Study on Fe Removal by MnCl_2 from Al-Si Alloy AITranslate

School of Materials and Metallurgical of Northeast University;School of Materials and Metallurgical of Northeast University;School of Materials and Metallurgical of Northeast University;School of Materials and Metallurgical of Northeast University;School of Materials and Metallurgical of Northeast University;School of Materials and Metallurgical of Northeast University;School of Materials and Metallurgical of Northeast University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The crude Al-Si alloy produced by carbon electrothermal reduction should be free of iron impurity after dilution refining. and slow manganese d However,iron removal by directly adding manganese will result in manganese loss illusion. Study is made on the feasibility of Fe removal from crude Al-Si alloy by MnCl2 instead of single Mn. The results show that MnCl2 can react with Al to produce Mn. Therefore, MnCl2 can substitute Mn to remove iron impurity from Al-Si alloy.

KeyWords AITranslate

crude Al-Si alloy iron removal MnCl2 Al-Si alloy for casting

1柳连舜.电热法制取铝硅合金──发展铝工业的捷径[J].轻金属,1995(6):40-44. 被引量:7

2国家机械工业委员会.有色金属熔炼工工艺学[M].北京:机械工业出版社,1988.

3印飞,杨江波,王亦新,王国祥,孙宝德,李振,王定国.消除铝硅合金中铁相有害作用的方法分析[J].热加工工艺,2001,30(3):61-63. 被引量:8

4孙业赞,于敞,厉松春,邱虹祥,张国伟.铁在铝硅合金中存在的形态及其作用分析[J].铸造,1998(7):42-46. 被引量:36

5杨江波,印飞.改善铝硅合金中铁相形态的措施[J].铸造,2000,49(8):454-459. 被引量:32

6张磊,焦万丽,尉海军,姚广春.锰结合预先热处理对铝硅合金中富铁相组织和力学性能的影响[J].中国有色金属学报,2005,15(3):368-373. 被引量:35

7Wang Yaowu, Feng Naixiang, You Jing, et al. Study of making casting grade aluminum-silicon alloy with coarse aluminum-silicon alloy produced by carbothermal reduction of aluminous ore[J]. Light Metals, 2007, (6) : 477- 482.

8梁英教 车荫昌.无机物热力学数据手册[M].沈阳:东北大学出版社,1994.383.

1罗旭东,汤昌廷,马军创,靳承岗,邵宇光,王家淳.铝及铝合金中Fe、Si杂质元素的冶金与熔铸过程控制[J].铸造,2015,64(5):440-444. 被引量:10

2孙德勤,徐正亚,戴军.废铝熔体中去除夹杂铁元素的工艺试验[J].铸造技术,2016,37(1):95-98. 被引量:3

3孙德勤,周自强,费有静,杨敬军,朱苏.改善废铝再生中Fe相析出形态的工艺试验[J].铸造,2017,66(4):403-407. 被引量:4

4林向飞,康巍,李红英.硼和稀土对铝阴极板耐腐蚀性能的影响[J].有色金属科学与工程,2017,8(3):42-47. 被引量:3

5林敏,林建国,易绿林.硼对电解锌用铝阴极板组织与耐腐蚀性能的影响[J].湘潭大学学报:自然科学版,2018,40(4):1-6.

6孙德勤,袁国超,王天华,刘峰,吴强.高Fe含量铝合金中优化富Fe析出相形态的工艺试验[J].常熟理工学院学报,2018,32(2):67-72.

7鲍雨,赵世民,吕国强,王毅博,肖庭,马文会.电磁分离一次铝硅合金中的富铁相[J].过程工程学报,2019,19(2):309-316. 被引量:1

1葛素静,刘永昌,叶珍,鲁园园,毛贻国,孙芳芳,苑高利,霍臣明,马朝利.再生A356铝合金生产工艺及性能研究[J].特种铸造及有色合金,2022,42(4):450-454. 被引量:2

2吴桃泉,杜军,关玉芹,曹东,李文芳,许德英.Mg_2Si/富铁A356再生铝基复合材料的组织及耐磨性研究[J].铸造,2016,65(10):970-974. 被引量:5

3倪威,倪红军,王平,汪兴兴,吉广健,吕帅帅.主要合金元素对6063铝型材表面质量的影响及控制[J].有色金属:冶炼部分,2017(5):59-63. 被引量:5

