
| MLA | [1] Guangjie Yuan, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00651. |
| APA | [1] Guangjie Yuan, Shaoguang Lv, Rui Zhang, Zhenhua Liu, Yige Zhao, Yin Dong, Zili Li, Weiping Gong, & Yueli Sun. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00651 |
| IEEE | [1] Guangjie Yuan, Shaoguang Lv, Rui Zhang, Zhenhua Liu, Yige Zhao, Yin Dong, Zili Li, Weiping Gong, and Yueli Sun, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00651. keywords: {electronic skin ultralow power consumption rGO/CNT composite film human−machine interactions intelligent roboticsShow More} |