Study of Decomposition of Enriched Ta-bearing Alkaline Metals AITranslate
Abstract AITranslate
Analysis is made of the influence of alkali metals K and Na on the decomposition ratio of enriched Ta.The decomposition ratio can be improved from 92% to ≥99% by the adoption of precipitation conversion theory and proper addition of quartz powder as conversion agent without heating throughout the process.
KeyWords AITranslate
1韩建设,赵明智,周勇.氟钽酸钾生产工艺及装备的进展[J].稀有金属与硬质合金,2004,32(3):44-48. 被引量:10
2韩建设,张劲.钽铌水冶分解提取工艺及设备的进展[J].稀有金属与硬质合金,2003,31(4):27-31. 被引量:14
1韩建设,周勇.钽铌萃取分离工艺与设备进展[J].稀有金属与硬质合金,2004,32(2):15-20. 被引量:16
2韩建设,赵明智,周勇.氟钽酸钾生产工艺及装备的进展[J].稀有金属与硬质合金,2004,32(3):44-48. 被引量:10
3赵明智,张劲.钛钽铌矿强化分解工艺的研究[J].稀有金属与硬质合金,2004,32(4):25-28. 被引量:2
4周丽.提高氟钽酸钾产品直收率的研究[J].稀有金属与硬质合金,2006,34(1):49-51. 被引量:3
5韩建设,赵明智,王才明,张劲,周勇.钽铌湿法冶炼的“三废”综合治理工艺探讨[J].稀有金属与硬质合金,2006,34(4):40-44. 被引量:12
6王伟,李辉,郑培生.低品位钽铌原料的湿法冶金新工艺研究[J].稀有金属快报,2008,27(4):31-36. 被引量:10
7王晓辉,郑诗礼,徐红彬,张懿.ICP-AES法测定难分解钽铌矿渣中多种金属元素[J].光谱学与光谱分析,2009,29(3):805-808. 被引量:19
8韩建设,李丰,吴鹰.钽铌湿法冶炼工序成本及其核算管理探讨[J].稀有金属与硬质合金,2010,38(4):46-51.
9姚卫东,曹七林,伍尊中.钽铌湿法冶炼含氟废水的综合利用及其治理[J].材料研究与应用,2011,5(1):71-73. 被引量:5
10林翠华,姜恒,宫红,苏婷婷.热分解法低温合成氟钽酸钾粉体[J].稀有金属,2011,35(6):934-938.
1张晓峰,宫茂武.火焰原子吸收法同时测定钢渣中的锶和钡[J].山东冶金,1998,20(3):45-46.
2专利名称:一种钼钒多金属冶金物料分解方法[J].中国钼业,2010,34(1):53-53.
3郭春泰,周取定.含碱金属铁氧化物还原的化学动力学研究[J].钢铁,1990,25(10):1-3. 被引量:10
4P.F.Sorensen,王家杨.金在含碱金属杂质解吸液中的沉淀[J].黄金科技动态,1989(11):26-28.
5反浸除杂稀土精矿分解方法[J].中国有色冶金,2011,40(4):82-82.
6新技术与新成果[J].中国有色冶金,2011,40(3):59-60.
7赵福生.镍闪速炉熔剂制备系统的改进实践[J].中国有色冶金,2005,34(4):44-47.
8赵明,陈雪波.大系统平衡分解的探讨[J].鞍山钢铁学院学报,2001,24(3):194-197. 被引量:1
9路永锁,叶标,宁建平.锌浸出渣烧结——还原熔炼回收铅锑锡[J].有色金属工程,2016,6(4):44-47. 被引量:2
10张伟,卫发源,叶冰峰.新型优质耐火材料及“陶瓷杯”在八钢380m^3高炉上的应用[J].新疆钢铁,1996,0(1):1-6. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]
Citation Information:
Analysis is made of the influence of alkali metals K and Na on the decomposition ratio of enriched Ta.The decomposition ratio can be improved from 92% to ≥99% by the adoption of precipitation conversion theory and proper addition of quartz powder as conversion agent without heating throughout the process.
quote
| GB/T 7714-2015 | [1] ZHONG Yue-lian. Study of Decomposition of Enriched Ta-bearing Alkaline Metals[J]. Rare Metals and Cemented Carbides, 2001(1): 12-14. |
| MLA | [1] ZHONG Yue-lian. "Study of Decomposition of Enriched Ta-bearing Alkaline Metals." Rare Metals and Cemented Carbides, no. 1, 2001, pp. 12-14. |
| APA | [1] ZHONG Yue-lian. (2001). Study of Decomposition of Enriched Ta-bearing Alkaline Metals. Rare Metals and Cemented Carbides(1), 12-14. |
| IEEE | [1] ZHONG Yue-lian, "Study of Decomposition of Enriched Ta-bearing Alkaline Metals," Rare Metals and Cemented Carbides, no. 1, pp. 12-14, 2001. keywords: {alkaline metal;enriched Ta;decomposition;quartz powder} |