Abstract AITranslate

Herein, we designed and synthesized a two-dimensional covalent organic framework (2D-COF) of a Schiff base using a mechanical chemical grinding method. Moreover, capsaicin@chitosan (CAP@CS) microcapsules were loaded on a TpPa-1 COF by a physical adsorption method to prepare composites (CAP@CS/TpPa-1), which realized the pH-sensitive controlled release of the fungicide CAP, dispersed in fluorocarbon resin to prepare an intelligent coating with environmentally friendly long-term antifouling performance. TpPa-1 improves the antibacterial efficiency by increasing the dispersity of CAP@CS in the resin. Therefore, a CAP release amount of 2 wt % composite coating can meet the minimum bacteriostatic concentration of 37.5 μg/mL required for antifouling. Importantly, pH-responsive controlled release caused by the protonation of CS and the electrostatic interaction between CAP@CS and TpPa-1 COF and increased bacterial contact area by CAP@CS reunion inhibited by TpPa-1 COF improve the bactericidal efficiency of the composite. The composite coating has excellent corrosion resistance, mainly because COF extends the propagation path of the corrosive medium.

KeyWords AITranslate

2DCOF pH response coating antibacterial anticorrosion
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02138

Chinese Library Classification Number:

Citation Information:

Herein, we designed and synthesized a two-dimensional covalent organic framework (2D-COF) of a Schiff base using a mechanical chemical grinding method. Moreover, capsaicin@chitosan (CAP@CS) microcapsules were loaded on a TpPa-1 COF by a physical adsorption method to prepare composites (CAP@CS/TpPa-1), which realized the pH-sensitive controlled release of the fungicide CAP, dispersed in fluorocarbon resin to prepare an intelligent coating with environmentally friendly long-term antifouling performance. TpPa-1 improves the antibacterial efficiency by increasing the dispersity of CAP@CS in the resin. Therefore, a CAP release amount of 2 wt % composite coating can meet the minimum bacteriostatic concentration of 37.5 μg/mL required for antifouling. Importantly, pH-responsive controlled release caused by the protonation of CS and the electrostatic interaction between CAP@CS and TpPa-1 COF and increased bacterial contact area by CAP@CS reunion inhibited by TpPa-1 COF improve the bactericidal efficiency of the composite. The composite coating has excellent corrosion resistance, mainly because COF extends the propagation path of the corrosive medium.

quote

GB/T 7714-2015 [1] Zhipeng Zhao, Huimeng Feng, Dong Qin, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02138.
MLA [1] Zhipeng Zhao, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02138.
APA [1] Zhipeng Zhao, Huimeng Feng, Dong Qin, Wen Li, Wei Wang, & Shougang Chen. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02138
IEEE [1] Zhipeng Zhao, Huimeng Feng, Dong Qin, Wen Li, Wei Wang, and Shougang Chen, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c02138. keywords: {2DCOF;pH response;coating;antibacterial;anticorrosion}