Enhancing the Separation Performance of Aqueous Phase Separation-Based Membranes through Polyelectrolyte Multilayer Coatings and Interfacial Polymerization AITranslate
Abstract AITranslate
The aqueous phase separation (APS) technique allows membrane fabrication without use of unsustainable organic solvents, while at the same time, it provides extensive control over membrane pore size and morphology. Herein, we investigate if polyelectrolyte complexation-induced APS ultrafiltration membranes can be the basis for different types of nanofiltration membranes. We demonstrate that APS membranes can be used as support membranes for functional surface coatings like thin polyelectrolyte multilayer (PEMs) and interfacial polymerization (IP) coatings. Three different PEMs were fabricated on poly(sodium 4-styrene sulfonate) (PSS) poly(allylamine hydrochloride) (PAH) APS ultrafiltration membranes, and only 4.5 bilayers were needed to create nanofiltration membranes with molecular weight cut-off (MWCO) values of 210–390 Da while maintaining a roughly constant water permeability (∼1.7 L·m–2·h–1·bar–1). The PEM-coated membranes showed excellent MgCl2 (∼98%), NaCl (∼70%), and organic micropollutant retention values (>90%). Similarly, fabricating thin polyamide layers on the ultrafiltration PSS-PAH APS membranes by IP resulted in nanofiltration membranes with MWCO values of ∼200 Da. This work shows for the first time that APS membranes can indeed be utilized as excellent support membranes for the application of functional coatings without requiring any form of pretreatment.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00457
Chinese Library Classification Number:
Citation Information:
The aqueous phase separation (APS) technique allows membrane fabrication without use of unsustainable organic solvents, while at the same time, it provides extensive control over membrane pore size and morphology. Herein, we investigate if polyelectrolyte complexation-induced APS ultrafiltration membranes can be the basis for different types of nanofiltration membranes. We demonstrate that APS membranes can be used as support membranes for functional surface coatings like thin polyelectrolyte multilayer (PEMs) and interfacial polymerization (IP) coatings. Three different PEMs were fabricated on poly(sodium 4-styrene sulfonate) (PSS) poly(allylamine hydrochloride) (PAH) APS ultrafiltration membranes, and only 4.5 bilayers were needed to create nanofiltration membranes with molecular weight cut-off (MWCO) values of 210–390 Da while maintaining a roughly constant water permeability (∼1.7 L·m–2·h–1·bar–1). The PEM-coated membranes showed excellent MgCl2 (∼98%), NaCl (∼70%), and organic micropollutant retention values (>90%). Similarly, fabricating thin polyamide layers on the ultrafiltration PSS-PAH APS membranes by IP resulted in nanofiltration membranes with MWCO values of ∼200 Da. This work shows for the first time that APS membranes can indeed be utilized as excellent support membranes for the application of functional coatings without requiring any form of pretreatment.
quote
| GB/T 7714-2015 | [1] Muhammad Irshad Baig, Joshua D. Willott, Wiebe M. de Vos. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00457. |
| MLA | [1] Muhammad Irshad Baig, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00457. |
| APA | [1] Muhammad Irshad Baig, Joshua D. Willott, & Wiebe M. de Vos. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00457 |
| IEEE | [1] Muhammad Irshad Baig, Joshua D. Willott, and Wiebe M. de Vos, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00457. keywords: {aqueous phase separation membranes;polyelectrolyte multilayer;interfacial polymerization;coatings;nanofiltration} |