4赵丽娟.过热处理温度对AlSi7Mg0.6铝合金组织及力学性能的影响[J].热加工工艺,2017,46(17):105-106. 被引量:2

5孙德勤,朱苏,吴培君.改善铝合金中富Fe相析出形态的技术进展[J].铸造,2018,67(1):20-23. 被引量:6

6马晴,王云龙,李慧慧.基于在线采集的电解铝自动化控制设计[J].中国锰业,2018,36(1):130-133. 被引量:1

7姜宏伟,丁文捷,张树玲,张佃平.废铝再生技术分析与对策[J].轻金属,2017(12):26-29. 被引量:5

8孙德勤,江宽,崔凯,周自强.再生铝制备汽车零部件技术的应用与发展[J].铸造技术,2018,39(6):1387-1391. 被引量:10

9张诗瀚,王广,杜亚星,王静松,薛庆国.含钛铌铁精矿含碳球团熔分过程试验研究[J].有色金属科学与工程,2018,9(3):5-10. 被引量:2

10孙德勤,陈慧君,文青草,王烨.耐热铝合金的发展与应用[J].有色金属科学与工程,2018,9(3):65-69. 被引量:14

1辛丽,李铁藩,周龙江,李美栓,杨锐,李东.表面涂少量氯化锰提高Ti47Al2Cr2Nb合金高温抗氧化性[J].中国腐蚀与防护学报,1999,19(5):311-314. 被引量:4

2刘扭参,杨安杰,李俊青,刘忠侠,杨明生.过滤对电热法制备ZL102合金显微组织和力学性能的影响[J].机械工程材料,2010,34(12):45-47. 被引量:2

3王建民,李志芳,张瑞英.稀土元素改善铝-硅合金铸造组织的研究[J].轻合金加工技术,2005,33(3):47-50. 被引量:13

4王华森.Ti-6Al-4V合金相变点的测定值与计算值的比较—计算相变点的经验公式[J].稀有金属材料与工程,1989(3):47-49. 被引量:5

5马景灵,文九巴,焦孟旺,郭炜.合金元素Mn对铝合金阳极组织与性能的影响[J].腐蚀与防护,2008,29(11):667-669. 被引量:5

6孙德勤,徐正亚,戴军.废铝熔体中去除夹杂铁元素的工艺试验[J].铸造技术,2016,37(1):95-98. 被引量:3

7孙德勤,徐越,戴国洪,勾淑苹.熔剂法去除废铝熔体中铁元素的试验研究[J].铸造,2016,65(1):80-83. 被引量:2

8刘扭参,李俊青,刘忠侠,杨瑞宾.电热法生产过共晶Al-Si合金的组织与性能研究[J].热加工工艺,2009,38(23):87-90. 被引量:4

9蒋咏,马文会,魏奎先,周阳,戴永年.定向凝固技术去除超冶金级硅中铁的实验研究[J].热加工工艺,2011,40(23):17-18. 被引量:8

10刘伏梅,刘志坚.铁在铝合金中的有害作用及其控制[J].内燃机配件,2002(4):7-10. 被引量:12

Basic Information:

DOI:

Chinese Library Classification Number:TG146.21[金属学及工艺—金属材料]

Citation Information:

The crude Al-Si alloy produced by carbon electrothermal reduction should be free of iron impurity after dilution refining. and slow manganese d However,iron removal by directly adding manganese will result in manganese loss illusion. Study is made on the feasibility of Fe removal from crude Al-Si alloy by MnCl2 instead of single Mn. The results show that MnCl2 can react with Al to produce Mn. Therefore, MnCl2 can substitute Mn to remove iron impurity from Al-Si alloy.

quote

GB/T 7714-2015 [1] WANG Yao-wu, FENG Nai-xiang, YOU Jing, et al. Study on Fe Removal by MnCl_2 from Al-Si Alloy[J]. Rare Metals and Cemented Carbides, 2008(4): 10-13.
MLA [1] WANG Yao-wu, et al., "Study on Fe Removal by MnCl_2 from Al-Si Alloy." Rare Metals and Cemented Carbides, no. 4, 2008, pp. 10-13.
APA [1] WANG Yao-wu, FENG Nai-xiang, YOU Jing, PENG Jian-ping, ZHANG Fu-shun, WANG Zi-qian, & WU Xiao-lei. (2008). Study on Fe Removal by MnCl_2 from Al-Si Alloy. Rare Metals and Cemented Carbides(4), 10-13.
IEEE [1] WANG Yao-wu, FENG Nai-xiang, YOU Jing, PENG Jian-ping, ZHANG Fu-shun, WANG Zi-qian, and WU Xiao-lei, "Study on Fe Removal by MnCl_2 from Al-Si Alloy," Rare Metals and Cemented Carbides, no. 4, pp. 10-13, 2008. keywords: {crude Al-Si alloy;iron removal;MnCl2;Al-Si alloy for casting}