daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Ni-based Alloy Aluminization Mechanism AITranslate

Department of Chemistry and Chemical Engineering, Yueyang Teachers College;Department of Chemistry and Chemical Engineering, Yueyang Teachers College;Department of Chemistry and Chemical Engineering, Yueyang Teachers College
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made on the formation of me chanism of Ni based alloy aluminization,whichisthonght to be made up of four steps to be controlled mostly by solid Phase diffusion.The diffusion speed is mainly depended on the aluminization temperature,then aluminization time.In addition,different aluminization temperature will result in different generation speed of phases with different activitation energy.

KeyWords AITranslate

Ni based alloy aluminization diffusion activitation energy

1李金桂.航空产品腐蚀及其控制手册[M].,1984,12..

2叶锐曾.不同温度时效对GH220合金渗Al层的影响[J].北京钢铁学院学报,1986,:85-85.

1蔡建宾,吴宇建,张冬冬,戴品强.Al_(0.5)CoCrFeNiB_x多主元高熵合金的组织结构和力学性能[J].稀有金属与硬质合金,2011,39(4):37-40. 被引量:11

2王晓妮,王新刚.包埋粉末渗铝的组织和性能[J].内江科技,2014,35(9):70-70.

3谢小武,刘光明,张正义,罗强,黄健航.K403镍基合金渗铝层微裂纹与扭转应力关系[J].金属热处理,2018,43(1):116-120. 被引量:2

1彭存远,马明星,叶晓阳,吴绮雯,张伟明,刘文今.添加Mn对激光制备Al_(1.3)FeCoNiCuCr涂层组织和性能的影响[J].应用激光,2014,34(3):175-180. 被引量:8

2安旭龙,刘其斌,郑波.碳化钨对激光熔覆高熵合金的影响[J].强激光与粒子束,2014,26(12):249-254. 被引量:15

3李栋梁,周芳,余师豪.激光熔覆FeCrNiMnMo_xB_(0.5)高熵合金涂层组织与耐蚀性能[J].强激光与粒子束,2016,28(2):190-195. 被引量:18

4饶湖常,戴品强,陈鼎宁,王乾廷.碳含量对FeCoCrNiMnC_x高熵合金显微组织与性能的影响[J].机械工程材料,2016,40(8):76-80. 被引量:10

5李涵,马玲玲,位超群,孙琳,张维平.钛合金表面激光熔覆AlB_xCoCrNiTi高熵合金涂层的组织与性能[J].表面技术,2017,46(6):226-231. 被引量:28

6黄纯可,李伟,刘平,张柯,马凤仓,刘新宽,陈小红,何代华.磁控溅射法制备Al_xCoCrFeNi高熵合金薄膜的微观组织和力学性能研究[J].功能材料,2017,48(6):6144-6148. 被引量:17

7李安敏,史君佐,谢明款.高熵合金力学性能的研究进展[J].材料导报,2018,32(3):461-466. 被引量:13

8谢亚茜,陈业新,马星星.硼含量对FeCoNiCrAl_(0.1)B_(x)高熵合金组织和力学性能的作用[J].上海大学学报:自然科学版,2021,27(2):280-288. 被引量:1

9桂敏,王华.某型航空发动机涡轮叶片榫头表面铝含量与渗铝层深度关系研究[J].航空维修与工程,2022(12):46-48.

10李荣斌,邹传乐,张志玺,张如林,彭望君.硼对铸态Al_(0.3)CoCrFeNi高熵合金组织及性能的影响[J].稀有金属材料与工程,2023,52(2):667-674.

1赵宇光,周伟,赵玉谦,梁云虹,秦庆东.分散剂Y_2O_3对渗铝层的影响[J].稀有金属材料与工程,2005,34(10):1574-1577. 被引量:3

2高原,贺志勇,李成明,唐宾.膏剂辉光离子渗硼渗铝机理的探讨[J].热加工工艺,1991(4):6-9. 被引量:2

3马勤,尤少君,贾建刚,安亮.AISI 1020钢表面熔融盐法渗铝及其机理[J].兰州理工大学学报,2010,36(3):10-12. 被引量:1

4查康,魏晓伟.添加剂对镁合金微弧氧化的影响[J].表面技术,2006,35(4):56-58. 被引量:15

5孙大仁,曹占义,杨晓红,刘勇兵,孙妍.低碳钢在铝合金熔体中冲蚀磨损的研究[J].腐蚀科学与防护技术,2003,15(5):288-291.

6安家菊,魏晓伟.大电流下铝合金快速硬质阳极氧化工艺的研究[J].电镀与涂饰,2005,24(6):29-31. 被引量:8

7徐瑞东,王军丽,薛方勤,郭忠诚.铝合金常温脉冲硬质阳极氧化膜性能的研究[J].材料保护,2003,36(9):34-35. 被引量:14

8王满力,周元康,黄威良.金属表面K_2Cr_2O_7氧化色膜研究[J].材料保护,2002,35(12):39-40. 被引量:1

9王平,赵文福,居冰峰,张飞虎,袁哲俊.铸铁砂轮电解氧化膜在ELID镜面磨削中的作用机理研究[J].金刚石与磨料磨具工程,1996,16(6):25-28. 被引量:3

10蒋建忠,赵永武.CMP过程芯片表面氧化膜生成速度影响因素的分析[J].现代制造工程,2006(10):51-55. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TG166.786[金属学及工艺—热处理]

Citation Information:

Study is made on the formation of me chanism of Ni based alloy aluminization,whichisthonght to be made up of four steps to be controlled mostly by solid Phase diffusion.The diffusion speed is mainly depended on the aluminization temperature,then aluminization time.In addition,different aluminization temperature will result in different generation speed of phases with different activitation energy.

quote

GB/T 7714-2015 [1] YAN Jian-hui, CHEN Guo-bin, LU Jian-hong. Study on Ni-based Alloy Aluminization Mechanism[J]. Rare Metals and Cemented Carbides, 2001(1): 8-11.
MLA [1] YAN Jian-hui, et al., "Study on Ni-based Alloy Aluminization Mechanism." Rare Metals and Cemented Carbides, no. 1, 2001, pp. 8-11.
APA [1] YAN Jian-hui, CHEN Guo-bin, & LU Jian-hong. (2001). Study on Ni-based Alloy Aluminization Mechanism. Rare Metals and Cemented Carbides(1), 8-11.
IEEE [1] YAN Jian-hui, CHEN Guo-bin, and LU Jian-hong, "Study on Ni-based Alloy Aluminization Mechanism," Rare Metals and Cemented Carbides, no. 1, pp. 8-11, 2001. keywords: {Ni based alloy;aluminization;diffusion;activitation energy}