Eco-Friendly Water Transfer Printing Free of Primers and Activators AITranslate
Abstract AITranslate
Water transfer printing (WTP) is popular in several industries due to its low cost and ability to coat complicated and heat-sensitive surfaces. However, the primers and activators used in WTP release volatile organic compounds that pollute the environment, and the transferred patterns may suffer from deformation. Herein, an eco-friendly WTP method free of primers and activators was developed by using multilayered films consisting of polyvinyl alcohol films, a pattern, and a hydrophobic supramolecular polymer with polydimethylsiloxane (PDMS) segments (PDMS-PU). PDMS-PU acted as a pressure-sensitive adhesive to adhere the patterns to the transfer objects, thus requiring no primer or activator. Pattern deformation was prevented by coating PDMS-PU on the patterns. Due to the strong adhesion of PDMS-PU, the eco-friendly WTP method could be applied to common substrates including glass, stainless steel, and polyurethane leather. The patterned films transferred by the eco-friendly WTP were hydrophobic and self-healing at room temperature, which prolonged their lifespan. Because it is environmentally friendly and produces hydrophobic and self-healing patterns, the primer/activator-free WTP method described here is superior to conventional methods.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00468
Chinese Library Classification Number:
Citation Information:
Water transfer printing (WTP) is popular in several industries due to its low cost and ability to coat complicated and heat-sensitive surfaces. However, the primers and activators used in WTP release volatile organic compounds that pollute the environment, and the transferred patterns may suffer from deformation. Herein, an eco-friendly WTP method free of primers and activators was developed by using multilayered films consisting of polyvinyl alcohol films, a pattern, and a hydrophobic supramolecular polymer with polydimethylsiloxane (PDMS) segments (PDMS-PU). PDMS-PU acted as a pressure-sensitive adhesive to adhere the patterns to the transfer objects, thus requiring no primer or activator. Pattern deformation was prevented by coating PDMS-PU on the patterns. Due to the strong adhesion of PDMS-PU, the eco-friendly WTP method could be applied to common substrates including glass, stainless steel, and polyurethane leather. The patterned films transferred by the eco-friendly WTP were hydrophobic and self-healing at room temperature, which prolonged their lifespan. Because it is environmentally friendly and produces hydrophobic and self-healing patterns, the primer/activator-free WTP method described here is superior to conventional methods.
quote
| GB/T 7714-2015 | [1] Yechang Feng, Wei Hong, Xudong Chen. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00468. |
| MLA | [1] Yechang Feng, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00468. |
| APA | [1] Yechang Feng, Wei Hong, & Xudong Chen. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00468 |
| IEEE | [1] Yechang Feng, Wei Hong, and Xudong Chen, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00468. keywords: {water transfer printing;activatorfree;primerfree;curvedsurfaceprinting;selfhealable} |