daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Surface Grafting of Electrospun Fibers: Multiscale Characterization and Perspective for Potential Applications AITranslate

Université Paris-Saclay;Lebanese Atomic Energy Commission, Lebanese National Council for Scientific Research (CNRS-L); Université Paris-Saclay; Université Paris-Saclay; Université Paris-Saclay; Université Paris-Saclay; Université Paris-Saclay
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In the previous work, the poly(4-vinyl dimethyl dipicolinate) (PVDPM) polymer grafted on poly(vinyl chloride) (PVC) and poly(ethylene terephthalate) (PET) film or industrial fibers proved its efficiency for trapping uranium and many lanthanides in a liquid environment. In this work, we propose to graft our active polymer on fibers obtained by electrospinning to increase the specific surface of our final material. To address this challenge, surface grafting of electrospun chlorinated poly(vinyl chloride) (PVC-co-CPVC) fibers using supplemental activation reducing agent atom transfer radical polymerization (SARA-ATRP) of poly(4-vinyldipicolinic acid) (PVDPA, acid form of PVDPM) were successfully prepared. The (PVC-co-CPVC)-g-PVDPA fibers show a fast increase in the degree of grafting that goes from 54% after 4 h to 369% after 72 h. Further insights demonstrate successful complexation between the new functional electrospun (PVC-co-CPVC)-g-PVDPA fibers and europium, which proves that it could be a potential candidate for scavenging lanthanides or any agent able to interact with ligands (PVDPA), which opens up innovative application perspectives in the field of polymeric materials.

KeyWords AITranslate

polymer science electrospinning scaffolds porous fibers surface grafting polymer surfaces graft polymerization
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00229

Chinese Library Classification Number:

Citation Information:

In the previous work, the poly(4-vinyl dimethyl dipicolinate) (PVDPM) polymer grafted on poly(vinyl chloride) (PVC) and poly(ethylene terephthalate) (PET) film or industrial fibers proved its efficiency for trapping uranium and many lanthanides in a liquid environment. In this work, we propose to graft our active polymer on fibers obtained by electrospinning to increase the specific surface of our final material. To address this challenge, surface grafting of electrospun chlorinated poly(vinyl chloride) (PVC-co-CPVC) fibers using supplemental activation reducing agent atom transfer radical polymerization (SARA-ATRP) of poly(4-vinyldipicolinic acid) (PVDPA, acid form of PVDPM) were successfully prepared. The (PVC-co-CPVC)-g-PVDPA fibers show a fast increase in the degree of grafting that goes from 54% after 4 h to 369% after 72 h. Further insights demonstrate successful complexation between the new functional electrospun (PVC-co-CPVC)-g-PVDPA fibers and europium, which proves that it could be a potential candidate for scavenging lanthanides or any agent able to interact with ligands (PVDPA), which opens up innovative application perspectives in the field of polymeric materials.

quote

GB/T 7714-2015 [1] Nael Berri, Tamara Elzein, Diana Dragoe, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00229.
MLA [1] Nael Berri, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00229.
APA [1] Nael Berri, Tamara Elzein, Diana Dragoe, Ludivine Houel Renault, Nadine BarrocaAubry, Abdel Wahab Mouhamad, & Philippe Roger. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00229
IEEE [1] Nael Berri, Tamara Elzein, Diana Dragoe, Ludivine Houel Renault, Nadine BarrocaAubry, Abdel Wahab Mouhamad, and Philippe Roger, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00229. keywords: {polymer science;electrospinning;scaffolds;porous fibers;surface grafting;polymer surfaces;graft polymerization}