Efficient Nondoped Pure Red/Near-Infrared TADF OLEDs by Designing and Adjusting Double Quantum Wells Structure Efficient Nondoped Pure Red/Near-Infrared TADF OLEDs by Designing and Adjusting Double Quantum Wells Structure AITranslate

University of Science and Technology of China; Changchun Institute of Applied Chemistry; Changchun Institute of Applied Chemistry; Changchun Institute of Applied Chemistry; Changchun Institute of Applied Chemistry; University of Science and Technology of China
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The selection of host materials has a great impact on the performance of doping devices, especially near-infrared (NIR) emitters. In this investigation, four diverse host materials serve as a potential barrier layer (PBL) to confine and balance holes and electrons within the potential well layer (PWL), TPA-DCPP, for fabricating nondoped NIR thermally activated delayed fluorescence (TADF) organic light-emitting diodes (OLEDs) (NNT-OLEDs) with double quantum wells’ (DQWs) structure. The hole-type host (mCP) forms an optimum interface energy barrier (IEB) and disperses carriers and excitons in each well, which helps to widen the recombination interval of carriers and restrain the quenching of excitons. Finally, OLEDs with pure red emission and a maximum external quantum efficiency (EQEmax) of nearly 15% (with 0.5 nm well width), deep-red emission with an EQEmax of 12% (with 1.0 nm well width), and NIR emission with an EQEmax of 3.3% (with 5.5 nm well width) are achieved with tunable emission peaks within the range of 641–700 nm by adjusting well width, which are significantly superior to those of doped devices based on the same emitter. This investigation demonstrates a simple, feasible, and effective design strategy for achieving efficient fluorescent OLEDs with controllable wavelength, which solves the blue shift problem in traditional NIR devices of host–guest structure.

KeyWords AITranslate

nearinfrared emission interface energy barrier nondoped devices double quantum wells well width
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00531

Chinese Library Classification Number:

Citation Information:

The selection of host materials has a great impact on the performance of doping devices, especially near-infrared (NIR) emitters. In this investigation, four diverse host materials serve as a potential barrier layer (PBL) to confine and balance holes and electrons within the potential well layer (PWL), TPA-DCPP, for fabricating nondoped NIR thermally activated delayed fluorescence (TADF) organic light-emitting diodes (OLEDs) (NNT-OLEDs) with double quantum wells’ (DQWs) structure. The hole-type host (mCP) forms an optimum interface energy barrier (IEB) and disperses carriers and excitons in each well, which helps to widen the recombination interval of carriers and restrain the quenching of excitons. Finally, OLEDs with pure red emission and a maximum external quantum efficiency (EQEmax) of nearly 15% (with 0.5 nm well width), deep-red emission with an EQEmax of 12% (with 1.0 nm well width), and NIR emission with an EQEmax of 3.3% (with 5.5 nm well width) are achieved with tunable emission peaks within the range of 641–700 nm by adjusting well width, which are significantly superior to those of doped devices based on the same emitter. This investigation demonstrates a simple, feasible, and effective design strategy for achieving efficient fluorescent OLEDs with controllable wavelength, which solves the blue shift problem in traditional NIR devices of host–guest structure.

quote

GB/T 7714-2015 [1] Yufu Sun, Weidong Sun, Wenxing Liu, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00531.
MLA [1] Yufu Sun, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00531.
APA [1] Yufu Sun, Weidong Sun, Wenxing Liu, Xiaokang Li, Jiaxuan Yin, & Liang Zhou. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00531
IEEE [1] Yufu Sun, Weidong Sun, Wenxing Liu, Xiaokang Li, Jiaxuan Yin, and Liang Zhou, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00531. keywords: {nearinfrared emission interface energy barrier nondoped devices double quantum wells well width}