Effect of Heat Treatment Temperature on Microstructure of Ti-42.5Al-4Nb-1Mo-0.2B Alloy for Internal Combustion Engine AITranslate
Abstract AITranslate
The effect was studied of heat treatment temperature on microstructure of Ti-42.5Al-4Nb-1Mo-0.2 Balloy for internal combustion engine.The results show that the alloy has nearly lamellar microstructure in the as-cast state,mainly composed of fine lamellar clusters and B2 phase andγphase around the lamellar clusters.The quenched alloys at 1200℃ and 1250℃ have similar microstructure.With the quenching temperature is increased to 1300℃,γphase in quenched microstructure disappears,and there are some long rod-shaped fine α2 grains in B2 grains.After heat treatment at 1200℃ and cooling to room temperature, the alloy has the microstructure of α2/γ lamellar clusters,B2 phase andγphase.When the heat treatment temperature is up to 1250℃,the number ofαgrains and α2/γ lamellar clusters begins to increase, and their size also gradually increases.When the heat treatment temperature rises to 1300℃,the alloy has nearly lamellar fine α+β microstructure.
KeyWords AITranslate
1王津,钟宏,张铁邦,寇宏超,胡锐.Mo对高Nb-TiAl合金凝固路径及凝固组织的影响[J].特种铸造及有色合金,2011,31(4):376-379. 被引量:7
2陈玉勇,张树志,孔凡涛,刘祖岩,林均品.新型β-γTiAl合金的研究进展[J].稀有金属,2012,36(1):154-160. 被引量:31
3郑立静,杨莉莉,张虎.微量元素B在γ-TiAl基合金的应用研究进展[J].稀有金属材料与工程,2010(10):1875-1880. 被引量:15
4李建波,刘咏,王岩,刘彬,杨广宇.微量B对铸态TiAl基合金显微组织及热变形行为的影响[J].粉末冶金材料科学与工程,2012,17(4):414-422. 被引量:4
5李书江,王艳丽,林均品,林志,陈国良.微量C,B对高铌TiAl合金显微组织与力学性能的影响[J].稀有金属材料与工程,2004,33(2):144-148. 被引量:24
6王慧,程芳.Ti-40Al-3.5Nb-0.8Mo-0.3Y高温合金组织和力学性能研究[J].稀有金属与硬质合金,2018,46(3):19-22. 被引量:2
7宗波,董恒平,冯冲.C元素含量对TiAl合金显微组织与力学性能的影响[J].热加工工艺,2018,47(16):104-107. 被引量:3
8范爱一,李慧中,梁霄鹏,陈永辉,齐叶龙.热变形Ti-45Al-7Nb-0.3W合金的显微组织与力学性能[J].材料工程,2018,46(7):121-126. 被引量:6
1何永胜,胡锐,罗文忠,何涛,赖运金,杜玉俊,刘向宏,杨劼人.热处理对近β锻造的多元Ti_2AlNb基合金组织和性能的影响[J].稀有金属材料与工程,2018,47(11):3460-3467. 被引量:7
2周玲玲,孙威.FIB加工、扫描及透射电子显微镜相结合的复杂合金相层状组织表征[J].电子显微学报,2018,37(6):590-595. 被引量:8
3胡春东,曾斌,孟利,董瀚.奥氏体化温度对3Cr3Mo2NiVNb钢组织和力学性能的影响[J].热加工工艺,2018,47(22):234-236. 被引量:3
4韩墨流,徐平伟,万明攀,梁益龙,杜剑平,梁宇.TA19钛合金中未完全转变组织特征与拉伸性能[J].稀有金属材料与工程,2018,47(12):3768-3775. 被引量:3
5孙才,罗虓,冯玮,曹婷婷,易义凤.γ-TiAl合金表面氧化形貌研究[J].湖南有色金属,2018,34(6):46-48.
6杨光,刘佳蓬,钦兰云,任宇航,王维.激光沉积TA15钛合金高周疲劳性能研究[J].稀有金属,2018,42(11):1134-1142. 被引量:8
7庞丹莉,邓炳耀,刘庆生,李大伟,申莹.石墨烯改性聚丙烯复合滤料的制备及其过滤性能[J].化工新型材料,2018,46(S1):51-53.
8马权,黄朝文.Ti-55531合金的高周疲劳断口形貌分析[J].中国有色金属学报,2018,28(12):2467-2475. 被引量:2
9付柯焴,潘明明,王守晶,雷明霞.离子氮化时间对DC53钢显微组织和性能的影响[J].热加工工艺,2018,47(22):162-164. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG146.2[金属学及工艺—金属材料]
Citation Information:
The effect was studied of heat treatment temperature on microstructure of Ti-42.5Al-4Nb-1Mo-0.2 Balloy for internal combustion engine.The results show that the alloy has nearly lamellar microstructure in the as-cast state,mainly composed of fine lamellar clusters and B2 phase andγphase around the lamellar clusters.The quenched alloys at 1200℃ and 1250℃ have similar microstructure.With the quenching temperature is increased to 1300℃,γphase in quenched microstructure disappears,and there are some long rod-shaped fine α2 grains in B2 grains.After heat treatment at 1200℃ and cooling to room temperature, the alloy has the microstructure of α2/γ lamellar clusters,B2 phase andγphase.When the heat treatment temperature is up to 1250℃,the number ofαgrains and α2/γ lamellar clusters begins to increase, and their size also gradually increases.When the heat treatment temperature rises to 1300℃,the alloy has nearly lamellar fine α+β microstructure.
quote
| GB/T 7714-2015 | [1] QIU Cui-rong. Effect of Heat Treatment Temperature on Microstructure of Ti-42.5Al-4Nb-1Mo-0.2B Alloy for Internal Combustion Engine[J]. Rare Metals and Cemented Carbides, 2018(6): 47-50. |
| MLA | [1] QIU Cui-rong. "Effect of Heat Treatment Temperature on Microstructure of Ti-42.5Al-4Nb-1Mo-0.2B Alloy for Internal Combustion Engine." Rare Metals and Cemented Carbides, no. 6, 2018, pp. 47-50. |
| APA | [1] QIU Cui-rong. (2018). Effect of Heat Treatment Temperature on Microstructure of Ti-42.5Al-4Nb-1Mo-0.2B Alloy for Internal Combustion Engine. Rare Metals and Cemented Carbides(6), 47-50. |
| IEEE | [1] QIU Cui-rong, "Effect of Heat Treatment Temperature on Microstructure of Ti-42.5Al-4Nb-1Mo-0.2B Alloy for Internal Combustion Engine," Rare Metals and Cemented Carbides, no. 6, pp. 47-50, 2018. keywords: {TiAl alloy;microstructure;heat treatment;quenching;temperature} |