Property of the Agglomerates for Al-Si Alloy Preparation by Electrothermal Process(Ⅰ)——Porosity AITranslate
Abstract AITranslate
Description is made of a novel method of measuring porosity of the agglomerates for Al-Si alloy preparation by electrothermal process. The influence of pressure, sintering conditions and material particle size on the agglomerate porosity was also investigated. The results show that the agglomerate porosity decreases with higher pressure and smaller particle size, but increases with higher sintering temperature and longer sintering time. Sintering conditions have greater influence on the agglomerate porosity than the pressure and the material particle size.
KeyWords AITranslate
1ZHONGXiangchong.Outlook on Refractories Development in China in the New Century[J].中国耐火材料:英文版,2001,10(4):3-9. 被引量:3
2李太昌,潘海娥.铝土矿选矿尾矿资源化利用途径探讨[J].矿产保护与利用,2007,27(1):40-43. 被引量:18
3张万福.利用俄罗斯技术建设我国的电热铝硅合金工厂[J].轻金属,1998(8):38-41. 被引量:3
4姚广春,张晓明,孙挺,于先进,王贵民.电热法制取硅铝合金中制团对还原反应的影响[J].有色金属:冶炼部分,1998(1):26-27. 被引量:3
5张烽,李蒙姬.含铝50%的硅铝合金生产技术[J].铁合金,2003,34(4):17-21. 被引量:9
6涂赣峰,张世荣,任存治,邢鹏飞,李春材,张成祥.内配碳稀土精矿团块的性能研究[J].有色矿冶,2000,16(3):18-21. 被引量:2
1霍光庶.硅铝合金的电热生产方法[J].轻金属,1990(10):37-40. 被引量:2
2吴贤熙.高铝铝硅合金作皮江法炼镁还原剂的探讨[J].轻金属,1991(7):36-39. 被引量:7
3姚广春,孙挺,张晓明,于先进,王贵民.电热法生产硅铝合金的探讨[J].有色金属:冶炼部分,1997(5):11-13. 被引量:7
4张晓明,姚广春,郭清富,张东峰,柳晓梅.铝硅合金热法炼镁的研究[J].轻金属,1998(5):42-44. 被引量:9
5程士富.钢水用Al—Si合金终脱氧的探讨[J].辽宁冶金,1994(2):20-23.
6周玲玉.泡沫陶瓷及其应用[J].耐火材料信息,2003(3):5-6.
7严昌永.铝硅合金熔炼新工艺[J].航空工艺技术,1992,0(5):38-39. 被引量:1
8文志军,岑明进,吴杰.高效无氟脱磷团块的实验研究[J].河南冶金,2010(3):20-23.
9邓涛,胡长庆.MgO在烧结矿中分布规律的研究[J].河南冶金,2014,22(2):8-11. 被引量:1
10张明杰,邱竹贤.以煤矸石及其粉煤灰为原料电热法直接制取铝硅铁合金[J].铁合金,1992(4):19-23. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TF802.6[冶金工程—有色金属冶金]
Citation Information:
Description is made of a novel method of measuring porosity of the agglomerates for Al-Si alloy preparation by electrothermal process. The influence of pressure, sintering conditions and material particle size on the agglomerate porosity was also investigated. The results show that the agglomerate porosity decreases with higher pressure and smaller particle size, but increases with higher sintering temperature and longer sintering time. Sintering conditions have greater influence on the agglomerate porosity than the pressure and the material particle size.
quote
| GB/T 7714-2015 | [1] YANG Dong, FU Da-xue, WANG Yao-wu, et al. Property of the Agglomerates for Al-Si Alloy Preparation by Electrothermal Process(Ⅰ)——Porosity[J]. Rare Metals and Cemented Carbides, 2008(4): 5-9. |
| MLA | [1] YANG Dong, et al., "Property of the Agglomerates for Al-Si Alloy Preparation by Electrothermal Process(Ⅰ)——Porosity." Rare Metals and Cemented Carbides, no. 4, 2008, pp. 5-9. |
| APA | [1] YANG Dong, FU Da-xue, WANG Yao-wu, & FENG Nai-xiang. (2008). Property of the Agglomerates for Al-Si Alloy Preparation by Electrothermal Process(Ⅰ)——Porosity. Rare Metals and Cemented Carbides(4), 5-9. |
| IEEE | [1] YANG Dong, FU Da-xue, WANG Yao-wu, and FENG Nai-xiang, "Property of the Agglomerates for Al-Si Alloy Preparation by Electrothermal Process(Ⅰ)——Porosity," Rare Metals and Cemented Carbides, no. 4, pp. 5-9, 2008. keywords: {Al-Si alloy;agglomerate porosity;pressure;sintering condition;particle size} |