Molecular Insights into the Interfacial Properties of Cellulose Surfaces with Varying Types of Ionic Liquid Epoxies AITranslate
Abstract AITranslate
Due to the excellent physio-chemical and mechanical properties, ionic liquid epoxies (ILE) can serve as a perfect material for various technologies along with many other materials as a substrate. In this study, we employed molecular dynamics simulations to gain fundamental molecular insights about a conventional epoxy and an imidazolium-based ILE and how adhesion on crystalline cellulose surfaces is affected by cross-linking and the type of ionic liquid (IL) counter anions (e.g. [OAc], [Cl], and [TF2N]) on thermo-mechanical and moisture absorption of bulk ILE were further investigated. When comparing the ILE/cellulose systems versus bulk ILE systems, the results indicate that the presence of a cellulose surface lowers the degree of cross-linking due to the adsorption of the hardener on its surface. Overall, the ILEs/cellulose exhibit a higher interfacial bonding energy than conventional epoxy/cellulose. Improved adhesion is significant for hydrophilic ILEs, which is likely attributed to hydrogen bonds formed between the cellulose and anion molecules. This computational study provides molecular-level insights into the adsorption mechanism of ILE onto a crystalline cellulose surface, leading to the design of smart and multifunctional thermoset adhesives.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00243
Chinese Library Classification Number:
Citation Information:
Due to the excellent physio-chemical and mechanical properties, ionic liquid epoxies (ILE) can serve as a perfect material for various technologies along with many other materials as a substrate. In this study, we employed molecular dynamics simulations to gain fundamental molecular insights about a conventional epoxy and an imidazolium-based ILE and how adhesion on crystalline cellulose surfaces is affected by cross-linking and the type of ionic liquid (IL) counter anions (e.g. [OAc], [Cl], and [TF2N]) on thermo-mechanical and moisture absorption of bulk ILE were further investigated. When comparing the ILE/cellulose systems versus bulk ILE systems, the results indicate that the presence of a cellulose surface lowers the degree of cross-linking due to the adsorption of the hardener on its surface. Overall, the ILEs/cellulose exhibit a higher interfacial bonding energy than conventional epoxy/cellulose. Improved adhesion is significant for hydrophilic ILEs, which is likely attributed to hydrogen bonds formed between the cellulose and anion molecules. This computational study provides molecular-level insights into the adsorption mechanism of ILE onto a crystalline cellulose surface, leading to the design of smart and multifunctional thermoset adhesives.
quote
| GB/T 7714-2015 | [1] Farzin Rahmani, Melissa A. Pasquinelli. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00243. |
| MLA | [1] Farzin Rahmani, and Melissa A. Pasquinelli. ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00243. |
| APA | [1] Farzin Rahmani, & Melissa A. Pasquinelli. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00243 |
| IEEE | [1] Farzin Rahmani and Melissa A. Pasquinelli, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00243. keywords: {ionic liquid epoxy;cellulose nanocrystalline;molecular dynamics simulation;interfacial properties;adhesive} |